COLD ROLLED STEEL SHEET AND A METHOD OF MANUFACTURING THEREOF

    公开(公告)号:US20210002740A1

    公开(公告)日:2021-01-07

    申请号:US16761417

    申请日:2018-11-05

    Applicant: ArcelorMittal

    Abstract: A cold rolled heat treated steel sheet having a composition with the following elements, expressed in percentage by weight 0.1%≤Carbon≤0.5%, 1%≤Manganese≤3.4%, 0.5%≤Silicon≤2.5%, 0.03%≤Aluminum≤1.5%, 0%≤Sulfur≤0.003%, 0.002%≤Phosphorus≤0.02%, 0%≤Nitrogen≤0.01% and can contain one or more of the following optional elements 0.05%≤Chromium≤1%, 0.001%≤Molybdenum≤0.5%, 0.001%≤Niobium≤0.1%, 0.001%≤Titanium≤0.1%, 0.01%≤Copper≤2%, 0.01%≤Nickel≤3%, 0.0001%≤Calcium≤0.005%, 0%≤Vanadium≤0.1%, 0%≤Boron≤0.003%, 0%≤Cerium≤0.1%, 0%≤Magnesium≤0.010%, 0%≤Zirconium≤0.010%, the remainder composition being composed of iron and unavoidable impurities caused by processing, the microstructure of the steel sheet having in area fraction, 10 to 30% Residual Austenite, 50 to 85% Bainite, 1 to 20% Quenched Martensite, and less than 30% Tempered Martensite.

    COLD ROLLED HEAT TREATED STEEL SHEET AND A METHOD OF MANUFACTURING THEREOF

    公开(公告)号:US20210207236A1

    公开(公告)日:2021-07-08

    申请号:US16761319

    申请日:2018-11-05

    Applicant: ArcelorMittal

    Abstract: A cold rolled and heat treated steel sheet having a composition with the following elements, expressed in percentage by weight: 0.10%≤Carbon≤0.5%,1%≤Manganese≤3.4%, 0.5%≤Silicon≤2.5%, 0.03%≤Aluminum≤1.5%, 0%≤Sulfur≤0.003% 0.002%≤Phosphorus≤0.02%, 0%≤Nitrogen≤0.01% and can contain one or more of the following optional elements 0.05%≤Chromium≤1%, 0.001%≤Molybdenum≤0. 5%, 0.001%≤Niobium≤0.1%, 0.001%≤Titanium≤0.1%, 0.01%≤Copper≤2%, 0.01%≤Nickel≤3%, 0.0001%≤Calcium≤0.005%, 0%≤Vanadium≤0.1%, 0%≤Boron≤0.003%, 0%≤Cerium≤0.1%, 0%≤Magnesium≤0.010%, 0%≤Zirconium≤0.010% the remainder composition being composed of iron and unavoidable impurities caused by processing, the microstructure of the steel sheet having in area fraction, 10 to 30% Residual Austenite, 10 to 40% Bainite, 5% to 50% Annealed Martensite, 1% to 20% Quenched Martensite and less than 30% Tempered Martensite, wherein the cumulated amounts of Bainite and Residual Austenite is more than or equal to 25%.

Patent Agency Ranking