公开(公告)号:US4151472A
公开(公告)日:1979-04-24
申请号:US851374
申请日:1977-11-14
申请人: Eiji Watanabe , Junichi Onozawa , Jouji Tanaka , Takazo Takahashi , Tsuneo Kitamura , Hiroshi Yamada , Hiroshi Noguchi , Yukio Ueno
发明人: Eiji Watanabe , Junichi Onozawa , Jouji Tanaka , Takazo Takahashi , Tsuneo Kitamura , Hiroshi Yamada , Hiroshi Noguchi , Yukio Ueno
CPC分类号: G01R15/09 , G01R23/005 , G08B3/1008
摘要: In a selective calling circuit including a band-pass filter which may be constituted by an active filter, and a power source for energizing the filter, a control signal is generated which has a predetermined duration in accordance with the output of the band-pass filter at a point of time whereat the output of the band-pass filter reaches a predetermined level. In response to the control signal, there is established a state in which the center frequency of the band-pass filter can be changed, and the output of the power source is changed from a first level to a second level for a period of time substantially corresponding to the predetermined duration of the control signal. At the aforementioned first level, the band-pass filter may be energized, while at the second level, it may be deenergized.
摘要翻译: 在包括可由有源滤波器构成的带通滤波器和用于激励滤波器的电源的选呼电路中,产生根据带通滤波器的输出具有预定持续时间的控制信号 在带通滤波器的输出达到预定电平的时间点。 响应于控制信号,建立了可以改变带通滤波器的中心频率并且将电源的输出从第一电平改变到第二电平一段时间的状态 对应于控制信号的预定持续时间。 在上述第一级,带通滤波器可以被激励,而在第二级,它可以被断电。
-
公开(公告)号:US3953558A
公开(公告)日:1976-04-27
申请号:US425870
申请日:1973-12-18
申请人: Itaru Hatano , Minoru Hara , Tsuneo Kitamura , Akira Ando , Yasuyuki Suganuma
发明人: Itaru Hatano , Minoru Hara , Tsuneo Kitamura , Akira Ando , Yasuyuki Suganuma
IPC分类号: C08J9/22 , B29C44/00 , B29C44/34 , B29C44/44 , B29C59/00 , B29C67/00 , C08J9/16 , C08J9/232 , B29D27/00
CPC分类号: B29C44/461 , B29C44/445 , C08J9/232 , B29K2023/00 , C08J2323/02 , Y10S264/05 , Y10S264/15 , Y10S264/18 , Y10S521/919 , Y10T428/254
摘要: A method of moulding foamed synthetic resin pellets of polyolefine in a mould, wherein the synthetic resin pellets are prepared with volumne of closed cells being more than 65 % of the total volume of the total cells and having an inorganic gas in the cells at a pressure higher than 1.18 atmospheres, then filled in a mould which is not completely gas tight, and then heated to expand and tightly adhere to each other. The pressure in the mould can be lower than ordinary pressure or at a vacuum and the pressure of the resin can be at a pressure higher than ordinary pressure. The moulded product may be removed from the mould after cooling or during cooling when the inner temperature of the product is between its melting point and a temperature 50.degree.C below the melting point. The obtained product may be stored at a temperature of 30.degree. to 70.degree.C below the melting point.
摘要翻译: 一种在模具中模制聚烯烃的发泡合成树脂颗粒的方法,其中合成树脂颗粒是以闭孔体积大于总细胞总体积的65%而制备的,并且在压力下在细胞中具有无机气体 高于1.18大气压,然后填充在不完全气密的模具中,然后加热膨胀并彼此紧密粘合。 模具中的压力可以低于常压或真空,并且树脂的压力可以处于高于常压的压力。 当产品的内部温度在其熔点和低于熔点50℃的温度之间时,模制产品可以在冷却之后或在冷却期间从模具中除去。 所得产物可以在低于熔点的30℃至70℃的温度下储存。
-