Method for manufacturing an elastic body of Al2O3 ceramic, measuring membrane for a pressure sensor and pressure sensor with such a membrane
    4.
    发明授权
    Method for manufacturing an elastic body of Al2O3 ceramic, measuring membrane for a pressure sensor and pressure sensor with such a membrane 有权
    制造Al2O3陶瓷弹性体的方法,用于压力传感器的测量膜和具有这种膜的压力传感器

    公开(公告)号:US08485042B2

    公开(公告)日:2013-07-16

    申请号:US13057487

    申请日:2009-06-23

    IPC分类号: G01L7/08

    摘要: A method for manufacturing an elastic deformation body made of an Al2O3 ceramic according to which a highly pure alumina having at most 2000 ppm MgO, at most 200 ppm inorganic impurities, a specific surface of at least 10 m2/g, an average grain size of at most 0.3 μm is applied. With the alumina and additives, there is produced via aqueous processing a homogeneous mixture, from which a pressable spray granulate is produced, which is formed by means of a uniaxial pressing method to a homogeneous, green body, which is subjected to a sinter process. The resulting elastic deformation body has a bending fracture stress σc, whose distribution F(σc) is given by the Weibull parameters σ0≧800 MPa and m≧24, with an average grain size of the sintered material of no more than 2 μm, and wherein the sintered material of the deformation body has a density of not less than 3.98 g/cm3.

    摘要翻译: 一种制造由Al 2 O 3陶瓷制成的弹性变形体的方法,根据该方法制备具有至多2000ppm MgO,至多200ppm无机杂质,比表面积至少为10m 2 / g的高纯氧化铝,平均粒径为 施加0.3μm以下。 使用氧化铝和添加剂,通过水性加工生产均匀的混合物,通过单轴压制方法制备可挤压的喷雾颗粒,该均匀的混合物经受烧结过程的均匀的生坯。 所得到的弹性变形体具有弯曲断裂应力sigmac,其分布F(sigmac)由威布尔参数σ= 800MPa和m = 24给出,烧结材料的平均粒径不大于2μm 所述变形体的烧结体的密度为3.98g / cm 3以上。