Polyarylene sulfide resin with excellent luminosity and preparation method thereof
    1.
    发明授权
    Polyarylene sulfide resin with excellent luminosity and preparation method thereof 有权
    具有优异亮度的聚芳硫醚树脂及其制备方法

    公开(公告)号:US08883960B2

    公开(公告)日:2014-11-11

    申请号:US12518369

    申请日:2008-01-04

    Abstract: The present invention relates to a polyarylene sulfide that is prepared from a composition including 100 parts by weight of solid sulfur, 500 to 10,000 parts by weight of iodinated aryl compounds, and 0.03 to 30 parts by weight of a sulfur-containing polymerization terminator with respect to 100 parts by weight of the solid sulfur, and has a melting temperature (Tm) of 255 to 285° C., and luminosity of 40 or higher as defined by the CIE Lab color model, and a process of preparing the same. The PAS resin is prepared from a composition including a sulfur-containing polymerization terminator and thus has excellent thermal properties and luminosity.

    Abstract translation: 本发明涉及一种聚芳硫醚,其由包含100重量份固体硫,500至10,000重量份碘化芳基化合物和0.03至30重量份含硫聚合终止剂的组合物制备,相对于 至100重量份固体硫,并且具有255至285℃的熔融温度(Tm)和由CIE Lab颜色模型所定义的40或更高的亮度及其制备方法。 PAS树脂由包含含硫聚合终止剂的组合物制备,因此具有优异的热性能和亮度。

    Manufacturing process for poly (arylene sulphide)
    2.
    发明授权
    Manufacturing process for poly (arylene sulphide) 有权
    聚(亚硫酰)制造工艺

    公开(公告)号:US08242233B2

    公开(公告)日:2012-08-14

    申请号:US12310336

    申请日:2007-08-21

    CPC classification number: C08G75/0213 C08G75/0231 C08G75/0263 C08G75/029

    Abstract: This invention relates to a method of preparing poly(arylene sulfide) (PAS) from an iodo compound and a sulfur compound, and more particularly, to a method of preparing PAS, including adding a sulfur-containing polymerization terminator when PAS is produced using an iodo compound as an intermediate. Thereby, in final PAS, the residual iodine content may be maintained at the same level or decreased and other properties may be maintained at equal or superior levels, thanks to the use of the sulfur-containing polymerization terminator, which is much lower in price than conventional polymerization terminators.

    Abstract translation: 本发明涉及一种由碘化合物和硫化合物制备聚(亚芳基硫醚)(PAS)的方法,更具体地说,涉及一种制备PAS的方法,包括在使用 碘化合物作为中间体。 因此,在最终的PAS中,残留的碘含量可以保持在相同的水平或降低,并且由于使用的硫含量聚合终止剂的价格低得多,所以其他性能可以维持在相同或更高的水平 常规聚合终止剂。

    METHOD FOR PRODUCTION OF POLYARYLENE SULFIDE RESIN WITH EXCELLENT LUMINOSITY AND THE POLYARYLENE SULFIDE RESIN
    3.
    发明申请
    METHOD FOR PRODUCTION OF POLYARYLENE SULFIDE RESIN WITH EXCELLENT LUMINOSITY AND THE POLYARYLENE SULFIDE RESIN 有权
    用于生产具有优异亮度的聚亚烷基硫酸盐树脂的方法和聚氯乙烯树脂

    公开(公告)号:US20100105845A1

    公开(公告)日:2010-04-29

    申请号:US12518243

    申请日:2008-01-04

    Abstract: The present invention relates to a process of producing polyarylene sulfide (PAS) and PAS resin produced therefrom, and more specifically, to a process of preparing polyarylene sulfide with better thermal properties and luminosity than conventional PAS and the PAS resin produced therefrom, including the steps of: a) melting and mixing a composition including solid sulfur, iodinated aryl compounds, and a polymerization terminator; b) polymerizing the molten mixture of step a) for 1 to 30 hours while increasing the temperature and decreasing the pressure from initial reaction conditions of a temperature of 180 to 250° C. and a pressure of 50 to 450 Torr to final reaction conditions of a temperature of 270 to 350° C. and a pressure of 0.001 to 20 Torr; and c) heating the reaction product of step b) at a temperature of 270 to 350° C. for 1 to 25 hours. The process of polyarylene sulfide resin further includes a step of heating the polymerized product at a high temperature following the polymerization step, and uses the polymerization terminator in a suitable amount to control the molecular weight of polyarylene sulfide, thereby producing polyarylene sulfide with excellent thermal properties and luminosity.

    Abstract translation: 本发明涉及一种生产聚芳硫醚(PAS)和由其制备的PAS树脂的方法,更具体地说,涉及制备具有比常规PAS和由其制备的PAS树脂更好的热性能和发光度的聚芳硫醚的方法,包括步骤 a)熔融和混合包括固体硫,碘化芳基化合物和聚合终止剂的组合物; b)使步骤a)的熔融混合物聚合1至30小时,同时增加温度并将温度从180-250℃的初始反应条件和50至450托的压力降低至最终反应条件 温度为270〜350℃,压力为0.001〜20托; 和c)将步骤b)的反应产物在270至350℃的温度下加热1至25小时。 聚芳硫醚树脂的方法还包括在聚合步骤之后在高温下加热聚合产物的步骤,并且使用适当量的聚合终止剂来控制聚芳硫醚的分子量,由此制备具有优异热性质的聚芳硫醚 和亮度。

