公开(公告)号:US20130165621A1
公开(公告)日:2013-06-27
申请号:US13707775
申请日:2012-12-07
发明人: Tomomich Kanda , Shimoda Tomoaki , Bok Nam Jang , Seung Hyun Jang
IPC分类号: C08F2/36
CPC分类号: C08F2/36 , C08G63/605 , C08G63/80 , C08G64/307 , C08G69/265 , C08G69/30
摘要: Disclosed herein is a method for preparing a polycondensation resin. The method includes preparing a low degree condensate; and solid phase polymerizing the low degree condensate, wherein a granular molded article is introduced into the solid phase polymerization. The method enables efficient manufacture of high quality resins without problems such as agglomeration or scaling of a low degree condensate in pipes.
摘要翻译: 本文公开了一种制备缩聚树脂的方法。 该方法包括制备低度冷凝物; 并将低级缩合物固相聚合,其中将粒状模制品引入固相聚合中。 该方法能够有效地制造高质量的树脂而没有问题,例如管道中的低度冷凝物的聚集或结垢。
-
公开(公告)号:US09029482B2
公开(公告)日:2015-05-12
申请号:US13707775
申请日:2012-12-07
发明人: Tomomich Kanda , Shimoda Tomoaki , Bok Nam Jang , Seung Hyun Jang
CPC分类号: C08F2/36 , C08G63/605 , C08G63/80 , C08G64/307 , C08G69/265 , C08G69/30
摘要: Disclosed herein is a method for preparing a polycondensation resin. The method includes preparing a low degree condensate; and solid phase polymerizing the low degree condensate, wherein a granular molded article is introduced into the solid phase polymerization. The method enables efficient manufacture of high quality resins without problems such as agglomeration or scaling of a low degree condensate in pipes.
摘要翻译: 本文公开了一种制备缩聚树脂的方法。 该方法包括制备低度冷凝物; 并将低级缩合物固相聚合,其中将粒状模制品引入固相聚合中。 该方法能够有效地制造高质量的树脂而没有问题,例如管道中的低度冷凝物的聚集或结垢。
-
公开(公告)号:US09840587B2
公开(公告)日:2017-12-12
申请号:US14437523
申请日:2013-10-23
发明人: Tomomich Kanda , Tomoaki Shimoda
CPC分类号: C08G69/30 , C08G69/26 , C08G69/265 , C08G69/28 , C08G69/46
摘要: The polyamide production method of the present invention comprises the steps of: producing a low-order condensate by effecting a polycondensation reaction between a dicarboxylic acid component containing between about 5 and about 40 mol. % of terephthalic acid, and a diamine component containing between about 70 and about 100 mol. % of a xylylenediamine in which the content of paraxylylenediamine is between about 50 and about 100 mol. %, under conditions of a reaction temperature of at least about 200° C. and less than about 230° C.; discharging and cooling the low-order condensate at a pressure at or below atmospheric pressure, in an inert gas atmosphere; and subjecting the discharged and cooled low-order condensate to solid state polymerization. The production method makes it possible to obtain a polyamide having outstanding mechanical strength, heat resistance, color tone and the like without problems such as gelling.
-
公开(公告)号:US20150329672A1
公开(公告)日:2015-11-19
申请号:US14437523
申请日:2013-10-23
发明人: Tomomich Kanda , Tomoaki Shimoda
CPC分类号: C08G69/30 , C08G69/26 , C08G69/265 , C08G69/28 , C08G69/46
摘要: The polyamide production method of the present invention comprises the steps of: producing a low-order condensate by effecting a polycondensation reaction between a dicarboxylic acid component containing between about 5 and about 40 mol. % of terephthalic acid, and a diamine component containing between about 70 and about 100 mol. % of a xylylenediamine in which the content of paraxylylenediamine is between about 50 and about 100 mol. %, under conditions of a reaction temperature of at least about 200° C. and less than about 230° C.; discharging and cooling the low-order condensate at a pressure at or below atmospheric pressure, in an inert gas atmosphere; and subjecting the discharged and cooled low-order condensate to solid state polymerization. The production method makes it possible to obtain a polyamide having outstanding mechanical strength, heat resistance, colour tone and the like without problems such as gelling.
摘要翻译: 本发明的聚酰胺制造方法包括以下步骤:通过在含有约5〜约40mol的二羧酸成分之间进行缩聚反应来制造低级缩合物。 %的对苯二甲酸和含有约70至约100mol的二胺组分。 %的对二甲苯二胺的含量为约50至约100摩尔的苯二甲胺。 在反应温度为至少约200℃且小于约230℃的条件下; 在惰性气体气氛中在低于或低于大气压的压力下排放和冷却低级冷凝物; 并将排出和冷却的低级缩合物进行固态聚合。 制造方法可以获得具有突出的机械强度,耐热性,色调等的聚酰胺,而没有诸如凝胶化的问题。
-
-
-