公开(公告)号:US10118975B2
公开(公告)日:2018-11-06
申请号:US15673456
申请日:2017-08-10
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Qing Yang , Connor D. Boxell , Tony R. Crain
IPC: C07F17/00 , C08F4/6592 , C08F10/00 , C08F4/659
Abstract: Disclosed herein are catalyst compositions containing bicyclic bridged metallocene compounds. These catalyst compositions can be used for the polymerization of olefins. For example, ethylene polymers produced using these catalyst compositions can be characterized by low molecular weights and high melt flow rates, and can be produced without the addition of hydrogen.
-
公开(公告)号:US20160319052A1
公开(公告)日:2016-11-03
申请号:US14699533
申请日:2015-04-29
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Eric D. Schwerdtfeger , Max P. McDaniel , Ted H. Cymbaluk , Connor D. Boxell , Kathy S. Collins , Alan L. Solenberger
IPC: C08F110/02
CPC classification number: C08F110/02 , C08F10/02 , C08F4/24 , C08F4/025 , C08F2500/12
Abstract: A method comprising a) calcining a silica support at temperature in the range of from about 100° C. to about 500° C. to form a precalcined silica support; b) contacting the precalcined silica support with a titanium alkoxide to form a titanated support; c) subsequent to b), contacting the titanated support with a polyol to form a polyol associated titanated support (PATS); d) contacting at least one of the silica support, pre-calcined silica support, the titanated support, the PATS, or combinations thereof with a chromium-containing compound to form a polymerization catalyst precursor; e) drying the polymerization catalyst precursor to form a dried polymerization catalyst precursor; and f) calcining the dried polymerization catalyst precursor to produce a polymerization catalyst, wherein less than about 0.1 wt. % of a highly reactive volatile organic compound (HRVOC) is emitted during the calcining of the dried polymerization catalyst precursor.
Abstract translation: 一种方法,包括a)在约100℃至约500℃的温度范围内煅烧二氧化硅载体以形成预煅烧二氧化硅载体; b)使预煅烧的二氧化硅载体与钛醇盐接触以形成钛酸化的载体; c)在b)之后,使钛酸化的载体与多元醇接触以形成多元醇相关的钛化载体(PATS); d)将二氧化硅载体,预煅烧二氧化硅载体,钛化载体,PATS或其组合中的至少一种与含铬化合物接触以形成聚合催化剂前体; e)干燥聚合催化剂前体以形成干燥的聚合催化剂前体; 和f)煅烧干燥的聚合催化剂前体以产生聚合催化剂,其中小于约0.1wt。 在干燥的聚合催化剂前体的煅烧期间发射%的高反应性挥发性有机化合物(HRVOC)。
-
公开(公告)号:US09758600B1
公开(公告)日:2017-09-12
申请号:US15465643
申请日:2017-03-22
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Qing Yang , Connor D. Boxell , Tony R. Crain
IPC: C08F4/6592 , C07F17/00
CPC classification number: C08F4/65927 , C07F17/00 , C08F4/65908 , C08F10/00
Abstract: Disclosed herein are catalyst compositions containing bicyclic bridged metallocene compounds. These catalyst compositions can be used for the polymerization of olefins. For example, ethylene polymers produced using these catalyst compositions can be characterized by low molecular weights and high melt flow rates, and can be produced without the addition of hydrogen.
-
公开(公告)号:US09758540B1
公开(公告)日:2017-09-12
申请号:US15163730
申请日:2016-05-25
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Qing Yang , Connor D. Boxell , Tony R. Crain
IPC: C07F17/00 , C08F4/6592 , C08F210/16 , C08F10/02
CPC classification number: C07F17/00 , C08F4/65912 , C08F4/65916 , C08F4/65927 , C08F210/16 , C08F210/14 , C08F2500/03
Abstract: Disclosed herein are catalyst compositions containing bicyclic bridged metallocene compounds. These catalyst compositions can be used for the polymerization of olefins. For example, ethylene polymers produced using these catalyst compositions can be characterized by low molecular weights and high melt flow rates, and can be produced without the addition of hydrogen.
-
5.
公开(公告)号:US20240279366A1
公开(公告)日:2024-08-22
申请号:US18648551
申请日:2024-04-29
Applicant: Chevron Phillips Chemical Company LP
Inventor: Max P. McDaniel , Qing Yang , Ryan N. Rose , Kathy S. Clear , Graham R. Lief , Eric D. Schwerdtfeger , Anand Ramanathan , Jeremy M. Praetorius , Connor D. Boxell
IPC: C08F4/02 , C08F4/659 , C08F4/6592 , C08F210/02
CPC classification number: C08F4/025 , C08F4/65916 , C08F4/65925 , C08F4/65927 , C08F210/02 , C08F2420/01 , C08F2420/03
Abstract: Sulfated bentonite compositions are characterized by a total pore volume from 0.4 to 1 mL/g, a total BET surface area from 200 to 400 m2/g, and an average pore diameter from 55 to 100 Angstroms. The sulfated bentonite compositions also can be characterized by a d50 average particle size in a range from 15 to 50 μm and a ratio of d90/d10 from 3 to 15. The sulfated bentonite compositions can contain a sulfated bentonite and from 10 to 90 wt. % of colloidal particles, or the sulfated bentonite compositions can contain a sulfated bentonite and from 0.2 to 10 mmol/g of zinc and/or phosphorus. These compositions can be utilized in metallocene catalyst systems to produce ethylene based polymers.
