公开(公告)号:US11746403B2
公开(公告)日:2023-09-05
申请号:US16054311
申请日:2018-08-03
发明人: Jochem Grewe , Feng Jiao , Friedrich Bohner , Jörn Tölle , Nikolay Soritov
CPC分类号: C22F1/05 , C21D9/0062 , C21D9/0068 , C22C21/04 , C22F1/002
摘要: A method for producing a motor vehicle component from a 6000 series aluminum alloy including providing a blank made of a 6000 series aluminum alloy, rapid heating of the blank to a temperature between 450 deg. C. and 600 deg. C. at a heating rate of more than 15 K/s in a period of less than 20 seconds, ending the heating process and optionally homogenizing, if a grain size between 20 and 50 μm has been produced, quenching the blank thus tempered, applying a lubricant, preferably at 20 deg. C. to 100 deg. C., forming the cooled blank in a forming tool, wherein the time between completion of the heating process and the start of the forming is less than 30 seconds, and aging.
-
公开(公告)号:US20150075246A1
公开(公告)日:2015-03-19
申请号:US14489014
申请日:2014-09-17
CPC分类号: B21K7/00 , B21D22/022 , B21D22/201 , B21D22/208 , B21D22/22 , B21D37/16 , C21D1/673 , C21D9/48 , C21D2221/00
摘要: A tool for hot forming and press hardening a steel structure includes an upper tool and a lower tool, each having a base body made of highly heat conductive material and comprised of at least two segments. The base body of at least one of the upper and lower tools has a cooling channel. Arranged on the base body of at least one of the upper and lower tools is a wear protection shield.
摘要翻译: 用于钢结构的热成型和加压硬化的工具包括上工具和下工具,每个具有由高导热材料制成并由至少两个段组成的基体。 上部和下部工具中的至少一个的基体具有冷却通道。 在上下工具中的至少一个上的基体上排列有防磨损护罩。
-
公开(公告)号:US09914491B2
公开(公告)日:2018-03-13
申请号:US14683734
申请日:2015-04-10
发明人: Friedrich Bohner , Jochen Doerr , Jochem Grewe , Christian Hielscher , Joern Toelle , Boris Rauscher
CPC分类号: B62D29/008 , B21D22/022 , B21D53/88 , C22C21/08 , C22F1/047
摘要: A method for producing a motor vehicle component, is disclosed having the steps of—providing a blank composed of a 5000 grade naturally hard aluminum alloy with an initial yield strength, completely heating the blank to a forming temperature between 150° C. and 350° C., preferably between 200° C. and 300° C. in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s, and performing forming in a forming tool in less than 20 s, preferably less than 10 s and in particular between 2 and 5 s, the temperature being held between 150° C. and 350° C. in at least one first region of the blank, and cooling to a temperature lower than 250° C., in particular lower than 200° C., being performed in a second region during or after the deformation.
-
公开(公告)号:US09821859B2
公开(公告)日:2017-11-21
申请号:US14683759
申请日:2015-04-10
发明人: Friedrich Bohner , Jochen Doerr , Jochem Grewe , Christian Hielscher , Joern Toelle , Boris Rauscher
IPC分类号: C22F1/04 , B62D29/00 , C22C21/00 , C21D9/46 , C21D1/673 , C22C21/06 , C22F1/047 , B21D22/02 , B21D53/88 , B21D35/00 , C21D8/02 , B62D25/04
CPC分类号: B62D29/008 , B21D22/022 , B21D35/006 , B21D53/88 , B62D25/04 , B62D29/001 , C21D1/673 , C21D8/0294 , C21D9/46 , C21D2221/00 , C22C21/00 , C22C21/06 , C22F1/04 , C22F1/047
摘要: A method for producing a motor vehicle component is disclosed having the steps of providing a strain-hardened blank composed of a 5000 grade aluminum alloy, partially heating the blank in a first region to a temperature higher than 350° C., in particular higher than 400° C., and in a second region to a temperature between 150° C. and 350° C., preferably to 300° C., in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s, and transferring the blank into a cooling tool, and performing cooling in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s.
-
公开(公告)号:US09938613B2
公开(公告)日:2018-04-10
申请号:US14683896
申请日:2015-04-10
发明人: Friedrich Bohner , Jochen Doerr , Jochem Grewe , Christian Hielscher , Joern Toelle , Boris Rauscher
CPC分类号: C22F1/047 , B62D29/008 , C22C21/08
摘要: A method for producing a motor vehicle component is disclosed having the steps of providing a strain-hardened blank composed of a 5000 grade aluminum alloy, partially heating the blank in a first region to a temperature higher than 350° C., in particular to 400° C., the blank being kept at a temperature between 15° C. and 30° C., preferably at 20° C., in a second region, and the partial heating being performed in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s, adjusting the temperature of the blank as a whole to between 150 and 350° C. in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s, and deforming the blank to form the motor vehicle component in less than 20 s, preferably less than 10 s and in particular in 2 to 5 s, and cooling the motor vehicle component.
-
公开(公告)号:US09719161B2
公开(公告)日:2017-08-01
申请号:US14683685
申请日:2015-04-10
发明人: Friedrich Bohner , Jochen Doerr , Jochem Grewe , Christian Hielscher , Joern Toelle , Boris Rauscher
IPC分类号: C22F1/04 , C22C21/02 , C22C21/10 , C22F1/05 , C22F1/053 , B62D29/00 , C22C21/00 , C22F1/00 , C22C21/08
CPC分类号: C22F1/04 , B62D29/008 , C22C21/00 , C22C21/02 , C22C21/08 , C22C21/10 , C22F1/002 , C22F1/05 , C22F1/053
摘要: A method for producing a motor vehicle component includes the steps of providing a precipitation-hardenable blank composed of a 6000 or 7000 grade aluminum alloy, solution-annealing the blank at a temperature between 350° C. and 550° C. for a time period of 2 to 30 min., in particular 3 to 20 min. and preferably 5 to 15 min., in particular at a temperature between 440° C. and 480° C. in the case of a 7000 grade aluminum alloy, and in particular at a temperature between 490° C. and 545° C. in the case of a 6000 grade aluminum alloy, subjecting the solution-annealed blank to partially different quenching, a first region being quenched to a temperature between 150° C. and 250° C., and a further region being quenched to a temperature below 150° C., deforming the blank during or after the partially different quenching.
-
-
-
-
-