PROCESS FOR PREPARING POLY(ALKYLENE FURANDICARBOXYLATE)

    公开(公告)号:US20230265239A1

    公开(公告)日:2023-08-24

    申请号:US18141613

    申请日:2023-05-01

    申请人: Covation Inc.

    摘要: A process to prepare poly(alkylene furandicarboxylate) polymer is disclosed herein. In one embodiment, the process comprises a) contacting a mixture comprising furandicarboxylic acid dialkyl ester, a diol comprising ethylene glycol, 1,3-propanediol, 1,4-butanediol, 1,4-cyclohexanedimethanol, or mixtures thereof, and a metal catalyst at a temperature in the range of from about 140° C. to about 220° C. to form prepolymer,



    wherein the mole ratio of the furandicarboxylic acid dialkyl ester to the diol is in the range of from 1:1.3 to 1:2.2;
    b) performing polycondensation by heating the prepolymer under reduced pressure to a temperature in the range of from about 220° C. to about 260° C. to form poly(alkylene furandicarboxylate) polymer;
    wherein the rate of polycondensation in step c) is faster with the anthraquinone compound present than without; and
    c) adding at least one anthraquinone compound as disclosed herein; and

    PROCESS FOR PREPARING POLY(ALKYLENE FURANDICARBOXYLATE)

    公开(公告)号:US20240218118A1

    公开(公告)日:2024-07-04

    申请号:US18601303

    申请日:2024-03-11

    申请人: Covation Inc.

    摘要: A process to prepare poly(alkylene furandicarboxylate) polymer is disclosed herein. In one embodiment, the process comprises a) contacting a mixture comprising furandicarboxylic acid dialkyl ester, a diol comprising ethylene glycol, 1,3-propanediol, 1,4-butanediol, 1,4cyclohexanedimethanol, or mixtures thereof, and a metal catalyst at a temperature in the range of from about 140° C. to about 220° C. to form prepolymer, wherein the mole ratio of the furandicarboxylic acid dialkyl ester to



    a) the diol is in the range of from 1:1.3 to 1:2.2;
    b) performing polycondensation by heating the prepolymer under
    reduced pressure to a temperature in the range of from about 220° C. to about 260° C. to form poly(alkylene furandicarboxylate) polymer; wherein the rate of polycondensation in step c) is faster with the anthraquinone compound present than without; and
    c) adding at least one anthraquinone compound as disclosed herein; and