摘要:
Catalyst particles of an active material of the general formula[Mo,V,W].sub.12 Bi.sub.a [Fe,Ce].sub.b [Ni,Co,Zn].sub.C [Alkali].sub.d [P,As,Sb,B].sub.e [Si,Al,Ti].sub.f O.sub.xwherea is from 0.1 to 5,b is from 0.1 to 10,c is from 1 to 15,d is from 0.01 to 2,e is from 0 to 2,f is from 0 to 30 andx is the number of oxygen atoms required to saturate the valences of the other components,have the shape of a 3-spoked to 5-spoked wheel or of a rosette which have wall thicknesses of from 0.5 to 4 mm and a diameter of from 3 to 20 mm.
摘要翻译:具有通式[Mo,V,W] 12Bia [Fe,Ce] b [Ni,Co,Zn] C [Al]的[P,As,Sb,B] e [Si,Al ,Ti] fOx,其中a为0.1至5,b为0.1至10,c为1至15,d为0.01至2,e为0至2,f为0至30,x为 使其它组分的价态饱和所需的氧原子数为3-壁的5-发轮或玫瑰花的形状,其壁厚为0.5-4毫米,直径为3-20毫米 。
摘要:
A silver catalyst containing one or more alkali metals and also tungsten as promotors for the direct oxidation of ethylene with oxygen to form ethylene oxide, on a porous support substantially consisting of .alpha.-aluminum oxide and having a specific surface area (BET) of from 0.3 to 3 m.sup.2 /g, which contains tungsten in a concentration of from 60 to 330 ppmwt, based on the total catalyst, per m.sup.2 of surface area for each gram of supporting material.
摘要:
Supported silver catalysts which contain one or more alkali metals are prepared in a two-stage process by doping a basic catalyst which contains silver in metallic form and may also contain lithium with the heavy alkali metal sodium, potassium, rubidium and/or cesium using an impregnating solution which contains the heavy alkali metal and one or more nitrates of the general formulaR.sup.+ NO.sub.3.sup.-wherein R.sup.+ is an ammonium, hydrazinium, C.sub.1 -C.sub.12 -monoalkylammonium, C.sub.2 -C.sub.12 -dialkylammonium, C.sub.3 -C.sub.12 -trialkylammonium or C.sub.4 -C.sub.12 -tetraalkylammonium cation.
摘要翻译:含有一种或多种碱金属的负载型银催化剂通过掺杂含有金属形式的银的碱性催化剂并且还可以使用重质碱金属钠,钾,铷和/或铯来包含锂,通过两步法制备。 含有重质碱金属和一种或多种通式为R + NO 3 - 的硝酸盐的浸渍溶液,其中R +是铵,肼,C1-C12-单烷基铵,C2-C12-二烷基铵,C3-C12-三烷基铵或C4-C12 四烷基铵阳离子。
摘要:
A molded supported catalyst which contains from 2 to 13% by weight of copper ions in the form of copper(II) chloride and/or copper oxychloride and from 0.2 to 3% by weight of alkali metal ion on a columnar carrier and has a diameter of from 4 to 7 mm and a height which is from 0.35 to 0.75 times the diameter is particularly suitable for preparing 1,2-dichloroethane by oxychlorination of ethylene.
摘要:
A honeycomb catalyst consisting of from 30 to 95% by weight, calculated as Fe.sub.2 O.sub.3, of an iron compound and from 0.1 to 60% by weight, calculated as Al.sub.2 O.sub.3, CeO.sub.2 or Cr.sub.2 O.sub.3, of an aluminum, cerium and/or chromium compound and/or from 1 to 50% by weight of an alkali metal compound, in particular potassium, calculated as K.sub.2 O, and/or from 0.2 to 20% by weight, calculated as MeO.sub.3, of an element of sub-group 6, preferably MoO.sub.3 and WO.sub.3, and/or from 0.1 to 20% by weight, calculated as V.sub.2 O.sub.5, of a compound of vanadium and/or from 0.1 to 20% by weight, calculated as P.sub.2 O.sub.5, of a compound of phosphorus, a process for the preparation of the honeycomb catalyst, and the use of the catalyst for organic reactions.
