Lead battery and lead battery storage method
    1.
    发明申请
    Lead battery and lead battery storage method 失效
    铅电池和铅蓄电池存储方式

    公开(公告)号:US20070184349A1

    公开(公告)日:2007-08-09

    申请号:US10588849

    申请日:2005-03-17

    摘要: This invention provides a lead battery that becomes usable by injecting an electrolyte thereinto. The battery includes: positive and negative electrode plates each having a grid comprising a Pb—Ca based alloy; separators that separate the positive electrode plates from the negative electrode plates; the electrolyte comprising sulfuric acid; and a battery container accommodating the positive and negative electrode plates, the separators, and the electrolyte. The battery container is sealed, and part of the positive and negative electrode plates is immersed in the electrolyte. The height Y0 of the positive and negative electrode plates and the distance Y1 from the bottom of the positive and negative electrode plates to the level of the electrolyte satisfy the relation: 15≦Y1/Y0×100≦60.

    摘要翻译: 本发明提供一种通过向其中注入电解质而可用的铅电池。 电池包括:正极板和负极板,每个板具有包含Pb-Ca基合金的栅格; 将正极板与负极板分离的分离器; 所述电解质包含硫酸; 以及容纳正极板和负极板,隔板和电解质的电池容器。 将电池容器密封,将正极板和负极板的一部分浸入电解液中。 正极板和负极板的高度Y 0 <0>和从正极板和负极板的底部到电解液层的距离Y 1 <1>满足以下关系: <?in-line-formula description =“In-line Formulas”end =“lead”?> 15 <= Y / Y x100 <= 60。 ?in-line-formula description =“In-line Formulas”end =“tail”?>

    Lead battery and lead battery storage method
    2.
    发明授权
    Lead battery and lead battery storage method 失效
    铅电池和铅蓄电池存储方式

    公开(公告)号:US07879490B2

    公开(公告)日:2011-02-01

    申请号:US10588849

    申请日:2005-03-17

    摘要: This invention provides a lead battery that becomes usable by injecting an electrolyte thereinto. The battery includes: positive and negative electrode plates each having a grid comprising a Pb—Ca based alloy; separators that separate the positive electrode plates from the negative electrode plates; the electrolyte comprising sulfuric acid; and a battery container accommodating the positive and negative electrode plates, the separators, and the electrolyte. The battery container is sealed, and part of the positive and negative electrode plates is immersed in the electrolyte. The height Y0 of the positive and negative electrode plates and the distance Y1 from the bottom of the positive and negative electrode plates to the level of the electrolyte satisfy the relation: 15≦Y1/Y0×100≦60.

    摘要翻译: 本发明提供一种通过向其中注入电解质而可用的铅电池。 电池包括:正极板和负极板,每个板具有包含Pb-Ca基合金的栅格; 将正极板与负极板分离的分离器; 所述电解质包含硫酸; 以及容纳正极板和负极板,隔板和电解质的电池容器。 将电池容器密封,将正极板和负极板的一部分浸入电解液中。 正极板和负极板的高度Y0以及从正极板和底板的底部到电解液层的距离Y1满足关系式:15&nlE; Y1 / Y0×100&nlE; 60。