Conductive polyphenylene ether-polyamide blend
    1.
    发明授权
    Conductive polyphenylene ether-polyamide blend 有权
    导电聚苯醚 - 聚酰胺共混物

    公开(公告)号:US06469093B1

    公开(公告)日:2002-10-22

    申请号:US09438998

    申请日:1999-11-12

    IPC分类号: C08K304

    摘要: The present invention relates to a thermoplastic resin composition and a method for making the same. The composition comprises the reaction product of about 10 wt. % to about 50 wt. % polyphenylene ether, about 35 wt. % to about 65 wt. % polyamide, preferably about 0.4 wt. % to about 3.0 wt. % carbon fibrils, and optionally about 5 wt. % to about 40 wt. % talc, up to about 10 wt. % compatibilizing agent and up to about 20 wt. % impact modifier. The method comprises forming a carbon masterbatch with polyamide and introducing the masterbatch and the polyamide subsequent to compounding the polyphenylene ether with a compatibilizing agent.

    摘要翻译: 本发明涉及热塑性树脂组合物及其制造方法。 该组合物包含约10wt。 %至约50wt。 %聚苯醚,约35wt。 %至约65wt。 %聚酰胺,优选约0.4wt。 %至约3.0wt。 %碳原纤维,和任选地约5wt。 %至约40wt。 %滑石,至多约10重量% %相容剂和高达约20wt。 %影响修饰符。 该方法包括用聚酰胺形成碳母粒并在将聚苯醚与相容剂混合之后引入母料和聚酰胺。

    Conductive polyphenylene ether-polyamide blend
    2.
    发明授权
    Conductive polyphenylene ether-polyamide blend 有权
    导电聚苯醚 - 聚酰胺共混物

    公开(公告)号:US07226963B2

    公开(公告)日:2007-06-05

    申请号:US10249929

    申请日:2003-05-20

    IPC分类号: C08J3/20 C08J3/22

    摘要: The present invention relates to a thermoplastic resin composition and a method for making the same. The composition comprises the reaction product of about 10 wt % to about 50 wt % polyphenylene ether, about 35 wt % to about 65 wt % polyamide, preferably about 0.4 wt % to about 3.0 wt % carbon fibrils, and optionally about 5 wt % to about 40 wt % talc, up to about 10 wt % compatibilizing agent and up to about 20 wt % impact modifier. The method comprises forming a carbon masterbatch with polyamide and introducing the masterbatch and the polyamide subsequent to compounding the polyphenylene ether with a compatibilizing agent.

    摘要翻译: 本发明涉及热塑性树脂组合物及其制造方法。 组合物包含约10重量%至约50重量%的聚苯醚,约35重量%至约65重量%的聚酰胺,优选约0.4重量%至约3.0重量%的碳原纤的反应产物,以及任选地约5重量%至 约40重量%的滑石,至多约10重量%的相容剂和至多约20重量%的抗冲改性剂。 该方法包括用聚酰胺形成碳母粒并在将聚苯醚与相容剂混合之后引入母料和聚酰胺。