公开(公告)号:US11965052B2
公开(公告)日:2024-04-23
申请号:US18111025
申请日:2023-02-17
Applicant: BOREALIS AG
Inventor: Irfan Saeed , Esa Kokko , Mika Salo , Sanjay Rastogi , Dario Romano , Sara Ronca
CPC classification number: C08F4/6492 , C08F2/001 , C08F4/025 , C08F4/6546 , C08F4/6555 , C08F110/02 , C08L23/06 , C08F2500/01 , C08F2500/12 , C08F2500/26 , C08F2500/34 , C08F2500/35 , C08L2203/16 , C08L2207/068 , C08L2314/02
Abstract: A process for the preparation of an ultra-high molecular weight ethylene homopolymer having a MFR21 of 0.01 g/10 min or less, said process comprising:
(I) prepolymerising at least ethylene at a temperature of 0 to 90° C. in the presence of a heterogeneous Ziegler Natta catalyst to prepare an ethylene prepolymer having an Mw of 40,000 to 600,000 g/mol; and thereafter in the presence of the prepolymer and said catalyst;
(II) polymerising ethylene at a temperature of 55° C. or less, such as 20 to 55° C., to prepare said UHMW ethylene homopolymer;
wherein the UHMW ethylene homopolymer comprises up to 8 wt. % of said prepolymer.-
公开(公告)号:US11680114B2
公开(公告)日:2023-06-20
申请号:US17261317
申请日:2019-07-18
Applicant: BOREALIS AG
Inventor: Irfan Saeed , Esa Kokko , Mika Salo , Sanjay Rastogi , Dario Romano , Sara Ronca
CPC classification number: C08F4/6492 , C08F4/025 , C08F4/6546 , C08F4/6555 , C08F110/02 , C08L23/06 , C08F2500/01 , C08F2500/12 , C08F2500/26 , C08F2500/34 , C08F2500/35 , C08L2203/16 , C08L2207/068
Abstract: A process for the preparation of an ultra-high molecular weight ethylene homopolymer having a MFR21 of 0.01 g/10 min or less, said process comprising: (I) prepolymerising at least ethylene at a temperature of 0 to 90° C. in the presence of a heterogeneous Ziegler Natta catalyst to prepare an ethylene prepolymer having an Mw of 40,000 to 600,000 g/mol; and thereafter in the presence of the prepolymer and said catalyst; (II) polymerising ethylene at a temperature of 55° C. or less, such as 20 to 55° C., to prepare said UHMW ethylene homopolymer; wherein the UHMW ethylene homopolymer comprises up to 8 wt. % of said prepolymer.
-