公开(公告)号:US09324998B2
公开(公告)日:2016-04-26
申请号:US13882501
申请日:2011-10-24
IPC分类号: H01M4/36 , H01M4/04 , H01M4/1391 , H01M4/13915 , H01M4/139 , H01M10/0525
CPC分类号: H01M4/364 , H01M4/0402 , H01M4/0404 , H01M4/0435 , H01M4/0471 , H01M4/131 , H01M4/136 , H01M4/139 , H01M4/1391 , H01M4/13915 , H01M4/485 , H01M4/505 , H01M4/525 , H01M4/5825 , H01M4/62 , H01M4/621 , H01M4/623 , H01M10/0525 , H01M10/058 , Y02E60/122 , Y02P70/54 , Y10T29/49115
摘要: The present invention relates to a method for manufacturing slurry for coating of electrodes for use in lithium ion batteries, wherein the method comprises mixing active materials with a binder into a binder solution, and adding an organic carbonate to the binder solution to generate the slurry. The present invention also relates to a method for manufacturing electrodes for a lithium battery cell, wherein the method comprises mixing active materials with a binder into a binder solution, adding an organic carbonate to the binder solution to generate slurry, wherein the above adding step is carried out at temperature above melting temperature of the organic carbonate, coating electrode material with the slurry, drying the coating on the electrode material by drying the organic carbonate, and surface treatment of the slurry so that the electrode is prepared for use in a lithium ion battery cell. Further, the invention also relates to a method for manufacturing a lithium ion battery cell.
摘要翻译: 本发明涉及一种用于制造用于锂离子电池的电极涂覆用浆料的方法,其中所述方法包括将活性材料与粘合剂混合到粘合剂溶液中,并将有机碳酸酯加入到粘合剂溶液中以产生浆料。 本发明还涉及一种用于制造锂电池电池的电极的方法,其中所述方法包括将活性材料与粘合剂混合到粘合剂溶液中,向粘合剂溶液中加入有机碳酸盐以产生浆料,其中上述添加步骤为 在有机碳酸酯的熔点以上的温度下进行,用浆料涂布电极材料,通过干燥有机碳酸酯干燥电极材料上的涂层,并对浆料进行表面处理,使得电极准备用于锂离子 电池单元 此外,本发明还涉及锂离子电池单元的制造方法。
-
公开(公告)号:US20130219704A1
公开(公告)日:2013-08-29
申请号:US13882501
申请日:2010-10-28
IPC分类号: H01M4/36 , H01M4/04 , H01M10/0525
摘要: The present invention relates to a method for manufacturing slurry for coating of electrodes for use in lithium ion batteries, wherein the method comprises mixing active materials with a binder into a binder solution, and adding an organic carbonate to the binder solution to generate the slurry. The present invention also relates to a method for manufacturing electrodes for a lithium battery cell, wherein the method comprises mixing active materials with a binder into a binder solution, adding an organic carbonate to the binder solution to generate slurry, wherein the above adding step is carried out at temperature above melting temperature of the organic carbonate, coating electrode material with the slurry, drying the coating on the electrode material by drying the organic carbonate, and surface treatment of the slurry so that the electrode is prepared for use in a lithium ion battery cell. Further, the invention also relates to a method for manufacturing a lithium ion battery cell.
摘要翻译: 本发明涉及一种用于制造用于锂离子电池的电极涂覆用浆料的方法,其中所述方法包括将活性材料与粘合剂混合到粘合剂溶液中,并将有机碳酸酯加入到粘合剂溶液中以产生浆料。 本发明还涉及一种用于制造锂电池电池的电极的方法,其中所述方法包括将活性材料与粘合剂混合到粘合剂溶液中,向粘合剂溶液中加入有机碳酸盐以产生浆料,其中上述添加步骤为 在有机碳酸酯的熔点以上的温度下进行,用浆料涂布电极材料,通过干燥有机碳酸酯干燥电极材料上的涂层,并对浆料进行表面处理,使得电极准备用于锂离子 电池单元 此外,本发明还涉及锂离子电池单元的制造方法。
-
公开(公告)号:US06444193B1
公开(公告)日:2002-09-03
申请号:US09503082
申请日:2000-02-14
申请人: Tore Omtveit , Bjorn Haugseter , Tony Pete
发明人: Tore Omtveit , Bjorn Haugseter , Tony Pete
IPC分类号: A61K4900
CPC分类号: B01F7/00766 , B01F7/00633 , B01F13/1016 , B01F2005/0005 , C02F3/08 , Y02W10/15
摘要: The invention provides a process for the preparation of gas-containing vesicles wherein a mixture of gas, liquid and vesicle membrane forming material is passed through a zone in which it is subject to shear forces exerted by surfaces moving relative to each other at a speed of at least 20 m/s.
摘要翻译: 本发明提供了一种制备含气泡囊的方法,其中气体,液体和囊泡膜形成材料的混合物通过其受到由相对于彼此移动的表面施加的剪切力的区域的速度 至少20米/秒。
-
-