Abstract:
Provided is oxide glass in which a content of P5+ is 7 to 43 cation %, a content of Nb ions is 10 to 21 cation %, a content of Li+ is 20 cation % or more, a total content of Nb ions and Li+ is 48 to 70 cation %, a content of Bi ions is more than 0 cation % and is equal to or less than 6 cation %, a content of Ba2+ is 5 cation % or less, a content of Zr4+ is 2 cation % or less, a total content of Ti ions and W ions is 5 cation % or less, and a cation ratio of the content of Li+ to a total content of Li+, Na+, and K+[Li+/(Li++Na++K+)] is 0.5 or more.
Abstract:
To provide glass including a colored layer and a manufacturing method thereof. Provided is glass containing one or more glass components selected from the group consisting of Ti ions, Nb ions, W ions, and Bi ions. The glass includes a colored layer having an arbitrary shape.
Abstract:
An optical element includes a glass body including a colored layer provided inside the glass body and positioned at an optical function surface of the optical element. An optical apparatus including the optical element is also provided.
Abstract:
An aspect of the present invention relates to an optical glass, which comprises, denoted as weight percent, 2 to 37 percent of SiO2, 0 to 25 percent of B2O3, 0 to 10 percent of GeO2, 18 to 55 percent of a combined content of Li2O, Na2O, K2O, CaO, SrO, and BaO, and 27 to 55 percent of a combined content of TiO2, Nb2O5, and WO3, wherein the weight ratio of SiO2 content relative to a combined content of SiO2 and B2O3 ranges from 0.1 to 1, a weight ratio of the Li2O content to a combined content of Li2O, Na2O, K2O, CaO, SrO, and BaO ranges from 0 to 0.4, and a weight ratio of TiO2 content relative to a combined content of TiO2, Nb2O5, and WO3 ranges from 0.35 to 1, with a refractive index nd of 1.860 to 1.990 and an Abbé number νd of 21 to 29.
Abstract translation:本发明的一个方面涉及一种光学玻璃,其包括以重量%表示2至37%的SiO 2,0至25%的B 2 O 3,0至10%的GeO 2,18至55%的组合含量 Li 2 O,Na 2 O,K 2 O,CaO,SrO和BaO以及TiO 2,Nb 2 O 5和WO 3的组合含量的27〜55%,其中SiO 2含量相对于SiO 2和B 2 O的组合含量的重量比为0.1〜 如图1所示,Li 2 O含量与Li 2 O,Na 2 O,K 2 O,CaO,SrO和BaO的组合含量的重量比为0〜0.4,TiO 2含量相对于TiO 2,Nb 2 O 5和 WO3的范围为0.35至1,折射率nd为1.860至1.990,Abbé数n为21至29。
Abstract:
An aspect of the present invention relates to glass for a magnetic recording medium substrate, which comprises essential components in the form of SiO2, Li2O, Na2O, and one or more alkaline earth metal oxides selected from the group consisting of MgO, CaO, SrO, and BaO wherein a molar ratio of a content of CaO to a combined content of MgO, CaO, SrO, and BaO (CaO/(MgO+CaO+SrO+BaO)) is equal to or less than 0.20, and which has a glass transition temperature of equal to or higher than 650° C.
Abstract:
An optical element includes a glass body including a colored layer provided inside the glass body and positioned outside an effective aperture of the optical element. An optical apparatus including the optical element is also provided.
Abstract:
An aspect of the present invention relates to glass for a magnetic recording medium substrate, which includes essential components in the form of SiO2, Li2O, Na2O, and one or more alkaline earth metal oxides selected from the group consisting of MgO, CaO, SrO, and BaO, wherein a molar ratio of a content of MgO to a combined content of MgO, CaO, SrO, and BaO (MgO/(MgO+CaO+SrO+BaO)) is equal to or greater than 0.80, and which has a Young's modulus of equal to or greater than 80 GPa, and a glass transition temperature of equal to or greater than 620° C.