Abstract:
A Mo—Si—B-based alloy for a heat-resistant alloy that satisfies, more than conventional, physical properties such as proof stress and hardness adapted to an increase in the melting point of 5 a welding object. The Mo—Si—B-based alloy powder is such that the full width at half maximum of (600) of Mo5SiB2 in X-ray diffraction peak data is 0.08 degrees or more and 0.7 degrees or less.
Abstract:
Provided is a Mo—Si—B-based alloy for a heat-resistant alloy that satisfies, more than conventional, physical properties such as proof stress and hardness adapted to an increase in the melting point of a welding object.A Mo—Si—B-based alloy powder of this invention is such that the full width at half maximum of (600) of Mo5SiB2 in X-ray diffraction peak data is 0.08 degrees or more and 0.7 degrees or less.
Abstract:
The present heat-resistant tungsten alloy has a first phase containing W as a major component, a second phase having a carbonitride of at least one element of Ti, Zr and Hf and containing the carbonitride as a major component when W is removed, and a third phase having a carbide of at least one element of group 5A elements in the periodic table and containing the carbide as a major component when W is removed, the heat-resistant tungsten alloy having a Vickers hardness of 550 Hv or more at a room temperature, a displacement of 1 mm or more when leading to fracture, as determined in a three point bending test at 1200° C., and a 0.2% proof stress of 900 MPa or more, as determined in the three point bending test at 1200° C.
Abstract:
A heat-resistant molybdenum alloy of this invention comprises a first phase containing Mo as a main component and a second phase comprising a Mo—Si—B-based intermetallic compound particle phase, wherein the balance is an inevitable impurity and wherein the Si content is 0.05 mass % or more and 0.80 mass % or less and the B content is 0.04 mass % or more and 0.60 mass % or less.
Abstract:
The present heat-resistant tungsten alloy has a first phase containing W as a major component, a second phase having a carbonitride of at least one element of Ti, Zr and Hf and containing the carbonitride as a major component when W is removed, and a third phase having a carbide of at least one element of group 5A elements in the periodic table and containing the carbide as a major component when W is removed, the heat-resistant tungsten alloy having a Vickers hardness of 550 Hv or more at a room temperature, a displacement of 1 mm or more when leading to fracture, as determined in a three point bending test at 1200° C., and a 0.2% proof stress of 900 MPa or more, as determined in the three point bending test at 1200° C.
Abstract:
A heat-resistant molybdenum alloy of this invention comprises a first phase containing Mo as a main component and a second phase comprising a Mo—Si—B-based intermetallic compound particle phase, wherein the balance is an inevitable impurity and wherein the Si content is 0.05 mass % or more and 0.80 mass % or less and the B content is 0.04 mass % or more and 0.60 mass % or less.
Abstract:
A heat-resistant member comprising a molybdenum alloy that comprises a first phase containing Mo as a main component and a second phase comprising a Mo—Si—B-based intermetallic compound particle phase, wherein the balance is an inevitable impurity and wherein the Si content is 0.05 mass % or more and 0.80 mass % or less and the B content is 0.04 mass % or more and 0.60 mass % or less. The member may be coated.