摘要:
A subjective vision testing system is used for visual function tests for examinees. The subjective vision testing system is provided with an optometric apparatus which selectively sets optical elements in front of both eyes of an examinee, an optotype presenting apparatus for displaying optotypes to the examinee, and a controller. The optotype presenting apparatus, based on a command signal for implementation of a binocular balance test, displays optotypes used for binocular balance tests. The optometric apparatus, based on a command signal for implementation of a binocular balance test, sets a first prism in front of the examinee's right eye and a second prism in front of the examinee's left eye. The second prism has a base direction vertically opposite to the first prism and the same prism power as the first prism.
摘要:
A ferritic stainless steel sheet for use in raw material pipes for forming bellows pipes has excellent formability. More specifically, the ferritic stainless steel sheet contains 10% to 25% by mass of Cr and has a yield stress in the range of 300 to 450 MPa and the product of the yield stress and the uniform elongation properties of at least 5200 (MPa·%). Preferably, the ferritic stainless steel sheet for use in raw material pipes for forming bellows pipes has an average crystal grain size D of 35 μm or less or a surface roughness of 0.40 μm or less as determined by Ra.
摘要:
A finish annealed non-oriented electromagnetic steel sheet includes about 0.01 wt % or less of C, greater than about 1.0 wt % and at most about 3.5 wt % of Si, at least about 0.6 wt % and at most about 3.0 wt % of Al, at least about 0.1 wt % and at most about 2.0 wt % of Mn, at least about 2 ppm and at most about 80 ppm of one or more rare earth metals (REM), a maximum content of Ti and Zr being about 15 ppm and 80 ppm, respectively, wherein oxygen on the surface layer of the steel sheet is 1.0 g/m2 or less. Since the non-oriented electromagnetic steel sheet has desirable mechanical properties resulting from the increased amounts of Si and Al, a high magnetic flux density can be maintained without sacrificing a punching property as well as very low iron loss can be obtained even after stress relief annealing.
摘要翻译:完成退火的无取向电磁钢板包括约0.01重量%或更少的C,大于约1.0重量%,至多约3.5重量%的Si,至少约0.6重量%和至多约3.0重量%的Al ,至少约0.1重量%,至多约2.0重量%的Mn,至少约2ppm和至多约80ppm的一种或多种稀土金属(REM),Ti和Zr的最大含量为约15ppm 和80ppm,其中钢板表层上的氧为1.0g / m 2以下。 由于无取向电磁钢板由于Si和Al的量增加而具有期望的机械特性,因此即使在消除应力退火后也可以获得高的磁通密度,同时不会牺牲冲压性能,甚至可以获得非常低的铁损 。
摘要:
A hydraulic actuating apparatus includes a cylindrical case having a fitting at one end connectable to a source of pressurized oil, the fitting having a passage for communication with the pressurized oil, a slider slidably carried by the cylindrical case, the slider being slidable in response to the oil pressure, a first spring device for biasing the slider in a predetermined direction to resist the force on the slider applied by the oil pressure, a slidable contact device carried by the slider, an oil pressure sensor which includes a resistor and a ground conductor, the slidable contact device being slidably engaged with the resistor, the resistor being fixed with respect to the slidable contact device, and a second spring device for biasing the slider in the predetermined direction. The second spring device is connected to the slider, with the second spring device having a smaller spring constant than the first spring device. The hydraulic actuating apparatus further includes a fuel pump switch having a movable contact and a fixed contact, wherein movement of the movable contact relative to the fixed contact causes one of contact and release of the fuel pump switch, the fuel pump switch is assembled integrally in the case, and the resistor includes a flat resistor.
摘要:
A process for manufacturing a dielectric member from aluminum or aluminum alloy which includes the steps of subjecting the aluminum or aluminum alloy to anodic oxidation in a nonaqueous electrolytic solution containing an organic solvent and dehydrated boric acid to form an oxide layer thereon, and buffing the oxide layer with a composition containing insulative abrasive grains and insulative binding material.
