摘要:
A white glass includes, in terms of mole percentage on the basis of oxides, from 50% to 74% of SiO2, from 0 to 8% of B2O3, from 1% to 8% of Al2O3, from 0 to 18% of MgO, from 0 to 7% of CaO, from 0 to 10% of SrO, from 0 to 12% of BaO, from 0 to 5% of ZrO2, from 5% to 15% of Na2O and from 2% to 10% of P2O5. In the white glass, a total content of CaO, SrO and BaO is from 1% to 22%, a total content RO of MgO, CaO, SrO and BaO is from 5% to 25% and a ratio CaO/RO of a content of CaO to the RO is 0.7 or less.
摘要:
A glass sheet includes, as represented by mole percentage based on oxides, from 55.5 to 80% of SiO2, from 12 to 20% of Al2O3, from 8 to 25% of Na2O, 2.5% or more of P2O5, and 1% or more of an alkaline earth metal RO (RO is MgO+CaO+SrO+BaO).
摘要:
The present invention relates to a method for producing phase-separated glass, sequentially including a melting step of melting a glass, a phase separation step of separating phases in the glass, and a shaping step of shaping the glass, and to the phase-separated glass obtained by the production method.
摘要:
An object of the present invention is to provide a glass for chemical strengthening which is capable of improving strength as compared with an ordinary soda lime silicate glass even when the same chemical strengthening treatment as that in a conventional process is applied and has good devitrification characteristics, a chemically strengthened glass using the glass for chemical strengthening, and a method for producing the chemically strengthened glass. The present invention provides a glass for chemical strengthening having a specific glass composition described in the present specification.
摘要:
A phase-separated glass for chemical strengthening has a total light reflectance of 10% or more in a wavelength range of 380 nm to 780 nm and a value obtained by dividing a maximum value of the total light reflectance by a minimum value of the total light reflectance of more than 4.2, when measured in a form of a plate having a thickness of 1 mm.
摘要:
An object is to provide a glass for chemical toughening treatment satisfying low brittleness, low melt viscosity and high chemical toughening characteristics, and a chemically toughened glass using the same. Provided is a glass for chemical toughening treatment containing, in mass % in terms of oxides, SiO2 63 to 76, B2O3 0 to 2, Al2O3 2 to 10, MgO 2 to 12, CaO 0.1 to 8, Na2O 14.5 to 19, K2O 0 to 3, and Fe2O3 0 to 0.5, satisfying a total content of alkali earth metal oxides (RO) being from 5 to 15, satisfying 15×MgO/RO−RO≥3, and having a temperature T2 at which a glass viscosity reaches 102 dPa·s being 1,600° C. or lower.
摘要:
A glass for chemical strengthening contains, in mole percentage on an oxide basis, 58 to 72% of SiO2, 7 to 18% of Al2O3, 1% or more of B2O3, 0 to 4% of P2O5, 5 to 16% of Li2O, 0 to 7% of Na2O, 0 to 2% of K2O, 0 to 6% of MgO, 0 to 20% of CaO, 0 to 20% of SrO, 0 to 15% of BaO, 0 to 10% of ZnO, 0 to 1% of TiO2, and 0 to 2% of ZrO2. A value of X is 30000 or more. The value of X is calculated based on the formula, X=SiO2×329+Al2O3×786+B2O3×627+P2O5×(−941)+Li2O×927+Na2O×47.5+K2O×(−371)+MgO×1230+CaO×1154+SrO×733+ZrO2×51.8, by using the contents in mole percentage on an oxide basis of components.
摘要:
A phase-separated glass for chemical strengthening has a total light reflectance of 10% or more in a wavelength range of 380 nm to 780 nm and a value obtained by dividing a maximum value of the total light reflectance by a minimum value of the total light reflectance of 4.2 or less, when measured in a form of a plate having a thickness of 1 mm.
摘要:
The present invention provides a cover glass for a display, having high durability to slow cracking and strong abraded strength even though a compressive stress is large and a depth of a compressive stress layer is deep. The present invention relates to a cover glass for a display, in which a depth of a compressive stress layer (DOL) is 30 μm or more, a surface compressive stress is 300 MPa or more, a position (HW) at which a compressive stress is half of a value of the surface compressive stress is a position of 8 μm or more from a glass surface, and the depth of the compressive stress layer (DOL) and the position (HW) at which the compressive stress is half of the value of the surface compressive stress satisfy the following formula: 0.05≦HW/DOL≦0.23 (1).
摘要:
The present invention provides a cover glass for a display, having high durability to slow cracking and strong abraded strength even though a compressive stress is large and a depth of a compressive stress layer is deep. The present invention relates to a cover glass for a display, in which a depth of a compressive stress layer (DOL) is 30 μm or more, a surface compressive stress is 300 MPa or more, a position (HW) at which a compressive stress is half of a value of the surface compressive stress is a position of 8 μm or more from a glass surface, and the depth of the compressive stress layer (DOL) and the position (HW) at which the compressive stress is half of the value of the surface compressive stress satisfy the following formula: 0.05≦HW/DOL≦0.23 (1).