Steel cylinder barrel having bonded bronze-iron valve plate
    1.
    发明授权
    Steel cylinder barrel having bonded bronze-iron valve plate 失效
    具有粘结的黄铜阀门的钢瓶筒

    公开(公告)号:US3709107A

    公开(公告)日:1973-01-09

    申请号:US3709107D

    申请日:1970-11-27

    申请人: GEN SIGNAL CORP

    发明人: ALGER M DUNN N

    IPC分类号: B22D19/08 F01B3/00 F01B11/02

    摘要: The disclosure concerns steel cylinder barrels for piston pumps and motors having bonded non-steel valve plates. The valve plate comprises a sintered iron powder matrix which is impregnated with bronze and is metallurgically and mechanically bonded to one end of the steel cylinder barrel. The valve plate is made from a porous sintered iron blank which is mounted in contact with one end of a steel barrel blank in an assembly which includes a mass of bronze in the solid state. The assembly is heated in a nonoxidizing atmosphere to a temperature between 1900*F and 2000*F to melt the bronze and cause it to infiltrate the sintered valve plate blank and bond to the steel. Thereafter, the assembly is cooled in the non-oxidizing atmosphere to solidify the bronze, followed by air cooling to room temperature. Finally, the finished valve plate is machined from the bronze-impregnated sintered preform.

    摘要翻译: 本公开涉及用于具有结合的非钢阀板的活塞泵和电动机的钢瓶筒。 阀板包括烧结铁粉基体,其被青铜浸渍并且在冶金和机械上结合到钢瓶筒的一端。 阀板由多孔烧结铁坯制成,该多孔烧结铁坯与包括一块固体状青铜质的组件中的钢桶坯料的一端接触。 将组件在非氧化性气氛中加热至1900°F至2000°F之间的温度,以熔化青铜,并使其渗透到烧结的阀板坯料上并结合到钢板上。 此后,将组件在非氧化性气氛中冷却,使青铜固化,然后空气冷却至室温。 最后,从青铜浸渍的烧结预制件加工完成的阀板。

    Steel cylinder barrel having bonded bronze-iron liners
    2.
    发明授权
    Steel cylinder barrel having bonded bronze-iron liners 失效
    具有粘结的钢铁衬板的钢瓶筒

    公开(公告)号:US3709108A

    公开(公告)日:1973-01-09

    申请号:US3709108D

    申请日:1970-11-27

    申请人: GEN SIGNAL CORP

    发明人: ALGER M DUNN N

    摘要: The disclosure concerns cylinder barrels for piston pumps and motors which have lined cylinder bores. Each liner comprises a matrix of sintered, powdered iron which is impregnated with bronze, and which is metallurgically and mechanically bonded to the steel barrel. The liners are formed from porous, sintered iron sleeves which are placed in the bores in contact with bronze slugs. The assembly is heated in a non-oxidizing atmosphere to a temperature between 1,900*F and 2,000*F to melt the bronze and cause it to infiltrate the sintered preform and bond to the steel. Thereafter, the assembly is cooled in the non-oxidizing atmosphere to solidify the bronze, followed by air cooling to room temperature. Finally, the finished cylinder bores are machined in the bonded bronze-iron sleeves.

    摘要翻译: 该公开涉及具有内衬缸孔的活塞泵和电动机的气缸筒。 每个衬垫包括用青铜浸渍的烧结的粉末铁的基质,并且其被冶金和机械地结合到钢桶上。 内衬由多孔烧结铁套筒形成,该套筒放置在与青铜塞接触的孔中。 将该组件在非氧化性气氛中加热至1900至200°F之间的温度,以使青铜熔化并使其渗透到烧结的预制件中并结合到钢。 此后,将组件在非氧化性气氛中冷却,使青铜固化,然后空气冷却至室温。 最后,成品缸孔在粘结青铜铁套管中加工。

    Bonded bronze-iron liners for steel cylinder barrel and method of making same
    3.
    发明授权
    Bonded bronze-iron liners for steel cylinder barrel and method of making same 失效
    用于钢瓶缸的粘结钢铁内胆及其制造方法

    公开(公告)号:US3808659A

    公开(公告)日:1974-05-07

    申请号:US27573172

    申请日:1972-07-27

    申请人: GEN SIGNAL CORP

    发明人: ALGER M DUNN N

    摘要: The disclosure concerns cylinder barrels for piston pumps and motors which have lined cylinder bores. Each liner comprises a matrix of sintered, powdered iron which is impregnated with bronze, and which is metallurgically and mechanically bonded to the steel barrel. The liners are formed from porous, sintered iron sleeves which are placed in the bores in contact with bronze slugs. The assembly is heated in a non-oxidizing atmosphere to a temperature between 1,900*F and 2,000*F to melt the bronze and cause it to infiltrate the sintered preform and bond to the steel. Thereafter, the assembly is cooled in the non-oxidizing atmosphere to solidify the bronze, followed by air cooling to room temperature. Finally, the finished cylinder bores are machined in the bonded bronze-iron sleeves.

    摘要翻译: 该公开涉及具有内衬缸孔的活塞泵和电动机的气缸筒。 每个衬垫包括用青铜浸渍的烧结的粉末铁的基质,并且其被冶金和机械地结合到钢桶上。 内衬由多孔烧结铁套筒形成,该套筒放置在与青铜塞接触的孔中。 将该组件在非氧化性气氛中加热至1900至200°F之间的温度,以使青铜熔化并使其渗透到烧结的预制件中并结合到钢。 此后,将组件在非氧化性气氛中冷却,使青铜固化,然后空气冷却至室温。 最后,成品缸孔在粘结青铜铁套管中加工。

    Bonded bronze-iron valve plate for steel cylinder barrel and method of making same
    4.
    发明授权
    Bonded bronze-iron valve plate for steel cylinder barrel and method of making same 失效
    用于钢瓶缸的粘结钢铁阀板及其制造方法

    公开(公告)号:US3803687A

    公开(公告)日:1974-04-16

    申请号:US27573072

    申请日:1972-07-27

    申请人: GEN SIGNAL CORP

    发明人: ALGER M DUNN N

    摘要: The disclosure concerns steel cylinder barrels for piston pumps and motors having bonded non-steel valve plates. The valve plate comprises a sintered iron powder matrix which is impregnated with bronze and is metallurgically and mechanically bonded to one end of the steel cylinder barrel. The valve plate is made from a porous sintered iron blank which is mounted in contact with one end of a steel barrel blank in an assembly which includes a mass of bronze in the solid state. The assembly is heated in a nonoxidizing atmosphere to a temperature between 1,900* F and 2,000* F to melt the bronze and cause it to infiltrate the sintered valve plate blank and bond to the steel. Thereafter, the assembly is cooled in the non-oxidizing atmosphere to solidify the bronze, followed by air cooling to room temperature. Finally, the finished valve plate is machined from the bronze-impregnated sintered preform.