1.
公开(公告)号:US20140202211A1
公开(公告)日:2014-07-24
申请号:US14158262
申请日:2014-01-17
Applicant: Corning Incorporated
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E. Womer
IPC: C03B11/08 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
Abstract translation: 用于成形玻璃的模具可以通过包括提供具有包括至少约90%的镍的成形表面的模具主体并通过将成形表面暴露于氧化热处理来改变模制体的成形表面的组成的方法来制备 。 氧化热处理可以包括斜坡加热处理,固定热处理或斜坡热处理和固定热处理两者。 升温热处理可以包括以约20℃/小时至约500℃/小时的速度升高加热温度至约700℃至约1000℃的温度。固定热处理可包括 将加热温度保持在约700℃至约1000℃,保持时间至少约5分钟。
-
2.
公开(公告)号:US20140206523A1
公开(公告)日:2014-07-24
申请号:US14158242
申请日:2014-01-17
Applicant: CORNING INCORPORATED
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: The present disclosure relates to high purity nickel molds for use in forming three dimensional glass substrates, along with methods of making three dimensional glass substrates. The mold compositions minimize imperfections in the formed glass substrates providing optical quality shaped glass articles for use in electronics applications.
Abstract translation: 本公开涉及用于形成三维玻璃基板的高纯度镍模具以及制造三维玻璃基板的方法。 模具组合物使形成的玻璃基底中的缺陷最小化,提供用于电子应用的光学质量成形玻璃制品。
-
3.
公开(公告)号:US09266768B2
公开(公告)日:2016-02-23
申请号:US14158242
申请日:2014-01-17
Applicant: CORNING INCORPORATED
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang
IPC: B32B9/00 , C03B40/00 , C03B11/00 , C03B23/035 , C23C8/10 , C03B40/02 , C03B23/025 , C03B23/03 , C03B23/00 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: The present disclosure relates to high purity nickel molds for use in forming three dimensional glass substrates, along with methods of making three dimensional glass substrates. The mold compositions minimize imperfections in the formed glass substrates providing optical quality shaped glass articles for use in electronics applications.
Abstract translation: 本公开涉及用于形成三维玻璃基板的高纯度镍模具以及制造三维玻璃基板的方法。 模具组合物使形成的玻璃基底中的缺陷最小化,提供用于电子应用的光学质量成形玻璃制品。
-
公开(公告)号:US09475723B2
公开(公告)日:2016-10-25
申请号:US14836561
申请日:2015-08-26
Applicant: CORNING INCORPORATED
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E. Womer
IPC: C03B40/00 , C03B11/00 , C03B23/035 , C23C8/10 , C03B40/02 , C03B23/025 , C03B23/03 , C03B23/00 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
-
5.
公开(公告)号:US20160167894A1
公开(公告)日:2016-06-16
申请号:US14966471
申请日:2015-12-11
Applicant: CORNING INCORPORATED
Inventor: Kevin Thomas Morris , Andrew Nathan Nassau , Michael George Shultz , Matthew John Towner , Kevin William Uhlig , Ljerka Ukrainczyk , Thomas Achille Yorio
CPC classification number: B65G47/905 , B29C31/008 , C03B23/023 , C03B23/0357 , C03B35/202 , C03B2215/61 , C03B2225/02
Abstract: An apparatus for locating a preform on a mold includes a preform handling tool and a force sensor coupled to the preform handling tool such that the force sensor is capable of sensing forces applied to the preform during handling of the preform by the preform handling tool. The apparatus includes a control device that is arranged and operable to move the preform handling tool relative to the mold. A method of locating the preform on the mold includes picking up the preform using the preform handling tool and placing the preform in a vicinity of the mold. Positions on the mold are mapped with an edge of the preform with the aid of the force sensor. The preform is paced on the mold according to the mapped positions.
Abstract translation: 用于在模具上定位预成型件的装置包括预成型件处理工具和耦合到预成型件处理工具的力传感器,使得力传感器能够感测由预成型件处理工具处理预成型件期间施加到预成型件的力。 该装置包括控制装置,该控制装置被布置和可操作以相对于模具移动预成型件处理工具。 将预型件定位在模具上的方法包括使用预成型件处理工具拾起预成型件并将预成型件放置在模具附近。 借助于力传感器,将模具上的位置与预成型件的边缘对准。 根据映射位置,预成型件在模具上起步。
-
6.
公开(公告)号:US20150360993A1
公开(公告)日:2015-12-17
申请号:US14836561
申请日:2015-08-26
Applicant: CORNING INCORPORATED
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E. Womer
IPC: C03B40/00 , C23C8/10 , C03B23/035 , C03B23/025 , C03B23/00 , C03B23/023
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
Abstract translation: 用于成形玻璃的模具可以通过包括提供具有包括至少约90%的镍的成形表面的模具主体并通过将成形表面暴露于氧化热处理来改变模制体的成形表面的组成的方法来制备 。 氧化热处理可以包括斜坡热处理,固定热处理,或斜坡加热处理和固定热处理两者。 升温热处理可以包括以约20℃/小时至约500℃/小时的速度升高加热温度至约700℃至约1000℃的温度。固定热处理可包括 将加热温度保持在约700℃至约1000℃,保持时间至少约5分钟。
-
7.
公开(公告)号:US09145323B2
公开(公告)日:2015-09-29
申请号:US14158262
申请日:2014-01-17
Applicant: Corning Incorporated
Inventor: Kristen Marie Horn , David Myron Lineman , Kevin Thomas Morris , Wenchao Wang , Kim E Womer
IPC: C03B11/08 , C03B11/00 , C03B23/035 , C23C8/10 , C03B40/02 , C03B23/025 , C03B23/03
CPC classification number: C03B40/00 , C03B11/00 , C03B23/002 , C03B23/023 , C03B23/0252 , C03B23/0302 , C03B23/0355 , C03B23/0357 , C03B40/02 , C23C8/10 , Y02P40/57
Abstract: A mold for shaping glass can be made by a method that includes providing a mold body having a shaping surface comprising at least about 90% nickel and modifying the composition of the shaping surface of the mold body by exposing the shaping surface to an oxidizing heat treatment. The oxidizing heat treatment may include a ramping heat treatment, a fixed heat treatment, or both the ramping heat treatment and the fixed heat treatment. The ramping heat treatment may include increasing a heating temperature at a rate from about 20° C./hour to about 500° C./hour to a temperature from about 700° C. to about 1000° C. The fixed heat treatment may include holding the heating temperature from about 700° C. to about 1000° C. for a holding time of at least about 5 minutes.
Abstract translation: 用于成形玻璃的模具可以通过包括提供具有包括至少约90%的镍的成形表面的模具主体并通过将成形表面暴露于氧化热处理来改变模制体的成形表面的组成的方法来制备 。 氧化热处理可以包括斜坡热处理,固定热处理,或斜坡加热处理和固定热处理两者。 升温热处理可以包括以约20℃/小时至约500℃/小时的速度升高加热温度至约700℃至约1000℃的温度。固定热处理可包括 将加热温度保持在约700℃至约1000℃,保持时间至少约5分钟。
-
-
-
-
-
-