CHEMICALLY STRENGTHENED GLASS ARTICLE AND MANUFACTURING METHOD THEREOF

    公开(公告)号:US20220289625A1

    公开(公告)日:2022-09-15

    申请号:US17805031

    申请日:2022-06-02

    Applicant: AGC Inc.

    Abstract: The present invention relates to a chemically strengthened glass article in which a compressive stress value on a first surface is 400 MPa or more, with a glass thickness of t (μm), the compressive stress value at the depth DB where the compressive stress value is maximum in the range where the depth from the first surface is (0.05×t)-(0.15×t) μm is larger than the compressive stress value at the depth DA where the compressive stress value is minimum in the range from the first surface to the depth DB, the tensile stress value at a depth (0.5×t) μm from the first surface is 125 MPa or less, and a compressive stress layer depth is (0.23×t) μm or more.

    GLASS, CRYSTALLIZED GLASS AND CHEMICALLY STRENGTHENED GLASS

    公开(公告)号:US20230082423A1

    公开(公告)日:2023-03-16

    申请号:US18053820

    申请日:2022-11-09

    Applicant: AGC Inc.

    Abstract: The present invention relates to a glass including, in terms of mole percentage based on oxides: 50.0 to 75.0% of SiO2; 7.5 to 25.0% of Al2O3; 0 to 25.0% of B2O3; 6.5 to 20.0% of Li2O; 1.5 to 10.0% of Na2O; 0 to 4.0% of K2O; 1.0 to 20.0% of MgO; one or more components selected from MgO, CaO, SrO, and BaO in a total amount of 1.0 to 20.0%; and 0 to 5.0% of TiO2, in which a value of Y calculated based on the following formula is 19.5 or less, Y=1.2×([MgO]+[CaO]+[SrO]+[BaO])+1.6×([Li2O]+[Na2O]+[K2O]), provided that [MgO], [CaO], [SrO], [BaO], [Li2O], [Na2O], and [K2O] are contents, in terms of mole percentage based on oxides, of components of MgO, CaO, SrO, BaO, Li2O, Na2O, and K2O respectively.

    GLASS FOR CHEMICAL STRENGTHENING
    5.
    发明申请

    公开(公告)号:US20200325066A1

    公开(公告)日:2020-10-15

    申请号:US16911878

    申请日:2020-06-25

    Applicant: AGC Inc.

    Abstract: The present invention relates to a glass for chemical strengthening including, in mole percentage on an oxide basis: 45 to 75% of SiO2; 1 to 30% of Al2O3; 1 to 20% of Li2O; 0 to 5% of Y2O3; 0 to 5% of ZrO2; and 0 to 1% of TiO2, having a total content of one or more kinds of MgO, CaO, SrO, BaO and ZnO of 1 to 20%, having a total content of Na2O and K2O of 0 to 10%, having a total content of B2O3 and P2O5 of 0 to 10%, and having a value M expressed by the following expression of 1,000 or more: M=−5×[SiO2]+121×[Al2O3]+50×[Li2O]−35×[Na2O]+32×[K2O]+85×[MgO]+54×[CaO]−41×[Sr O]−4×[P2O5]+218×[Y2O3]+436×[ZrO2]−1180, in which each of [SiO2], [Al2O3], [Li2O], [Na2O], [K2O], [MgO], [CaO], [SrO], [P2O5], [Y2O3], and [ZrO2] designates a content of each component in mole percentage on an oxide basis.