IRON POWDER FOR ORGANIC CHLORINATED COMPOUND DECOMPOSITION AND DETOXIFYING TREATMENT METHOD USING THE SAME
    1.
    发明申请
    IRON POWDER FOR ORGANIC CHLORINATED COMPOUND DECOMPOSITION AND DETOXIFYING TREATMENT METHOD USING THE SAME 失效
    用于有机氯化化合物分解的铁粉和使用其的脱氧处理方法

    公开(公告)号:US20080114198A1

    公开(公告)日:2008-05-15

    申请号:US11779005

    申请日:2007-07-17

    IPC分类号: A62D3/00 C22C38/08

    摘要: In an iron powder for decomposition of organic chlorinated compounds, an iron powder having high decomposition performance in the treatment of a solid such as in a soil, and having low Ni content was required.An iron powder for decomposition of organic chlorinated compounds, comprising from 0.03 to 0.5% by weight of Ni and from 0.005 to 5% by weight of carbon, wherein particles having a particle size of less than 53 μm occupies less than 40% by weight, is used. It is particularly preferable that Ni, carbon and iron are partially alloyed. When the iron powder for decomposition is used by mixing with, for example, an Ni-free iron powder, the total Ni content can be reduced without deterioration of decomposition performance to organic chlorinated compounds.

    摘要翻译: 在用于分解有机氯化合物的铁粉中,需要在固体如土壤中处理并具有低Ni含量的具有高分解性能的铁粉。 一种用于分解有机氯化合物的铁粉,其包含0.03-0.5重量%的Ni和0.005-5重量%的碳,其中粒径小于53μm的颗粒占重量的40%以下, 用来。 特别优选Ni,碳和铁部分合金化。 当通过与例如不含Ni的铁粉混合使用用于分解的铁粉时,可以降低总的Ni含量而不降低对有机氯化合物的分解性能。

    Method of heating glass sheet for laminated glass
    2.
    发明授权
    Method of heating glass sheet for laminated glass 失效
    夹层玻璃板加热方法

    公开(公告)号:US5169423A

    公开(公告)日:1992-12-08

    申请号:US751344

    申请日:1991-08-28

    摘要: First and second glass sheets, which are to be combined together into a single laminated glass sheet, are heated in a heating furnace so that the temperature of the first glass sheet at the exit of the heating furnace and the temperature of the second glass sheet at the exit of the heating furnace are substantially equal to each other.

    摘要翻译: 将要组合成单个夹层玻璃板的第一和第二玻璃板在加热炉中加热,使得加热炉出口处的第一玻璃板的温度和第二玻璃板的温度在 加热炉的出口基本相等。

    Method of and apparatus for forming bent sheet glass
    3.
    发明授权
    Method of and apparatus for forming bent sheet glass 失效
    弯曲玻璃板成型方法及装置

    公开(公告)号:US5318615A

    公开(公告)日:1994-06-07

    申请号:US940655

    申请日:1992-09-04

    IPC分类号: C03B23/03 C03B23/035

    摘要: A heated sheet of glass discharged from a heating furnace is lifted by a ring mold until it is held against a fully continuous lower molding surface of a bent shape of an upper mold. After the sheet of glass is held against the lower molding surface by the ring mold, a vacuum is developed in the upper mold to attract the sheet of glass to the lower molding surface through suction holes defined in the lower molding surface. Thereafter, the ring mold is lowered away from the upper mold to allow the sheet of glass to be bent by the lower molding surface while the sheet of glass is being attracted thereto only under the vacuum developed in the upper mold. The sheet of glass is continuously attracted under the vacuum to the lower molding surface until the sheet of glass is annealed.

    摘要翻译: 从加热炉排出的加热玻璃片通过环形模具提升,直到其被保持在上模弯曲形状的完全连续的下模制表面上。 在通过环形模具将玻璃板保持抵靠下模制表面之后,在上模具中形成真空,以通过限定在下模制表面中的抽吸孔将玻璃板吸引到下模制表面。 此后,将环模从上模放下,使得玻璃板在下模具表面弯曲,而玻璃板仅在上模中显影的真空下被吸引。 将玻璃板在真空下连续地吸引到下模制表面,直到玻璃板退火。

    Iron powder for organic chlorinated compound decomposition and detoxifying treatment method using the same
    5.
    发明授权
    Iron powder for organic chlorinated compound decomposition and detoxifying treatment method using the same 失效
    铁粉用于有机氯化合物的分解和解毒处理方法使用

    公开(公告)号:US07718843B2

    公开(公告)日:2010-05-18

    申请号:US11779005

    申请日:2007-07-17

    摘要: An iron powder for decomposition of organic chlorinated compounds, comprising from 0.03 to 0.5% by weight of Ni and from 0.005 to 5% by weight of carbon, wherein particles having a particle size of less than 53 μm occupies less than 40% by weight, is used. It is particularly preferable that Ni, carbon and iron are partially alloyed. When the iron powder for decomposition is used by mixing with, for example, an Ni-free iron powder, the total Ni content can be reduced without deterioration of decomposition performance to organic chlorinated compounds. The iron powder has high decomposition performance in the treatment of a solid such as soil.

