Patch and method for producing the same
    1.
    发明授权
    Patch and method for producing the same 有权
    补片及其制作方法

    公开(公告)号:US08802134B2

    公开(公告)日:2014-08-12

    申请号:US13772843

    申请日:2013-02-21

    CPC classification number: A61J3/00 A61K9/7053 A61K9/7061 A61K31/216

    Abstract: A method for producing a patch having a high skin penetrability and a high pharmaceutical physical properties such as adhesion and cohesiveness, and a long-term storability. The patch is produced by first obtaining an adhesive agent layer composition containing oxybutynin and/or salt thereof as a drug, an acrylic-based polymer and/or a rubber-based polymer as an adhesive base agent, liquid paraffin, an organic acid, and a tackifier; heating the adhesive agent layer composition at a temperature in a range from a melting point of the drug to a temperature higher than the melting point by 10° C. for 2 to 24 hours; and slowly cooling the heated adhesive agent layer composition to obtain the adhesive agent layer comprising the drug at a supersaturated concentration in a dissolved form.

    Abstract translation: 一种具有高皮肤渗透性和高的药物物理性质如粘附性和内聚性以及长期保存性的贴剂的制造方法。 通过首先获得含有奥昔布宁和/或其盐作为药物的粘合剂层组合物,作为粘合剂的丙烯酸类聚合物和/或橡胶类聚合物,液体石蜡,有机酸和 增粘剂 在从药物的熔点到高于熔点10℃的温度的温度下加热粘合剂层组合物2〜24小时; 并缓慢冷却加热的粘合剂层组合物以获得以溶解形式的过饱和浓度的包含药物的粘合剂层。

    PATCH AND METHOD FOR PRODUCING THE SAME
    2.
    发明申请
    PATCH AND METHOD FOR PRODUCING THE SAME 有权
    配对及其制造方法

    公开(公告)号:US20140161865A1

    公开(公告)日:2014-06-12

    申请号:US13772843

    申请日:2013-02-21

    CPC classification number: A61J3/00 A61K9/7053 A61K9/7061 A61K31/216

    Abstract: A method for producing a patch having a high skin penetrability and a high pharmaceutical physical properties such as adhesion and cohesiveness, and a long-term storability. The patch is produced by first obtaining an adhesive agent layer composition containing oxybutynin and/or salt thereof as a drug, an acrylic-based polymer and/or a rubber-based polymer as an adhesive base agent, liquid paraffin, an organic acid, and a tackifier; heating the adhesive agent layer composition at a temperature in a range from a melting point of the drug to a temperature higher than the melting point by 10° C. for 2 to 24 hours; and slowly cooling the heated adhesive agent layer composition to obtain the adhesive agent layer comprising the drug at a supersaturated concentration in a dissolved form.

    Abstract translation: 一种具有高皮肤渗透性和高的药物物理性质如粘附性和内聚性以及长期保存性的贴剂的制造方法。 通过首先获得含有奥昔布宁和/或其盐作为药物的粘合剂层组合物,作为粘合剂的丙烯酸类聚合物和/或橡胶类聚合物,液体石蜡,有机酸和 增粘剂 在从药物的熔点到高于熔点10℃的温度的温度下加热粘合剂层组合物2〜24小时; 并缓慢冷却加热的粘合剂层组合物以获得以溶解形式的过饱和浓度的包含药物的粘合剂层。