ORIGINAL PLATE MATERIAL FOR HEAT-EXCHANGING PLATE AND HEAT-EXCHANGING PLATE USING THE SAME
    3.
    发明申请
    ORIGINAL PLATE MATERIAL FOR HEAT-EXCHANGING PLATE AND HEAT-EXCHANGING PLATE USING THE SAME 审中-公开
    用于换热板和加热板的原料板材料

    公开(公告)号:US20140202677A1

    公开(公告)日:2014-07-24

    申请号:US14232549

    申请日:2012-09-14

    IPC分类号: F28F3/02

    摘要: An original plate material for a heat exchanging plate includes a titanium flat plate material including a minute recess and projections on the surface thereof, and the flat plate material is press-worked to obtain the heat exchanging plate. The shape parameter, defined as [height (μm) of the projections]×[width (μm) of the recess/pitch (μm) of adjacent projections], is 85 μm or less. Relating to this original plate material for a heat exchanging plate, the shape parameter, defined as [height (μm) of the projections]×[width (μm) of the recess/pitch (μm) of adjacent projections/angle (deg) of the projections], is 0.94 μm/deg or less.

    摘要翻译: 用于热交换板的原始板材包括在其表面上包括微小凹陷和突起的钛平板材料,并且对平板材料进行压力加工以获得热交换板。 形状参数定义为[凸起的高度(μm)]×[相邻突起的凹部/间距(μm)的宽度(μm)]为85μm以下。 关于这种用于热交换板的原始板材,形状参数被定义为[凸起的高度(μm)]×[相邻突起的凹部/间距(μm)的宽度(μm)/角度(度) 投影]为0.94μm/ deg以下。

    ORIGINAL PLATE MATERIAL FOR HEAT-EXCHANGING PLATE, AND METHOD FOR FABRICATING ORIGINAL PLATE MATERIAL FOR HEAT-EXCHANGING PLATE
    4.
    发明申请
    ORIGINAL PLATE MATERIAL FOR HEAT-EXCHANGING PLATE, AND METHOD FOR FABRICATING ORIGINAL PLATE MATERIAL FOR HEAT-EXCHANGING PLATE 有权
    热交换板用原板材及其加热板原料板材料的制造方法

    公开(公告)号:US20130037246A1

    公开(公告)日:2013-02-14

    申请号:US13643715

    申请日:2011-04-27

    IPC分类号: F28F3/04 B21D53/02 B21D22/02

    摘要: Provided is an original plate material for a heat-exchanging plate fabricated by press working, and also provided is a method for fabricating the original plate material. An original plate material (2) for a heat-exchanging plate (4) is a flat plate material (1) made of titanium on the surface of which convex parts and concave parts are formed, and the heat-exchanging plate (4) is then fabricated by press working the original plate material (2). The convex parts (5) and the concave parts (6) are formed in a manner such that the shape parameter defined by (Rz×L/P) is 12 μm or less, where Rz (μm) denotes the height of the convex parts (5), L (μm) denotes the width of the concave parts (6), and P (μm) denotes the pitch between neighboring convex parts (5).

    摘要翻译: 提供了一种用于通过冲压加工制造的热交换板的原始板材,并且还提供了用于制造原始板材的方法。 用于热交换板(4)的原板材(2)是在其上形成有凸部和凹部的表面上由钛制成的平板材料(1),并且热交换板 然后通过冲压加工原始板材(2)制成。 凸部(5)和凹部(6)以(Rz×L / P)所定义的形状参数为12μm以下的方式形成,其中,Rz(μm)表示凸部 (5)中,L(μm)表示凹部(6)的宽度,P(μm)表示相邻的凸部(5)之间的间距。

    PURE TITANIUM SHEET EXCELLENT IN BALANCE BETWEEN STAMPING FORMABILITY AND STRENGTH
    5.
    发明申请
    PURE TITANIUM SHEET EXCELLENT IN BALANCE BETWEEN STAMPING FORMABILITY AND STRENGTH 有权
    纯钛片与冲压强度之间的平衡优良

    公开(公告)号:US20120193084A1

    公开(公告)日:2012-08-02

    申请号:US13350057

    申请日:2012-01-13

    IPC分类号: F28F7/00 C22C14/00

    摘要: Disclosed is a pure titanium sheet having a strength corresponding to JIS Grade 2 level (215 MPa in terms of 0.2% yield strength) or more and having satisfactory stamping formability. The pure titanium sheet includes titanium and inevitable impurities, has a 0.2% yield strength of 215 MPa or more, has an average grain size d of its structure of 25 μm or more and 75 μm or less, and has a hexagonal crystal structure, in which respective grains in the hexagonal crystal structure have an average of Schmidt factors (SF) of (11-22) twins with a rolling direction as axes, and the average Schmidt factor (SF) and the average grain size d satisfy following Expression (1): 0.055≦[SF/√d]≦0.084  (1)

    摘要翻译: 公开了具有JIS等级2的强度(屈服强度为0.2%的215MPa)以上且具有令人满意的冲压成形性的纯钛片。 纯钛片包括钛和不可避免的杂质,其屈服强度的0.2%为215MPa以上,其结构的平均粒径d为25μm以上且75μm以下,具有六方晶系结构, 六方晶系结构中的各晶粒的平均Schmidt因子(SF)为(11-22)双轴,轧制方向为轴,平均施密特因子(SF)和平均晶粒尺寸d满足下式(1 ):0.055≦̸ [SF /√d]≦̸ 0.084(1)

    Pure titanium sheet excellent in balance between stamping formability and strength
    7.
    发明授权
    Pure titanium sheet excellent in balance between stamping formability and strength 有权
    纯钛板在冲压成型性和强度之间的平衡优异

    公开(公告)号:US09353432B2

    公开(公告)日:2016-05-31

    申请号:US13350057

    申请日:2012-01-13

    IPC分类号: C22F1/18 C22C14/00 F28F21/08

    摘要: Disclosed is a pure titanium sheet having a strength corresponding to JIS Grade 2 level (215 MPa in terms of 0.2% yield strength) or more and having satisfactory stamping formability. The pure titanium sheet includes titanium and inevitable impurities, has a 0.2% yield strength of 215 MPa or more, has an average grain size d of its structure of 25 μm or more and 75 μm or less, and has a hexagonal crystal structure, in which respective grains in the hexagonal crystal structure have an average of Schmidt factors (SF) of (11-22) twins with a rolling direction as axes, and the average Schmidt factor (SF) and the average grain size d satisfy following Expression (1): 0.055≦[SF/√d]≦0.084  (1).

    摘要翻译: 公开了具有JIS等级2的强度(屈服强度为0.2%的215MPa)以上且具有令人满意的冲压成形性的纯钛片。 纯钛片包括钛和不可避免的杂质,其屈服强度的0.2%为215MPa以上,其结构的平均粒径d为25μm以上且75μm以下,具有六方晶系结构, 六方晶系结构中的各晶粒的平均Schmidt因子(SF)为(11-22)双轴,轧制方向为轴,平均施密特因子(SF)和平均晶粒尺寸d满足下述式(1 ):0.055≦̸ [SF /√d]≦̸ 0.084(1)。