    摘要翻译: 一种用于分解有机氯化合物的铁粉,其包含0.03-0.5重量%的Ni和0.005-5重量%的碳,其中粒径小于53μm的颗粒占40重量%以下, 用来。 特别优选Ni,碳和铁部分合金化。 当通过与例如不含Ni的铁粉混合使用用于分解的铁粉时,可以降低总的Ni含量而不降低对有机氯化合物的分解性能。 铁粉在土壤等固体的处理中具有较高的分解性能。

    Apparatus and method for bend-shaping a glass sheet
    7.
    发明授权
    Apparatus and method for bend-shaping a glass sheet 失效
    用于弯曲成形玻璃板的装置和方法

    公开(公告)号:US07178367B2

    公开(公告)日:2007-02-20

    申请号:US10786145

    申请日:2004-02-23

    摘要: An apparatus for bend-shaping a glass sheet is disclosed, which comprises a heating furnace, a plurality of in-furnace beds disposed within the heating furnace, at least one out-furnace bed disposed externally of the heating furnace proximately to an outlet of the heating furnace, and an elevating mechanism disposed below that one of the in-furnace beds which is positioned proximately to the outlet and the out-furnace bed. The in- and out-furnace beds have upper surfaces curved transversely and capable of jetting air to floatingly support a glass sheet. For producing a dual curved glass sheet, the elevating mechanism is operated to elevate opposed ends of the one in-furnace bed and the out-furnace bed so that these beds jointly form a hill. For producing a single-curved glass sheet, the elevating mechanism is operated to lower the opposed ends of those beds to their original flat positions.

    摘要翻译: 公开了一种用于玻璃板弯曲成形的装置,其包括加热炉,设置在加热炉内的多个炉内床,至少一个外加炉床,位于加热炉外部,靠近出口处 加热炉和位于靠近出口和外炉床的炉内床之一的下方的升降机构。 炉内和外炉床的上表面横向弯曲并能够喷射空气以浮动地支撑玻璃板。 为了制造双曲面玻璃板,操作升降机构以升高一个炉内床和外炉床的相对端,使得这些床共同形成山丘。 为了制造单曲面玻璃板,升降机构被操作以将这些床的相对端部降低到原来的平坦位置。

    Method for bend-shaping a glass sheet
    8.
    发明授权
    Method for bend-shaping a glass sheet 失效
    弯曲成形玻璃板的方法

    公开(公告)号:US06725689B2

    公开(公告)日:2004-04-27

    申请号:US09909437

    申请日:2001-07-19

    IPC分类号: C03B2100

    摘要: An apparatus for bend-shaping a glass sheet is disclosed, which comprises a heating furnace, a plurality of in-furnace beds disposed within the heating furnace, at least one out-furnace bed disposed externally of the heating furnace proximately to an outlet of the heating furnace, and an elevating mechanism disposed below that one of the in-furnace beds which is positioned proximately to the outlet and the out-furnace bed. The in- and out-furnace beds have upper surfaces curved transversely and capable of jetting air to floatingly support a glass sheet. For producing a dual curved glass sheet, the elevating mechanism is operated to elevate opposed ends of the one in-furnace bed and the out-furnace bed so that these beds jointly form a hill. For producing a single-curved glass sheet, the elevating mechanism is operated to lower the opposed ends of those beds to their original flat positions.

    摘要翻译: 公开了一种用于玻璃板弯曲成形的装置,其包括加热炉,设置在加热炉内的多个炉内床,至少一个外加炉床,位于加热炉外部,靠近出口处 加热炉和位于靠近出口和外炉床的炉内床之一的下方的升降机构。 炉内和外炉床的上表面横向弯曲并能够喷射空气以浮动地支撑玻璃板。 为了制造双曲面玻璃板,操作升降机构以升高一个炉内床和外炉床的相对端,使得这些床共同形成山丘。 为了制造单曲面玻璃板,升降机构被操作以将这些床的相对端部降低到原来的平坦位置。