Abstract:
The present invention is related to a pink colored pre-sintered or fully-sintered blank for use for the production of a dental restoration, such as a denture base of a full or a partial denture, a partial denture, or an implant supported denture, consisting of a ceramic material which comprises zirconium dioxide doped with yttrium oxide (Y2O3), calcium oxide (CaO), magnesium oxide (MgO) and/or cerium oxide (CeO2), wherein the pink colored blank comprises 2 to 25 wt %, preferably 4 to 17 wt %, and more preferably 5 to 12 wt %, erbium oxide.
Abstract:
The invention relates to a method to increase the strength of a form body of lithium silicate glass ceramic, which after it has a desired end geometry and after the application of a material which influences its surface to form a coating, is subject to a heat treatment. To create a surface compressive stress through the replacement of lithium ions by alkali ions of greater diameter at least that region not covered by the application layer is covered by a melt or paste consisting of or containing a salt of an alkali metal with ions of greater diameter and the form body is in contact with the melt or paste for a period of time t at a temperature T and the melt or paste is subsequently removed from the form body.
Abstract:
A blank for milling or grinding a dental article, the blank having a plate-shaped body adapted to be received in a blank holder of a CAM system, which plate-shaped body comprises one or more ceramic or glass ceramic blank portions and two or more through holes, wherein each through hole is contiguous with at least one of the ceramic or glass ceramic blank portions for receiving a working end of a milling or grinding tool of the CAM system.
Abstract:
A method for forming a multi-layer blank of a ceramic material including the steps of: providing a mold that includes at least one side wall surrounding a lower press plunger to form a cavity therebetween, wherein the lower press plunger has a movable pin; filling into the mold a first ceramic material; extending the movable pin from an upper surface of the lower press plunger and into the cavity; pressing a first upper press plunger against the first ceramic material so that a first open cavity is formed while at least a portion of the first upper press plunger is in contact with the movable pin to maintain the through-hole through the first layer; filling into the mold a second ceramic material of a different composition; extending the movable pin from an upper surface of the first layer and into the first open cavity; and pressing a second upper press plunger against the second layer so that a second open cavity is formed in communication with the through-hole that extends through the first and second layers to form the blank.
Abstract:
The present invention is related to a dental implant comprising at least a lower part and at least an upper part; wherein said lower part of the dental im-plant, which is adapted to be connected to the jawbone of a patient, is made of an at least first material; wherein said upper part of the dental implant, which is adapted to be connected to the lower part of the dental implant, is made of an at least second material; and wherein the upper surface of the upper part of the dental implant is adapted to be aligned with the upper surface of the jawbone of a patient; wherein said at least first material is different from said at least second material; wherein the at least second material of the upper part of the implant is made of a ceramic material, and wherein said ceramic material comprises zirco-nium dioxide comprising at least one coloring additive. The present invention is further related to a dental restoration system com-prising at least such an inventive dental implant and at least an abutment, wherein the abutment is adapted to be connected to the dental implant, and wherein the abutment is made of at least a third material; wherein the abutment is made of a ceramic material, and wherein said ceramic material comprises zirconium dioxide comprising at least one coloring additive.
Abstract:
The invention relates to a medical form body of lithium silicate glass ceramic. To increase its strength it is proposed that in the form body comprising lithium silicate glass or containing lithium silicate glass the lithium ions are replaced by alkali ions of greater diameter to generate a surface compressive stress. To this end the form body is covered with a melt containing an alkali metal for which an aliquoted quantity of salt containing the alkali metal is used.
Abstract:
The present invention is related to a method for producing a ceramic multilayer blank comprising at least a first layer of a first ceramic material and at least a second layer of a second ceramic material, wherein the first layer and the second layer are made of ceramic materials of different compositions, which are filled in pourable condition layer-by-layer into a mold and thereafter they are pressed and then sintered, wherein the first layer is a pink colored layer, wherein the first ceramic material comprises 2 to 25 wt % erbium oxide.
Abstract:
The invention relates to a method to derive a medical form body of lithium silicate glass ceramic. To increase its strength it is proposed that in the form body comprising lithium silicate glass or containing lithium silicate glass the lithium ions are replaced by alkali ions of greater diameter to generate a surface compressive stress. To this end the form body is covered with a melt containing an alkali metal for which an aliquoted quantity of salt containing the alkali metal is used.