CRYSTALLIZED GLASS AND CHEMICALLY STRENGTHENED GLASS

    公开(公告)号:US20200239354A1

    公开(公告)日:2020-07-30

    申请号:US16747586

    申请日:2020-01-21

    Applicant: AGC Inc.

    Abstract: A crystallized glass that: has a visible light transmittance of at least 85% when the thickness thereof is converted to 0.8 mm; has a haze value of no more than 1.0% when the thickness thereof is converted to 0.8 mm; contains, in terms of mass % on an oxide basis, 58%-70% SiO2, 15%-30% Al2O3, 2%-10% Li2O, 0%-5% Na2O, 0%-2% K2O, 0%-1.8% SrO, 0%-2% BaO, 0.5%-6% SnO2, 0.5%-6% ZrO2, and 0%-6% P2O5; has a total SrO and BaO content of 0.1%-3%; and has a total Na2O and K2O content of 1%-5%.

    CRYSTALLIZED GLASS MANUFACTURING METHOD
    2.
    发明公开

    公开(公告)号:US20240092678A1

    公开(公告)日:2024-03-21

    申请号:US18520792

    申请日:2023-11-28

    Applicant: AGC Inc.

    Inventor: Qing LI Seiki OHARA

    CPC classification number: C03B32/02 C03B11/125

    Abstract: The present invention relates to a method for producing crystallized glass, including: (a1) melting a glass raw material to obtain molten glass; (a2) molding the molten glass into a predetermined shape by a molding unit to obtain a glass molded body; (a3) slowly cooling the glass molded body to obtain a raw glass plate containing at least one of a crystal nucleus and a separated phase; and (a4) heat-treating the raw glass plate containing the at least one of the crystal nucleus and the separated phase to cause crystal growth so as to obtain the crystallized glass.

    CHEMICALLY-STRENGTHENED GLASS CONTAINING GLASS CERAMIC, AND METHOD FOR MANUFACTURING SAME

    公开(公告)号:US20230406763A1

    公开(公告)日:2023-12-21

    申请号:US18461121

    申请日:2023-09-05

    Applicant: AGC Inc.

    CPC classification number: C03C21/002 C03C23/0075 C03C10/0027 C03C3/097

    Abstract: The present invention relates to a chemically-strengthened glass having a first main surface and a second main surface, including a glass ceramic including a crystal and a residual glass, having a surface compressive stress value (CS0) of 450 MPa or more, and a compressive stress value (CS50) at a depth of 50 μm of 150 MPa or more, having a plurality of non-through holes having a diameter average value of 5 nm to 50 nm on the first main surface and the second main surface, the non-through holes having a depth average value measured by a cross-sectional SEM image of the first main surface and the second main surface of 5 nm to 50 nm, and having a total area ratio to a total visual field area of a surface SEM image of the first main surface and the second main surface of 1% to 40%.

    GLASS CERAMIC AND CHEMICALLY STRENGTHENED GLASS

    公开(公告)号:US20230365456A1

    公开(公告)日:2023-11-16

    申请号:US18355545

    申请日:2023-07-20

    Applicant: AGC INC.

    CPC classification number: C03C10/0009 C03C10/0054

    Abstract: The present invention is a glass ceramic including a crystal and a residual glass, in which the residual glass has a Young's modulus parameter ER of 75 or more, the Young's modulus parameter ER being calculated based on the following formula: ER=62.2×[SiO2]+134.9×[Al2O3]+121.7×[B2O3]+33.0×[P2O5]+72.6×[MgO]+121.5×[CaO]+43.7×[SrO]+38.6×[BaO]+84.0×[Li2O]+26.2×[Na2O]+17.8×[K2O]+156.8×[ZrO2]+154.3×[TiO2]+74.7×[La2O3]+80.3×[Y2O3]+54.3×[ZnO].