    Abstract: A 1-butene copolymer composition made from or containing:



    A) from 75.0 wt % to 95.0 wt % of a polymer composition (A) made from or containing
    A1) from 56 wt % to 77 wt % of a propylene ethylene copolymer;
    A2) from 15 wt % to 32 wt % of a low density polyethylene; and
    A3) from 4 wt % to 17 wt % of a 1-butene homopolymer,

    wherein the sum of the amounts of A1, A2, and A3 being 100 wt %; and

    B) from 5.0 wt % to 25.0 wt % of a copolymer of 1-butene and ethylene containing from 2.8 wt % to 4.2 wt % of ethylene derived units, based upon the total weight of the copolymer of 1-butene and ethylene,

    wherein the sum of the amounts of A) and B) being 100 wt %.

    Soft polyolefin composition
    2.
    发明授权

    公开(公告)号:US10793655B2

    公开(公告)日:2020-10-06

    申请号:US16087731

    申请日:2017-03-23

    Abstract: The present disclosure provides a polyolefin composition made from or containing: A) from about 60 to about 89% by weight based upon the total weight of the polyolefin composition of a copolymer of butene-1 with ethylene having a copolymerized ethylene content of up to about 18% by mole based upon the molar composition of the copolymer, and no melting peak detectable at the DSC at the second heating scan; and B) from about 11 to about 40% by weight based upon the total weight of the polyolefin composition of an ethylene polymer having density of from about 0.900 to about 0.970 g/cm3, measured according to ISO 1183 at 23° C.; wherein the amounts of A) and B) are referred to the total weight of A)+B) and the DSC second heating scan is carried out with a heating rate of 10° C. per minute. The composition is useful for preparing gaskets.

    POLYOLEFIN FILAMENT
    5.
    发明申请

    公开(公告)号:US20250051973A1

    公开(公告)日:2025-02-13

    申请号:US18717910

    申请日:2022-12-05

    Abstract: A stretched polyolefin filament, having elongation at break EB of equal to or higher than 80% and a ratio SR/EB, where SR is the stretching ratio, of equal to or lower than 45, made from or containing: a polyolefin composition (I), made from or containing A) from 40% to 78% by weight of a propylene polymer; B) from 22% to 60% by weight of a butene-1 polymer having: 1) a flexural modulus value from 100 to 800 MPa; 2) a ratio MI10/MI2 of from 20 to 40; and 3) a content of fraction soluble in xylene at 0° C. of 15% by weight or lower; wherein the amounts of A) and B) are referred to the total weight of A)+B).

    POLYOLEFIN FILAMENT
    6.
    发明申请

    公开(公告)号:US20250043464A1

    公开(公告)日:2025-02-06

    申请号:US18717886

    申请日:2022-12-05

    Abstract: A stretched polyolefin filament, having elongation at break EB of equal to or higher than 90% and a ratio SR/EB, where SR is the stretching ratio, of equal to or lower than 75, made from or containing: a polyolefin composition (I), made from or containing A) from 80% to 95% by weight of a propylene polymer; B) from 5% to 20% by weight of a butene-1 polymer having: 1) a flexural modulus value from 100 to 800 MPa; 2) a ratio MI10/MI2 of from 20 to 40; and 3) a content of fraction soluble in xylene at 0° C. of 15% by weight or lower; wherein the amounts of A) and B) are referred to the total weight of A)+B).

    Soft and flexible polyolefin composition

    公开(公告)号:US10214640B2

    公开(公告)日:2019-02-26

    申请号:US15536052

    申请日:2015-11-17

    Abstract: The present disclosure provides a polyolefin composition made from or containing: A) from about 63 to about 78% by weight of a copolymer of butene-1 with ethylene having a copolymerized ethylene content of up to about 18% by mole and no melting peak detectable at the DSC at the second heating scan; B) from about 22 to about 37% by weight of (i) a propylene homopolymer, or (ii) a propylene copolymer, or (iii) a mixture of two or more of (i) and (ii), having a melting temperature Tm, measured by DSC at the second heating scan, of from about 130° C. to about 165° C.; wherein (i) the amounts of A) and B) are referred to the total weight of A)+B) and (ii) having a melting enthalpy ΔHfus, measured by DSC at the second heating scan, of from 7 to 30 J/g.

Patent Agency Ranking