Abstract:
The present invention is directed to a polypropylene composition (C) comprising a heterophasic propylene copolymer and an inorganic filler, the use of said polypropylene composition (C) for the production of a foamed article and a foamed article obtained from said polypropylene composition (C).
Abstract:
The present invention relates to novel polypropylene compositions suitable for automotive applications, having a good balance of mechanical properties and especially low gloss. The inventive compositions are characterized by at least two heterophasic propylene copolymers (HECOs), where at least one of the HECOs is characterized by a rather high molecular weight rubber, an ethylene-a-olefin elastomer (EOE) having a rather low melt flow rate MFR2 (190° C.) and a specific ratio between the MFR of the ethylene-a-olefin elastomer (EOE) and of at least one of the heterophasic propylene copolymers (HECOs).
Abstract:
Polyolefin composition comprising a heterophasic propylene copolymer and glass material, wherein said heterophasic propylene copolymer has • a xylene cold soluble fraction in the range of 25 to 50 wt.-%, and • a comonomer content in the range of 10.0 to 15.0 wt.-%, wherein further the xylene cold soluble fraction of the heterophasic propylene copolymer has a comonomer content in the range of 20 to 30 wt.-% and the polyolefin composition has a melt flow rate MFR2 (230° C.) of 2.0 to 15.0 g/10 min.
Abstract:
The invention relates to a novel polyolefin composition having a reduced occurrence of flow marks especially at high injection speeds. The novel polyolefin compositions comprise a heterophasic polypropylene composition, ethylene/propylene elastomer and an inorganic filler.
Abstract:
Tiger stripe modifier being a heterophasic polypropylene composition having a melt flow rate MFR2 (230° C.) in the range of 0.5 to 20 g/10 min and comprises a propylene homopolymer and an elastomeric propylene copolymer, wherein said propylene homopolymer has a melt flow rate MFR2 (230° C.) in the range of above 10 to 300 g/10 min; the xylene cold soluble fraction of the heterophasic polypropylene composition has an intrinsic viscosity in the range of more than 2.5 to below 11.0 dl/g; and the comonomer content of the xylene cold soluble fraction of the heterophasic polypropylene composition is in the range of 10.0 to 25.0 wt.-%; wherein further the heterophasic polypropylene composition fulfills the inequation (I) 0.3≧(0.241×C)-(1.14×IV) (I) wherein C is the comonomer content of the xylene cold soluble (XCS) fraction of the heterophasic polypropylene composition (HECO1), and IV is the intrinsic viscosity of the xylene cold soluble (XCS) fraction of the heterophasic polypropylene composition (HECO1).
Abstract:
The present invention is directed to a polypropylene composition (C) comprising a heterophasic propylene copolymer and an inorganic filler, the use of said polypropylene composition (C) for the production of a foamed article and a foamed article obtained from said polypropylene composition (C).
Abstract:
Polyolefin composition comprising a heterophasic propylene copolymer and glass material, wherein said heterophasic propylene copolymer has • a xylene cold soluble fraction in the range of 25 to 50 wt.-%, and • a comonomer content in the range of 10.0 to 15.0 wt.-%, wherein further the xylene cold soluble fraction of the heterophasic propylene copolymer has a comonomer content in the range of 20 to 30 wt.-% and the polyolefin composition has a melt flow rate MFR2 (230° C.) of 2.0 to 15.0 g/10 min.