摘要:
The disclosure relates to a process for the discontinuous separation of a solid consisting predominantly of carbon black from its aqueous suspension by filtration. To this end, the disclosure provides for use to be made of a tube pressure filter which is operated under a final pressure of 30 to 100 bars.
摘要:
The invention relates to improving the degree of graphitization of carbon black produced by subjecting hydrocarbons which are liquid or gaseous under normal conditions to a thermal conversion reaction in the presence of oxygen or an oxygen-containing gas and steam, if desired, at temperatures of 1200.degree. to 2000.degree. C. and pressures of 1 to 80 bars. To this end, the carbon black is conveyed downwardly in a quasi-fluid state, within 1 to 5 hours through a sojourn zone in upright position, the sojourn zone being maintained at a temperature of at least 1200.degree. C.The invention relates to an apparatus for carrying out this process, the apparatus comprising a graphite tube; a steel container concentrically surrounding the graphite tube; a feed pipe penetrating into the interior of the graphite tube; a water-cooled discharge means; and a nitrogen feed inlet arranged below the lower end of the graphite tube; the space left between the graphite tube and steel container being occupied by insulating material.
摘要:
Phosphorus in vapor form and phosphanes are separated from gas mixtures which consist of carbon monoxide, with or without hydrogen, nitrogen and steam. Concerned are more particularly the off-gases of phosphorus-producing furnaces. To this end, the gas mixture is admixed with at least the stoichiometric amount of oxygen and/or of oxygen-containing gases necessary to achieve conversion of the total phosphorus contained in the gas mixture to oxidation level V. The resulting mixture is introduced into a reaction zone maintained at a temperature within the range 200.degree. to 700.degree. C. and allowed to remain therein over a period of 0.5 to 20 seconds. Resulting phosphorus-V compounds are finally separated from the gas mixture.
摘要:
The disclosure relates to a process for making phosphorus pentoxide by subjecting elemental yellow phosphorus to combustion with dried air inside a steel-made combustion chamber with utilization of the reaction heat for the production of energy. To this end, the disclosure provides for the combustion to be effected inside a combustion chamber of which the walls are arranged so as to form a cooling system with cavities therein; for a liquid or liquid/steam-mixture as a heat carrier abstracting the reaction heat to be circulated through the cooling system, the liquid or liquid/steam-mixture assuming an increased temperature being preferably so circulated under increased pressure; for steam formed in the cooling system to be continuously taken therefrom; for an equivalent proportion of fresh liquid to be introduced into the cooling system; for hot P.sub.2 O.sub.5 issuing in vapor form from the combustion chamber to be condensed or worked up into desirable final product, the combustion chamber being a cylindrical vessel with a height/diameter-ratio of 2.5:1 to 5:1 and having 1 to 10 burners disposed axisymmetrically in its circular base plate.The disclosure also relates to an apparatus for carrying out the process.
摘要:
For producing finely disperse aluminum nitride by reacting hydroxides of aluminum with carbon in a molar ratio of (1:1.5) to (1:2.5), the hydroxides of aluminum are intensively ground together with carbon, in particular carbon black, using a non-aqueous grinding fluid. After the non-aqueous grinding fluid has been separated off from the suspension, the ground material obtained is calcined at 400.degree. to 1000.degree. C., while passing nitrogen through. The material obtained is then treated under intensive contact with nitrogen for 1 to 100 hours at 1400.degree. to 1700.degree. C., before the excess carbon contained in the reaction product is removed by heating to 500.degree. to 900.degree. C. in contact with oxygen-containing gases.The hydroxides of aluminum and the carbon can also be intensively ground separately from one another, using a non-aqueous grinding fluid, and the suspensions obtained can be mixed.
摘要:
To produce tubular molded parts made of high-temperature superconductor oxide material based on bismuth, calcium, strontium and copper, a homogeneous melt of the oxide with a specified stoichiometry is allowed to run at temperatures of 900.degree. to 1100.degree. C. into a casting zone rotating about its horizontal axis. The solidified molded part is removed from the casting zone and it is annealed for 4 to 150 hours at 700.degree. to 900.degree. C. in an oxygen-containing atmosphere. A plant for producing tubular molded parts includes a rotatably arranged mold (4, 9) which is provided at least at one end face with a front plate 6 which reduces its free cross section, a runner 7 extending into the interior of the mold (4, 9) and a crucible 8 arranged above the runner 7 which is capable of feeding the runner 7 with melt (cf. FIG. 2 A).