摘要翻译:一种蜂窝状催化剂,其以Al 2 O 3,CeO 2或Cr 2 O 3计算的铝,铈和/或铬化合物和/或铬化合物计为30至95重量%,以Fe 2 O 3计,铁化合物和0.1至60重量% 或1至50重量%的碱金属化合物,特别是钾(以K 2 O计)和/或0.2至20重量%(以MeO 3计),为第6族元素,优选MoO 3和WO 3 ,和/或0.1至20重量%,以V 2 O 5计,钒化合物和/或按重量计0.1至20重量%的磷化合物,磷化合物的制备方法 催化剂和催化剂用于有机反应。
摘要:
A silver catalyst containing lithium and cesium as promoters for the direct oxidation of ethylene with oxygen to give ethylene oxide is applied to a porous carrier and essentially consists of .alpha.-alumina and contains certain amounts of soluble calcium, aluminum, potassium and sodium salts. The carrier has a BET surface area of from 0.4 to 0.8 m.sup.2 /g, a pore volume of not less than 0.45 ml/g, the pores being equally accessible to cold and warm water, a bulk density of less than 700 kg/m.sup.3 and a shape which, in the reactor, provides a geometrical surface area of not less than 600 m.sup.2 /m.sup.3, on which more than 13% by weight of silver are applied as active component and more than 115 kg of silver are available per m.sup.3 of reactor, and from 100 to 300 ppm by weight of lithium and from 200 to 600 ppm by weight of cesium are present as promoters. A process for the preparation of the silver catalyst and its use for the oxidation of ethylene are described.
摘要翻译:含有锂和铯作为用于直接氧化乙烯以产生环氧乙烷的促进剂的银催化剂被施加到多孔载体上,并且基本上由α-氧化铝组成并含有一定量的可溶性钙,铝,钾和钠盐。 载体的BET表面积为0.4至0.8m2 / g,孔体积不低于0.45ml / g,孔隙对于冷和热水均等可及,堆积密度小于700kg / m 3, 在反应器中,形成不小于600m 2 / m 3的几何表面积的形状,其上以13重量%以上的银作为活性组分,每立方米反应器可获得超过115kg的银 和100〜300重量ppm的锂和200〜600重量ppm的铯作为助催化剂存在。 描述了用于制备银催化剂的方法及其用于乙烯氧化的用途。
摘要:
1,4-Diacyloxybut-2-enes and 3,4-diacyloxybut-1-enes are converted into one another in the gas phase or liquid phase at from 100.degree. to 350.degree. C. under atmospheric or superatmospheric pressure in the presence of a zeolite as a catalyst.
摘要:
A silver catalyst for the direct oxidation of ethylene with oxygen to give ethylene oxide is applied on a porous carrier and essentially consists of .alpha.-alumina and contains certain amounts of soluble calcium, aluminum, potassium and sodium salts. The carrier has a BET surface area of from 0.2 to 0.8 m.sup.2 /g, a pore volume of not less than 0.5 ml/g, the pores being equally accessible to cold and warm water, and a bulk density of less than 650 kg/m.sup.3, and has a shape which, in the reactor, provides a geometric surface area of not less than 600 m.sup.2 /m.sup.3, on which more than 13% by weight of silver are applied as the active component, more than 110 kg of silver being available per m.sup.3 of reactor.
摘要翻译:用于用氧直接氧化乙烯以产生环氧乙烷的银催化剂被施加到多孔载体上,并且基本上由α-氧化铝组成并含有一定量的可溶性钙,铝,钾和钠盐。 载体的BET表面积为0.2至0.8m2 / g,孔体积不小于0.5ml / g,孔隙对于冷和温水均等可及,并且堆积密度小于650kg / m 3 ,并且具有在反应器中提供不小于600m 2 / m 3的几何表面积的形状,其上施加超过13重量%的银作为活性组分,可获得超过110kg的银 每立方米反应堆。
摘要:
C.sub.2 -C.sub.4 -olefins are prepared by catalytic conversion of methanol and/or dimethyl ether in the presence of a zeolite catalyst at elevated temperatures, by a process in which the catalyst used is a pure borosilicate zeolite which has been tableted or extruded without a binder and treated with hydrofluoric acid and hydrochloric acid. The treatment of the catalyst with hydrofluoric acid is carried out using 0.001-1N HF, and that with hydrochloric acid is carried out using 3-25% strength acid. The time-on-stream of the catalyst is improved.
摘要:
Olefins are prepared by converting methanol and/or dimethyl ether in the presence of a zeolite catalyst at elevated temperatures by a process wherein the catalyst used is a borosilicate zeolite which has been molded together with an amorphous binder containing aluminum oxide and silicon dioxide. The advantage of using the borosilicate catalyst is that the yield of C.sub.2 -C.sub.4 -olefins is improved at the expense of formation of higher hydrocarbons.