METHOD FOR PROCESSING NI-RICH ELECTRODE ACTIVE MATERIALS

    公开(公告)号:US20210376318A1

    公开(公告)日:2021-12-02

    申请号:US17254559

    申请日:2019-06-17

    Applicant: BASF SE

    Abstract: Process for modifying an electrode active material according to general formula Li1+xTM1−xO2, wherein TM contains a combination of Ni and at least one transition metal selected from Co and Mn, and, optionally, at least one metal selected from Al, Ba, and Mg and, optionally, one or more transition metals other than Ni, Co, and Mn, wherein at least 75 mole-% of TM is Ni, and x is in the range of from −0.05 to 0.2, said process comprising the steps of (a) treating said Li1+xTM1−xO2 with an aqueous medium with a pH value of at least 5 and up to 14, (b) removing said aqueous medium from treated Li1+xTM1−xO2 by way of a solid-liquid separation, wherein steps (a) and (b) are commenced with a maximum time difference of 3 minutes. In addition, the present invention is directed towards Ni-rich electrode active materials.

    PROCESS FOR MAKING AN ELECTRODE ACTIVE MATERIAL

    公开(公告)号:US20200161652A1

    公开(公告)日:2020-05-21

    申请号:US16627884

    申请日:2018-07-05

    Applicant: BASF SE

    Abstract: Process for making an electrode active material according to general formula Li1+χTM1−χO2, wherein TM is a combination of Mn, Co and Ni in combination with at least one more metal selected from Al, Ti, and W, wherein at least 60 mole-% of TM is Ni, the percentage referring to the sum of Ni, Co and Mn, and x is in the range of from zero to 0.2, said process comprising the following steps: (a) mixing (A) a mixed oxide or oxyhydroxide of Mn, Co and Ni, (B) at least one lithium compound selected from lithium hydroxide, lithium oxide and lithium carbonate, and (C) an oxide, hydroxide or oxyhydroxide of Al, Ti or W, (b) Subjecting said mixture to heat treatment at a temperature in the range of from 700 to 1000° C.

    PROCESS FOR MAKING A COATED CATHODE ACTIVE MATERIAL

    公开(公告)号:US20230406724A1

    公开(公告)日:2023-12-21

    申请号:US18248461

    申请日:2021-10-12

    Applicant: BASF SE

    CPC classification number: C01G53/50 H01M10/0525 C01P2006/40 C01P2004/61

    Abstract: Described herein is a process for making an electrode active material according to general formula Li1+(TM1-yM1y)1-xO2, where TM includes a combination of Ni and at least one of Co, Mn and Al, M1 is selected from the group consisting of Nb, Ta, and at least one of Co, Mn and Al, y is in a range of from 0.001 to less than 0.01, and x is in a range of from zero to 0.2, said process including the following steps:



    (a) mixing

    (A) a mixed oxide or (oxy)hydroxide of Mn, Co and Ni, and
    (B) at least one lithium compound selected from the group consisting of lithium hydroxide, lithium oxide and lithium carbonate, and
    (C) an amorphous compound of Nb or Ta, and


    (b) subjecting said mixture to heat treatment,
    where at least 60 mole-% of a transition metal of TM is Ni.

    PROCESS FOR MAKING AN ELECTRODE ACTIVE MATERIAL

    公开(公告)号:US20220098053A1

    公开(公告)日:2022-03-31

    申请号:US17310023

    申请日:2020-01-06

    Applicant: BASF SE

    Abstract: Process for making an electrode active material according to general formula Li1+xTM1−xO2, wherein TM is a combination of Ni and Co and Zr and at least one metal selected from Mn and Al, and, optionally, at least one of Mg, Ti, and W, wherein GC at least 60 mole-% is Ni, referring to the sum of Ni, Co and, if applicable, Mn and Al, and x is in the range of from zero to 0.2, said process comprising the following steps: (a) mixing (A) a mixed oxide or oxyhydroxide of Ni, Co and, if applicable, Mn, (B) at least one lithium compound selected from lithium hydroxide, lithium oxide and lithium carbonate, and (C) at least one oxide or hydroxide or oxyhydroxide of Zr with an average diameter D50 in the range of from 1 to 7 μm, and in compounds (C) that are selected from oxides of Zr, their crystallite size is in the range of from 5 to 20 nm and (b) Subjecting said mixture to heat treatment at a temperature in the range of from 700 to 1000° C.

    PROCESS FOR MAKING A COATED OXIDE MATERIAL

    公开(公告)号:US20210399291A1

    公开(公告)日:2021-12-23

    申请号:US17309205

    申请日:2019-11-11

    Applicant: BASF SE

    Abstract: Process for making a coated oxide material wherein said process comprises the following steps: (a) providing a particulate material selected from lithiated nickel-cobalt aluminum oxides, lithium cobalt oxide, lithiated cobalt-manganese oxides and lithiated layered nickel-cobalt-manganese oxides, (b) treating said particulate material with an aqueous medium, (c) removing said aqueous medium, (d) drying said treated particulate material, (e) treating said particulate material from step (d) with a metal amide or alkyl metal compound, (f) treating the material obtained in step (e) with moisture or an oxidizing agent, and, optionally, repeating the sequence of steps (e) and (f).