    Method for production of polyarylene sulfide resin with excellent luminosity and the polyarylene sulfide resin
    4.
    发明授权
    Method for production of polyarylene sulfide resin with excellent luminosity and the polyarylene sulfide resin 有权
    具有优异亮度的聚芳硫醚树脂的生产方法和聚芳硫醚树脂

    公开(公告)号:US08492502B2

    公开(公告)日:2013-07-23

    申请号:US12518243

    申请日:2008-01-04

    Abstract: The present invention relates to a process of producing polyarylene sulfide (PAS) and PAS resin produced therefrom, and more specifically, to a process of preparing polyarylene sulfide with better thermal properties and luminosity than conventional PAS and the PAS resin produced therefrom, including the steps of: a) melting and mixing a composition including solid sulfur, iodinated aryl compounds, and a polymerization terminator; b) polymerizing the molten mixture of step a) for 1 to 30 hours while increasing the temperature and decreasing the pressure from initial reaction conditions of a temperature of 180 to 250° C. and a pressure of 50 to 450 Torr to final reaction conditions of a temperature of 270 to 350° C. and a pressure of 0.001 to 20 Torr; and c) heating the reaction product of step b) at a temperature of 270 to 350° C. for 1 to 25 hours. The process of polyarylene sulfide resin further includes a step of heating the polymerized product at a high temperature following the polymerization step, and uses the polymerization terminator in a suitable amount to control the molecular weight of polyarylene sulfide, thereby producing polyarylene sulfide with excellent thermal properties and luminosity.

    Abstract translation: 本发明涉及一种生产聚芳硫醚(PAS)和由其制备的PAS树脂的方法,更具体地说,涉及制备具有比常规PAS和由其制备的PAS树脂更好的热性能和发光度的聚芳硫醚的方法,包括步骤 a)熔融和混合包括固体硫,碘化芳基化合物和聚合终止剂的组合物; b)使步骤a)的熔融混合物聚合1至30小时,同时增加温度并将温度从180-250℃的初始反应条件和50至450托的压力降低至最终反应条件 温度为270〜350℃,压力为0.001〜20托; 和c)将步骤b)的反应产物在270至350℃的温度下加热1至25小时。 聚芳硫醚树脂的方法还包括在聚合步骤之后在高温下加热聚合产物的步骤,并且使用适当量的聚合终止剂来控制聚芳硫醚的分子量,由此制备具有优异热性质的聚芳硫醚 和亮度。

    POLYARYLENE SULFIDE RESIN WITH EXCELLENT LUMINOSITY AND PREPARATION METHOD THEREOF
    5.
    发明申请
    POLYARYLENE SULFIDE RESIN WITH EXCELLENT LUMINOSITY AND PREPARATION METHOD THEREOF 有权
    具有优异荧光性的聚亚烷基硫酸酯树脂及其制备方法

    公开(公告)号:US20100022743A1

    公开(公告)日:2010-01-28

    申请号:US12518369

    申请日:2008-01-04

    Abstract: The present invention relates to a polyarylene sulfide that is prepared from a composition including 100 parts by weight of solid sulfur, 500 to 10,000 parts by weight of iodinated aryl compounds, and 0.03 to 30 parts by weight of a sulfur-containing polymerization terminator with respect to 100 parts by weight of the solid sulfur, and has a melting temperature (Tm) of 255 to 285° C., and luminosity of 40 or higher as defined by the CIE Lab color model, and a process of preparing the same. The PAS resin is prepared from a composition including a sulfur-containing polymerization terminator and thus has excellent thermal properties and luminosity.

    Abstract translation: 本发明涉及一种聚芳硫醚,其由包含100重量份固体硫,500至10,000重量份碘化芳基化合物和0.03至30重量份含硫聚合终止剂的组合物制备,相对于 至100重量份固体硫,并且具有255至285℃的熔融温度(Tm)和由CIE Lab颜色模型所定义的40或更高的亮度及其制备方法。 PAS树脂由包含含硫聚合终止剂的组合物制备,因此具有优异的热性能和亮度。

    MANUFACTURING PROCESS FOR POLY (ARYLENE SULPHIDE)
    6.
    发明申请
    MANUFACTURING PROCESS FOR POLY (ARYLENE SULPHIDE) 有权
    聚亚磺酸的制造工艺

    公开(公告)号:US20090203872A1

    公开(公告)日:2009-08-13

    申请号:US12310336

    申请日:2007-08-21

    CPC classification number: C08G75/0213 C08G75/0231 C08G75/0263 C08G75/029

    Abstract: This invention relates to a method of preparing poly(arylene sulfide) (PAS) from an iodo compound and a sulfur compound, and more particularly, to a method of preparing PAS, including adding a sulfur-containing polymerization terminator when PAS is produced using an iodo compound as an intermediate. Thereby, in final PAS, the residual iodine content may be maintained at the same level or decreased and other properties may be maintained at equal or superior levels, thanks to the use of the sulfur-containing polymerization terminator, which is much lower in price than conventional polymerization terminators.

    Abstract translation: 本发明涉及一种由碘化合物和硫化合物制备聚(亚芳基硫醚)(PAS)的方法,更具体地说,涉及一种制备PAS的方法,包括在使用 碘化合物作为中间体。 因此,在最终的PAS中,残留的碘含量可以保持在相同的水平或降低,并且由于使用的硫含量聚合终止剂的价格低得多,所以其他性能可以维持在相同或更高的水平 常规聚合终止剂。