公开(公告)号:US08211399B2
公开(公告)日:2012-07-03
申请号:US12858563
申请日:2010-08-18
Applicant: Ya-Dong Li , Qing Peng , Zhong-Bin Zhuang , Xiao-Tang Lu
Inventor: Ya-Dong Li , Qing Peng , Zhong-Bin Zhuang , Xiao-Tang Lu
IPC: C01B17/20
CPC classification number: C01G21/21 , B82Y30/00 , C01G3/12 , C01G5/00 , C01G9/08 , C01G49/12 , C01P2002/72 , C01P2004/03 , C01P2004/30 , C01P2004/32 , C01P2004/38 , C01P2004/62 , C01P2004/64 , Y10S977/773 , Y10S977/81
Abstract: A method for making metal sulfide nanocrystals is provided. First, some metal salt powders are provided in a container. Second, superfluous mercaptan is added into the container. Then the superfluous mercaptan and the metal salt are stirred uniformly to get a precursor mixture and the precursor mixture is heated to get the metal sulfide nanocrystals. Lastly, the metal sulfide nanocrystals are separated and washed.
Abstract translation: 提供了制备金属硫化物纳米晶体的方法。 首先,在容器中设置一些金属盐粉末。 第二,将多余的硫醇加入容器中。 然后将多余的硫醇和金属盐均匀搅拌,得到前体混合物,并将前体混合物加热得到金属硫化物纳米晶体。 最后,分离和洗涤金属硫化物纳米晶体。
-
公开(公告)号:US20110311434A1
公开(公告)日:2011-12-22
申请号:US12858563
申请日:2010-08-18
Applicant: YA-DONG LI , QING PENG , ZHONG-BIN ZHUANG , XIAO-TANG LU
Inventor: YA-DONG LI , QING PENG , ZHONG-BIN ZHUANG , XIAO-TANG LU
IPC: C01B17/20
CPC classification number: C01G21/21 , B82Y30/00 , C01G3/12 , C01G5/00 , C01G9/08 , C01G49/12 , C01P2002/72 , C01P2004/03 , C01P2004/30 , C01P2004/32 , C01P2004/38 , C01P2004/62 , C01P2004/64 , Y10S977/773 , Y10S977/81
Abstract: A method for making metal sulfide nanocrystals is provided. First, some metal salt powders are provided in a container. Second, superfluous mercaptan is added into the container. Then the superfluous mercaptan and the metal salt are stirred uniformly to get a precursor mixture and the precursor mixture is heated to get the metal sulfide nanocrystals. Lastly, the metal sulfide nanocrystals are separated and washed.
Abstract translation: 提供了制备金属硫化物纳米晶体的方法。 首先,在容器中设置一些金属盐粉末。 第二,将多余的硫醇加入容器中。 然后将多余的硫醇和金属盐均匀搅拌,得到前体混合物,并将前体混合物加热得到金属硫化物纳米晶体。 最后,分离和洗涤金属硫化物纳米晶体。
-
公开(公告)号:US08795550B2
公开(公告)日:2014-08-05
申请号:US12647643
申请日:2009-12-28
Applicant: Ya-Dong Li , Qing Peng , Zhong-Bin Zhuang
Inventor: Ya-Dong Li , Qing Peng , Zhong-Bin Zhuang
CPC classification number: H01M4/5825 , C01B33/24 , H01M4/366 , H01M4/625
Abstract: A method for preparing a cathode active material includes mixing a phosphorus source material, a lithium source material, and a dispersing agent together to form a first liquid mixture. An iron powder is added into the first liquid mixture. The first liquid mixture with the iron powder therein is dried to achieve a precursor. The precursor is calcined in a protective gas at a temperature of about 600° C. to about 800° C. for more than about 2 hours.
Abstract translation: 制备阴极活性材料的方法包括将磷源材料,锂源材料和分散剂混合在一起形成第一液体混合物。 将铁粉加入到第一液体混合物中。 将其中含有铁粉的第一液体混合物干燥以获得前体。 该前体在保护气体中在约600℃至约800℃的温度下煅烧超过约2小时。
-
公开(公告)号:US20110073803A1
公开(公告)日:2011-03-31
申请号:US12647643
申请日:2009-12-28
Applicant: YA-DONG LI , QING PENG , ZHONG-BIN ZHUANG
Inventor: YA-DONG LI , QING PENG , ZHONG-BIN ZHUANG
IPC: H01M4/136
CPC classification number: H01M4/5825 , C01B33/24 , H01M4/366 , H01M4/625
Abstract: A method for preparing a cathode active material includes mixing a phosphorus source material, a lithium source material, and a dispersing agent together to form a first liquid mixture. An iron powder is added into the first liquid mixture. The first liquid mixture with the iron powder therein is dried to achieve a precursor. The precursor is calcined in a protective gas at a temperature of about 600° C. to about 800° C. for more than about 2 hours.
Abstract translation: 制备阴极活性材料的方法包括将磷源材料,锂源材料和分散剂混合在一起形成第一液体混合物。 将铁粉加入到第一液体混合物中。 将其中含有铁粉的第一液体混合物干燥以获得前体。 该前体在保护气体中在约600℃至约800℃的温度下煅烧超过约2小时。
-
-
-