摘要:
A martensitic stainless steel, having high temper softening resistance, for disc brakes is provided. The martensitic stainless steel is not seriously softened by maintaining the steel at more than 600° C. The steel has a hardness of 32 or more or a hardness of 30 or more in HRC after the steel is tempered at 650° C. for one hour or tempered at 670° C. for one hour, respectively. In particular, the martensitic stainless steel for disc brakes contains less than 0.050 mass % carbon, 1.0 mass % or less silicon, 2.0 mass % or less manganese, 0.04 mass % or less phosphorus, 0.010 mass % or less sulfur, 0.2 mass % or less aluminum, more than 11.5 mass % to 15.0 mass % chromium, 0.5 mass % to 2.0 mass % nickel, more than 0.50 mass % to 4.0 mass %. copper, more than 0.08 mass % to 0.6 mass % niobium, and less than 0.09 mass % nitrogen, the remainder being iron and unavoidable impurities. The carbon content, the nitrogen content, the niobium content, the chromium content, the silicon content, the nickel content, the manganese content, and the copper content satisfy the following inequalities (1) and (2): 0.03≦[C]+[N]−13/93×[Nb]≦0.09 (1) 5×[Cr]+10×[Si]+30×[Nb]−9×[Ni]−5×[Mn]−3×[Cu]−225×[N]−270×[C]≦40 (2).
摘要:
A subjective vision testing system is used for visual function tests for examinees. The subjective vision testing system is provided with an optometric apparatus which selectively sets optical elements in front of both eyes of an examinee, an optotype presenting apparatus for displaying optotypes to the examinee, and a controller. The optotype presenting apparatus, based on a command signal for implementation of a binocular balance test, displays optotypes used for binocular balance tests. The optometric apparatus, based on a command signal for implementation of a binocular balance test, sets a first prism in front of the examinee's right eye and a second prism in front of the examinee's left eye. The second prism has a base direction vertically opposite to the first prism and the same prism power as the first prism.
摘要:
A martensitic stainless steel sheet which is hard to be softened by tempering caused by heating during the use of a disk brake, can maintain the predetermined hardness, and has excellent punching workability, bending workability before quenching, and a particularly small shear drop, and in which a predetermined hardness after quenching is constantly achieved, in a low carbon martensitic stainless steel sheet used only after quenching. Specifically, the sheet contains, on the basis of mass percent, 0.030% to 0.100% C; 0.50% or less of Si; 1.00% to 2.50% Mn; more than 10.00% to 15.00% Cr; at least one selected from the group consisting of 0.01% to 0.50% Ti, 0.01% to 0.50% V, 0.01% to 1.00% Nb, and 0.01% to 1.00% Zr; N in an amount defined by the following expression, N: 0.005% to (Ti+V)×14/50+(Nb+Zr)×14/90; and the balance being Fe and incidental impurities.
摘要:
A ferritic stainless steel sheet for use in automobile fuel tanks and fuel pipes having smooth surface and resistance to organic acid is provided. The sheet contains, by mass, not more than about 0.1% C, not more than about 1.0 Si, not more than about 1.5 % Mn, not more than about 0.06% P, not more than about 0.03% S, about 11% to about 23% Cr, not more than about 2.0% Ni, about 0.5% to about 3.0% Mo, not more than about 1.0% Al, not more than about 0.04% N, at least one of not more than about 0.8% Nb and not more than about 1.0% Ti, and the balance being Fe and unavoidable impurities, satisfying the relationship: 18≦Nb/(C+N)+2Ti/(C+N)≦60, wherein C, N, Nb, and. Ti in the relationship represent the C, N, Nb, and Ti contents by mass percent, respectively. A process for making the same is also provided.
摘要:
A method of producing diphenyl sulfone compounds of the formula (I) ##STR1## wherein R is an alkyl having 1 to 8 carbon atoms, a cycloalkyl having 3 to 8 carbon atoms, an alkenyl having 2 to 8 carbon atoms or an arylalkyl which may have substituent(s) on the aromatic ring, comprising reacting 4,4'-dihydroxydiphenyl sulfone with a compound of the formulaR--Xwherein R is as defined above and X is halogen, characterized by conducting the reaction in 0.3-1.5 weight parts of an aqueous solvent per weight part of 4,4'-dihydroxydiphenyl sulfone in the presence of 1.5-3 moles of an alkali per mole of 4,4'-dihydroxydiphenyl sulfone. Since the method of the invention permits production of 4-substituted hydroxy-4'-hydroxydiphenyl sulfones, specifically 4-n-propoxy-4'-hydroxydiphenyl sulfone or 4-isopropoxy-4'-hydroxydiphenyl sulfone using an inexpensive solvent, with good selectivity and economical feasibility, they are industrially advantageous.