PROCESS FOR MAKING AN ELECTRODE ACTIVE MATERIAL, AND ELECTRODE ACTIVE MATERIAL

    公开(公告)号:US20230002242A1

    公开(公告)日:2023-01-05

    申请号:US17758742

    申请日:2021-02-18

    Abstract: Process for making an electrode active material wherein said process comprises the following steps: (a) Providing a hydroxide TM(OH)2 or at least one oxide TMO or oxyhydroxide of TM or combination of at least two of the foregoing wherein TM contains at least 99 mol-% Ni and, optionally, in total up to 1 mol-% of at least one metal selected from Ti, Zr, V, Co, Zn, Ba, or Mg, (b) mixing said hydroxide TM(OH)2 or oxide TMO or oxyhydroxide of TM or combination with a source of lithium and an aqueous solution of a compound of Me wherein Me is selected from Al or Ga or a combination of the foregoing and wherein the molar amount of TM corresponds to the sum of Li and Me, (c) removing the water by evaporation, (d) treating the solid residue obtained from step (c) thermally at a temperature in the range of from 500 to 800° C. in the presence of oxygen.

    PROCESS FOR MAKING AN ELECTRODE ACTIVE MATERIAL

    公开(公告)号:US20220098053A1

    公开(公告)日:2022-03-31

    申请号:US17310023

    申请日:2020-01-06

    Applicant: BASF SE

    Abstract: Process for making an electrode active material according to general formula Li1+xTM1−xO2, wherein TM is a combination of Ni and Co and Zr and at least one metal selected from Mn and Al, and, optionally, at least one of Mg, Ti, and W, wherein GC at least 60 mole-% is Ni, referring to the sum of Ni, Co and, if applicable, Mn and Al, and x is in the range of from zero to 0.2, said process comprising the following steps: (a) mixing (A) a mixed oxide or oxyhydroxide of Ni, Co and, if applicable, Mn, (B) at least one lithium compound selected from lithium hydroxide, lithium oxide and lithium carbonate, and (C) at least one oxide or hydroxide or oxyhydroxide of Zr with an average diameter D50 in the range of from 1 to 7 μm, and in compounds (C) that are selected from oxides of Zr, their crystallite size is in the range of from 5 to 20 nm and (b) Subjecting said mixture to heat treatment at a temperature in the range of from 700 to 1000° C.

    PROCESS FOR MAKING A LITHIATED OXIDE

    公开(公告)号:US20230130367A1

    公开(公告)日:2023-04-27

    申请号:US17906270

    申请日:2021-04-01

    Abstract: Process for making a lithiated oxide, said process comprising the following steps: (a) making a particulate hydroxide, oxide or oxyhydroxide of nickel, and, optionally, at least one of Co and Mn and, by combining an aqueous solution of sodium or potassium hydrox-ide with an aqueous solution containing a water-soluble salt of nickel and, optionally, a water-soluble salt of Co, Mn, Al, Ti, Zr, W, Mo, Ga, Nb, Ta, or Mg, (b) adding a source of lithium, (c) treating the mixture obtained from step (b) thermally at at least two different temperatures: (c1) at 300 to 500° C. under an atmosphere that may comprise oxygen, (c2) at 500 to 600° C. under an atmosphere of oxygen, wherein the temperature in step (c2) is set to be higher than in step (c1).