Abstract:
There is provided a manufacturing method for a thermal conductive layer, with which a thermal conductive layer having a thermal diffusivity of 3.0×10−7 m2s−1 or more is manufactured on a support by using a composition for forming a thermal conductive layer, the composition containing a resin, a filler, and a solvent and having a concentration of solid contents of less than 90% by mass, the manufacturing method including a discharge step of discharging the composition toward the support; and a solvent amount reduction step of reducing a solvent amount in the composition such that a first solvent amount reduction time taken after the composition is discharged until the concentration of solid contents in the composition reaches 90% by mass on the support is 10 seconds or more for each position on the support.
Abstract:
There is provided a photosensitive transparent composition for a color filter of a solid-state imaging device, containing (A) a photopolymerization initiator, (B) a polymerizable compound, and (C) an alkali-soluble resin, wherein the cured film obtained from the photosensitive transparent composition has a refractive index of 1.60 to 1.90 for light at a wavelength of 633 nm.