摘要:
A ceramic bonding material including at least one fibrous material, a flux agent and a thickening agent wherein the ceramic bonding material fired at a set temperature to bond the two adjacent substrate faces.
摘要:
Methods for forming ceramic cores are disclosed. A ceramic core formed using the method of the present application includes a silica depletion zone encapsulating an inner zone. The inner zone includes mullite and the silica depletion zone includes alumina. The method includes heat-treating a ceramic body in a non-oxidizing atmospheric condition for an effective temperature and time combination at a pressure less than 10−2 atmosphere to form the silica depletion zone at a surface of the ceramic core.
摘要:
One aspect relates to a composite, including a ceramic body having a first layer surface and a second layer surface and at least one cermet conductor that electrically connects the surfaces. The composite includes a first layer with the first layer surface, a first ceramic, a first hole and a first cermet element in the first hole, a second layer with the second layer surface, a second ceramic, a second hole and a second cermet element in the second hole, and an intermediate layer that is located between the first and the second layer. The intermediate layer includes an intermediate layer ceramic, an intermediate hole and one intermediate cermet element in the intermediate hole. A projection of the cross-section of the first hole and a projection of the cross section of the second hole onto a plane Px,y are arranged offset to each other.
摘要:
A turbine power generation system with enhanced stabilization of refractory carbides provided by hydrocarbon from high carbon activity gases is disclosed. The disclosure also includes a method of using high carbon activity gases to stabilize hot gas path components.
摘要:
A method of inhibiting an irregular aggregation of a nanosized powder includes (A) providing a nanosized ceramic powder to perform thereon a thermal analysis and thereby attain an endothermic peak temperature; (B) performing an impurity-removal heat treatment on the nanosized ceramic powder at a temperature higher than the endothermic peak temperature; (C) switching the nanosized ceramic powder from a temperature environment of the impurity-removal heat treatment to an environment of a temperature higher than a phase change temperature of the nanosized ceramic powder, followed by performing a calcination heat treatment on the nanosized ceramic powder in the environment of the temperature higher than the phase change temperature of the nanosized ceramic powder, wherein the nanosized ceramic powder skips the temperature environment between impurity-removal heat treatment and calcination heat treatment to shun generating a vermicular structure, avoid crystalline irregularity and abnormal growth, reduce particle aggregation, and achieve satisfactory distribution.
摘要:
Functionalized microspheres for being dispersed in matrix materials to reduce the density and weight of the materials may be configured to include a covalently bound surface component which is configured to covalently bond with the matrix material so that when combined with the matrix material a strong, light-weight matrix material may be produced.
摘要:
Functionalized microspheres for being dispersed in matrix materials to reduce the density and weight of the materials may be configured to include a covalently bound surface component which is configured to covalently bond with the matrix material so that when combined with the matrix material a strong, light-weight matrix material may be produced.
摘要:
There is provided a binder for ceramic formation or a conductive paste, comprising polyvinyl acetal having a degree of acetalization of from 50 to 85 mol %, a content of vinyl ester monomer unit of from 0.1 to 20 mol %, and having a viscosity-average degree of polymerization of from 200 to 5000, wherein a peak-top molecular weight (A) as measured by a differential refractive index detector and a peak-top molecular weight (B) as measured by an absorptiometer (measurement wavelength: 280 nm) in gel permeation chromatographic measurement of the polyvinyl acetal heated at 230° C. for 3 hours satisfy a formula (1) (A−B)/A
摘要翻译:提供了一种用于陶瓷形成的粘合剂或导电性糊剂,其包含缩醛化度为50〜85摩尔%的聚乙烯醇缩醛,乙烯基酯单体单元的含量为0.1〜20摩尔%,粘度平均 聚合度为200至5000,其中通过差示折射率检测器测量的峰顶分子量(A)和通过吸光光度计(测量波长:280nm)测量的峰顶分子量(B)在 在230℃下加热3小时的聚乙烯醇缩醛的凝胶渗透色谱测定满足式(1)(A-B)/ A <0.60,聚乙烯醇缩醛的峰顶分子量(B) 从0.50×10-3到1.00×10-2。
摘要:
A selective laser sintering system includes a leveling roller having a first orientation. The leveling roller is configured to roll over a first feed bin. The build chamber is configured to receive, from the first feed bin and by the leveling roller, a transfer of a portion of matrix material. The selective laser sintering system is configured to transfer the portion to the build chamber in a number of orientations.
摘要:
Embodiments described herein generally relate to apparatus and methods for thermally treating chamber components for use in ultraviolet semiconductor processing chambers. Thermal treatment of chamber components comprising unitary ceramic or glass articles may reduce the probability of particle generation when the chamber components are exposed to corrosive environments, such as exposure to ultraviolet light and ozone/oxygen radicals. A method of thermally treating chamber components includes heating the unitary article at an acceptable ramp rate to a desired temperature for a desired time period and subsequently cooling the unitary article at the ramping rate.