公开(公告)号:US20210229479A1
公开(公告)日:2021-07-29
申请号:US17050941
申请日:2018-08-03
Applicant: Hewlett-Packard Development Company, L.P.
Inventor: Tao CHEN , Xulong FU , Beverly CHOU , Or BRANDSTEIN
Abstract: The present disclosure is drawn to coated print media, methods of making coated print media, and methods of printing. In one example, a coated print medium can include a substrate, a base coating layer on the substrate, and a top coating layer on the base coating layer. The base coating layer can include an inorganic pigment, a binder, and a fixing agent. The top coating layer can include polyvinyl alcohol and polymer nanobeads having a gloss transition temperature from 70° C. to 350° C. The polyvinyl alcohol and polymer nanobeads can be included at from 50 wt % to 100 wt % by dry weight of the top coating layer.
-
公开(公告)号:US20210069961A1
公开(公告)日:2021-03-11
申请号:US17050053
申请日:2018-06-15
Applicant: Hewlett-Packard Development Company, L.P.
Inventor: Adam WEISMAN , Or BRANDSTEIN , Beverly CHOU
Abstract: The present disclosure is drawn to methods of embossing print media, printing systems, and printers. In one example, a method of embossing a print medium can include printing a radiation absorbing ink on a coated print medium to form a printed area. The coated print medium can include a print substrate and an expanding coating layer on the print substrate. The expanding coating layer can include a thermal expansion agent having a minimum expansion temperature. The method can further include heating the coated print medium using a heater such that the printed area and unprinted area reach a first temperature from 5 C to 90 C below the minimum expansion temperature. The coated print medium can be irradiated with radiation having a wavelength from 200 nm to 400 nm to selectively heat the print area and expand the thermal expansion agent in the printed area.
-
公开(公告)号:US20220154402A1
公开(公告)日:2022-05-19
申请号:US17439205
申请日:2019-10-11
Applicant: HEWLETT-PACKARD DEVELOPMENT COMPANY, L.P.
Inventor: Beverly CHOU , Xiaoqi ZHOU , Xulong FU , Jake THOMAS , Tao CHEN
Abstract: A coating composition for a base paper is described. The coating composition comprises a porous clay and an ink pigment fixation agent. The porous clay comprises an alumina-silicate, and has a surface area from 100 m2/g to 400 m2/g.
-
公开(公告)号:US20200324535A1
公开(公告)日:2020-10-15
申请号:US16768516
申请日:2018-03-09
Applicant: Hewlett-Packard Development Company, L.P.
Inventor: Fereshteh KHORRAMI , Beverly CHOU , Tao CHEN , Jesse DAWN
Abstract: The present disclosure is drawn to coating compositions that can include an inorganic pigment, a non-ionic surfactant, latex particles, a polyvinyl alcohol, and a cationic fixing agent. The inorganic pigment can be included in an amount from 60 wt % to 90 wt % by dry weight. The latex particles can include a styrene-butadiene copolymer, and can be present in an amount of 4 wt % to less than 10 wt % by dry weight. The polyvinyl alcohol can have a weight average molecular weight of 150,000 Mw to 400,000 Mw.
-
公开(公告)号:US20210237428A1
公开(公告)日:2021-08-05
申请号:US17050514
申请日:2018-06-15
Applicant: Hewlett-Packard Development Company, L.P.
Inventor: Adam WEISMAN , Beverly CHOU , Or BRANDSTEIN
IPC: B41F19/02 , C09D11/54 , C09D11/38 , C09D11/322 , C09D11/037 , C09D11/106
Abstract: The present disclosure is drawn to methods of embossing print media, printing systems, and printers. In one example, a method of embossing a print medium can include printing an enhancing fluid on a coated print medium to form a printed area. The enhancing fluid can include a colorless radiation absorbing agent capable of converting radiation having a wavelength from 200 nm to 400 nm to heat. A colored ink can also be printed on the print medium to form a visible image. The print medium can include a print substrate and an expanding coating layer on the print substrate. The expanding coating layer can include a thermal expansion agent having a minimum expansion temperature. The coated print medium can be irradiated with radiation having a wavelength from 200 nm to 400 nm to selectively heat the printed area and expand the thermal expansion agent in the printed area.
-
公开(公告)号:US20210129572A1
公开(公告)日:2021-05-06
申请号:US17050491
申请日:2018-06-15
Applicant: Hewlett-Packard Development Company, L.P.
Inventor: Adam Weisman , Beverly CHOU , Or BRANDSTEIN
Abstract: The present disclosure is drawn to methods of radiative embossing print media. In one example, the method of radiative embossing a print medium can include printing a radiation absorbing ink on a coated print medium to form a printed area. The coated print medium can include a print substrate and an expanding coating layer on the print substrate. The expanding coating layer can include a thermal expansion agent having a minimum expansion temperature. The method can further include heating the coated print medium using a heater such that the printed area and unprinted area reach a first temperature from 5° C. to 90° C. below the minimum expansion temperature. The coated print medium can be irradiated with radiation having a wavelength from 200 nm to 400 nm to selectively heat the print area and expand the thermal expansion agent in the printed area.
-
公开(公告)号:US20200086670A1
公开(公告)日:2020-03-19
申请号:US16309893
申请日:2017-10-10
Applicant: Hewlett-Packard Development Company, L.P.
Inventor: Beverly CHOU , Tao CHEN , Xulong FU , Or BRANDSTEIN , Fereshteh KHORRAMI
IPC: B41M5/52
Abstract: The present disclosure is drawn to a recording medium including a substrate, a first coating applied to the substrate, and a second coating applied to the first coating. The first coating can include inorganic pigment, fixative agent, and a first binder. The second coating can include inorganic nanoparticles, aluminum silicate, and a second binder.
-
公开(公告)号:US20190329581A1
公开(公告)日:2019-10-31
申请号:US16311048
申请日:2016-10-26
Applicant: HEWLETT-PACKARD DEVELOPMENT COMPANY, L.P.
Inventor: Xulong FU , Fereshteh KHORRAMI , Tao CHEN , Beverly CHOU
Abstract: An example of a printable recording medium includes a base substrate, a first ink-receiving layer, and a second ink-receiving layer. The first ink-receiving layer includes a first inorganic pigment in an amount equal to or greater than 70 wt % and a first ink-fixing agent in an amount ranging from about 3 wt % to about 10 wt % based on a total wt % of the first ink-receiving layer. The second ink-receiving layer includes a second inorganic pigment. Both the first ink-receiving layer and the second ink-receiving layer exclude precipitated calcium carbonate.
-
-
-
-
-
-
-