-
公开(公告)号:US11331650B2
公开(公告)日:2022-05-17
申请号:US16237011
申请日:2018-12-31
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Eric D. Schwerdtfeger , Max P. McDaniel , Ted H. Cymbaluk , Connor D. Boxell , Alan L. Solenberger , Kathy S. Clear
Abstract: A method comprising a) drying a support material comprising silica at temperature in the range of from about 150° C. to about 220° C. to form a dried support; b) contacting the dried support with methanol to form a slurried support; c) subsequent to b), cooling the slurried support to a temperature of less than about 60° C. to form a cooled slurried support; d) subsequent to c), contacting the cooled slurried support with a titanium alkoxide to form a titanated support; and e) thermally treating the titanated support by heating to a temperature of equal to or greater than about 150° C. for a time period of from about 5 hours to about 30 hours to remove the methanol and yield a dried titanated support.
-
公开(公告)号:US20170342099A1
公开(公告)日:2017-11-30
申请号:US15666663
申请日:2017-08-02
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Qing Yang , Connor D. Boxell , Tony R. Crain
IPC: C07F17/00 , C08F4/6592 , C08F10/02 , C08F210/16
CPC classification number: C07F17/00 , C08F4/65912 , C08F4/65916 , C08F4/65927 , C08F210/16 , C08F210/14 , C08F2500/03
Abstract: Disclosed herein are catalyst compositions containing bicyclic bridged metallocene compounds. These catalyst compositions can be used for the polymerization of olefins. For example, ethylene polymers produced using these catalyst compositions can be characterized by low molecular weights and high melt flow rates, and can be produced without the addition of hydrogen.
-
公开(公告)号:US09796798B2
公开(公告)日:2017-10-24
申请号:US15281514
申请日:2016-09-30
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Eric D. Schwerdtfeger , Max P. McDaniel , Ted H. Cymbaluk , Connor D. Boxell , Kathy S. Collins , Alan L. Solenberger
IPC: C08F10/02 , C08F110/02
CPC classification number: C08F110/02 , C08F10/02 , C08F4/24 , C08F4/025 , C08F2500/12
Abstract: A method comprising a) calcining a silica support at temperature in the range of from about 100° C. to about 500° C. to form a precalcined silica support; b) contacting the precalcined silica support with a titanium alkoxide to form a titanated support; c) subsequent to b), contacting the titanated support with a polyol to form a polyol associated titanated support (PATS); d) contacting at least one of the silica support, pre-calcined silica support, the titanated support, the PATS, or combinations thereof with a chromium-containing compound to form a polymerization catalyst precursor; e) drying the polymerization catalyst precursor to form a dried polymerization catalyst precursor; and f) calcining the dried polymerization catalyst precursor to produce a polymerization catalyst, wherein less than about 0.1 wt. % of a highly reactive volatile organic compound (HRVOC) is emitted during the calcining of the dried polymerization catalyst precursor.
-
公开(公告)号:US11999814B2
公开(公告)日:2024-06-04
申请号:US18065003
申请日:2022-12-13
Applicant: Chevron Phillips Chemical Company LP
Inventor: Max P. McDaniel , Qing Yang , Ryan N. Rose , Kathy S. Clear , Graham R. Lief , Eric D. Schwerdtfeger , Anand Ramanathan , Jeremy M. Praetorius , Connor D. Boxell
IPC: C08F4/02 , C08F4/659 , C08F4/6592 , C08F210/02
CPC classification number: C08F4/025 , C08F4/65916 , C08F4/65925 , C08F4/65927 , C08F210/02 , C08F2420/01 , C08F2420/03
Abstract: Sulfated bentonite compositions are characterized by a total pore volume from 0.4 to 1 mL/g, a total BET surface area from 200 to 400 m2/g, and an average pore diameter from 55 to 100 Angstroms. The sulfated bentonite compositions also can be characterized by a d50 average particle size in a range from 15 to 50 μm and a ratio of d90/d10 from 3 to 15. The sulfated bentonite compositions can contain a sulfated bentonite and from 10 to 90 wt. % of colloidal particles, or the sulfated bentonite compositions can contain a sulfated bentonite and from 0.2 to 10 mmol/g of zinc and/or phosphorus. These compositions can be utilized in metallocene catalyst systems to produce ethylene based polymers.
-
公开(公告)号:US10213766B2
公开(公告)日:2019-02-26
申请号:US14858512
申请日:2015-09-18
Applicant: Chevron Phillips Chemical Company LP
Inventor: Jeremy M. Praetorius , Eric D. Schwerdtfeger , Max P. McDaniel , Ted H. Cymbaluk , Connor D. Boxell , Alan L. Solenberger , Kathy S. Clear
Abstract: A method comprising a) drying a support material comprising silica at temperature in the range of from about 150° C. to about 220° C. to form a dried support; b) contacting the dried support with methanol to form a slurried support; c) subsequent to b), cooling the slurried support to a temperature of less than about 60° C. to form a cooled slurried support; d) subsequent to c), contacting the cooled slurried support with a titanium alkoxide to form a titanated support; and e) thermally treating the titanated support by heating to a temperature of equal to or greater than about 150° C. for a time period of from about 5 hours to about 30 hours to remove the methanol and yield a dried titanated support.
-
-
-
-
-
-
-
-
-