PROCESS FOR MAKING AN ELECTRODE ACTIVE MATERIAL

    公开(公告)号:US20200274159A1

    公开(公告)日:2020-08-27

    申请号:US16646641

    申请日:2018-09-10

    Applicant: BASF SE

    Abstract: Process for making an electrode active material according to general formula Li1+xTM1−xO2, wherein TM is a combination of Mn, Co and Ni, optionally in combination with at least one more metal selected from Al, Ti, and W, wherein at least 50 mole-% of TM is Ni, and x is in the range of from zero to 0.2, said process comprising the following steps: (a) mixing (A) a mixed oxide or oxyhydroxide or hydroxide of TM, and (B) at least one lithium compound selected from lithium hydroxide, lithium oxide and lithium carbonate, and so that the molar ratio of Li to TM is in the range of from 0.70 to 0.97. (b) Subjecting said mixture to heat treatment at a temperature in the range of from 300 to 900° C., (c) Mixing with at least one lithium compound (B), so that the total molar ratio of Li to TM is in the range of from 1.0 to 1.1, (d) Subjecting said mixture to heat treatment at a temperature in the range of from 700 to 1000° C.

    PROCESS FOR MAKING AN ELECTRODE ACTIVE MATERIAL

    公开(公告)号:US20200161652A1

    公开(公告)日:2020-05-21

    申请号:US16627884

    申请日:2018-07-05

    Applicant: BASF SE

    Abstract: Process for making an electrode active material according to general formula Li1+χTM1−χO2, wherein TM is a combination of Mn, Co and Ni in combination with at least one more metal selected from Al, Ti, and W, wherein at least 60 mole-% of TM is Ni, the percentage referring to the sum of Ni, Co and Mn, and x is in the range of from zero to 0.2, said process comprising the following steps: (a) mixing (A) a mixed oxide or oxyhydroxide of Mn, Co and Ni, (B) at least one lithium compound selected from lithium hydroxide, lithium oxide and lithium carbonate, and (C) an oxide, hydroxide or oxyhydroxide of Al, Ti or W, (b) Subjecting said mixture to heat treatment at a temperature in the range of from 700 to 1000° C.

Patent Agency Ranking