摘要:
There is provided a steam turbine blade made of Ti-base alloy comprising an &agr;+&bgr; type phase in which a difference of a tensile strength is small between a blade portion and a dovetail portion, a tensile strength at a room temperature of the dovetail portion is equal to or more than 100 kg/mm2 and a suitable toughness is commonly provided together with a strength, as a steam turbine blade having a length of 43 inch or more, a method of manufacturing the same, a steam turbine power generating plant and a low pressure steam turbine. In the steam turbine blade having a blade portion and a plurality of fork type dovetails, wherein the blade is made of Ti-base alloy structured such that a length of the blade portion is equal to or more than 52 inches with respect to a rotational speed 3000 rpm of the blade or equal to or more than 43 inches with respect to the rotational speed 3600 rpm, and a tensile strength at a room temperature of the dovetail is equal to or more than 100 kg/mm2, preferably equal to or more than 110 kg/mm2 and equal to or more than 96% of the tensile strength at the room temperature of the blade portion.
摘要:
A steam turbine blade made of Ti-base alloy comprising an &agr;+&bgr; type phase in which a difference of a tensile strength is small between a blade portion and a dovetail portion, a tensile strength at a room temperature of the dovetail portion is equal to or more than 100 kg/mm2 and a suitable toughness is commonly provided together with a strength, as a steam turbine blade having a length of 43 inch or more, a method of manufacturing the same, a steam turbine power generating plant and a low pressure steam turbine. In the steam turbine blade having a blade portion and a plurality of fork type dovetails, wherein the blade is made of Ti-base alloy structured such that a length of the blade portion is equal to or more than 52 inches with respect to a rotational speed 3000 rpm of the blade or equal to or more than 43 inches with respect to the rotational speed 3600 rpm, and a tensile strength at a room temperature of the dovetail is equal to or more than 100 kg/mm2, preferably equal to or more than 110 kg/mm2 and equal to or more than 96 % of the tensile strength at the room temperature of the blade portion.
摘要:
A steam turbine in which principal components to be exposed to high temperatures are all made of ferritic steel, whereby the temperatures of main steam and reheat steam can be increased to 610-660 (.degree.C.). The rotor shaft (23 in FIG. 1) of the steam turbine is made of ferritic forged steel whose 100,000-hour creep rupture strength is at least 15 (kg/mm.sup.2) at the service temperature of the rotor shaft. Likewise, the casing (18) is made of ferritic cast steel whose 100,000-hour creep rupture strength is at least 10 (kg/mm.sup.2). The steam turbine of high thermal efficiency can be applied to a steam-turbine power plant.
摘要翻译:其中主要组分暴露在高温下的汽轮机全部由铁素体钢制成,主蒸汽和再热蒸汽的温度可以提高到610-660(℃)。 蒸汽轮机的转子轴(图1中的23)由铁素体锻钢制成,其在转子轴的使用温度下的100,000小时蠕变断裂强度为至少15(kg / mm 2)。 同样,壳体(18)由铁素体铸钢制成,其100,000小时蠕变断裂强度至少为10(kg / mm2)。 具有高热效率的蒸汽轮机可以应用于蒸汽轮机发电厂。
摘要:
A steam turbine in which principal components to be exposed to high temperatures are all made of ferritic steel, whereby the temperatures of main steam and reheat steam can be increased to 610-660 (° C.). The rotor shaft (23 in FIG. 1) of the steam turbine is made of ferritic forged steel whose 100,000-hour creep rupture strength is at least 15 (kg/mm2) at the service temperature of the rotor shaft. Likewise, the casing (18) is made of ferritic cast steel whose 100,000-hour creep rupture strength is at least 10 (kg/mm2). The steam turbine of high thermal efficiency can be applied to a steam-turbine power plant.
摘要翻译:一个蒸汽轮机,其主要部件暴露在高温下均由铁素体钢制成,主蒸汽和再热蒸汽的温度可以提高到610-660(℃)。 蒸汽轮机的转子轴(图1中的23)由铁素体锻钢制成,其在转子轴的使用温度下的100,000小时蠕变断裂强度为至少15(kg / mm 2)。 同样,壳体(18)由铁素体铸钢制成,其100,000小时蠕变断裂强度至少为10(kg / mm2)。 具有高热效率的蒸汽轮机可以应用于蒸汽轮机发电厂。
摘要:
A steam turbine includes a rotor shaft, movable blades assembled on the rotor shaft, fixed blades for guiding inflow of steam to the moving blades, and an inner casing for holding the fixed blades. The rotor shaft and at least a first stage of the movable blades are made of high-strength martensitic steel comprising 0.05-0.20(%) of C, at most 0.15(%) of Si, 0.3-0.7(%) of Mn, 9.5-13(%) of Cr, 0.3-0.7(%) of Ni, 0.05-0.35(%) of V, 0.02-0.15(%) of Nb, 0.01-0.06(%) of N, 0.05-0.5(%) of Mo, 1.0-3.5(%) of W, 2-10(%) of Co and 0.0005-0.03(%) of B and at least 78(%) of Fe (the percentages being given in terms of weight). The inner casings is made of martensitic cast steel comprising 0.06-0.16(%) of C, at most 0.5(%) of Si, at most 1(%) of Mn, 0.2-1.0(%) of Ni, 8-12(%) of Cr, 0.05-0.35(%) of V, 0.01-0.15(%) of Nb, 0.01-0.1(%) of N, at most 1.5% of Mo, 1-4(%) of W and 0.0005-0.03(%) of B and at least 85(%) of Fe (the percentages being given in terms of weight). The rotor shaft has a length of at least 5 (m) and has a minimum diameter of at least 600 (mm) at a portion where the fixed blades are assembled. The first stage of said moving blades has a length of at least 35 (mm) at a blade portion thereof.
摘要:
The present invention relates to a steam turbine comprising a rotor shaft integrating high and low pressure portions provided with blades at the final stage thereof having a length not less than 30 inches, wherein a steam temperature at first stage blades is 530.degree. C., a ratio (L/D) of a length (L) defined between bearings of the rotor shaft to a diameter (D) measured between the terminal ends of final stage blades is 1.4 to 2.3. This rotor shaft is composed of heat resisting steel containing by weight 0.15 to 0.4 % C, not more than 0.1 % Si, 0.05 to 0.25 % Mn, 1.5 to 2.5 % Ni, 0.8 to 2.5 % Cr, 0.8 to 2.5 % Mo and 0.15 to 0.35 % V and, further, the heat resisting steel may contain at least one of Nb, Ta, W, Ti, Al, Zr, B, Ca, and rare earth elements.
摘要:
A steam turbine comprising a rotor shaft integrating high and low pressure portions provided with blades at the final stage thereof having a length not less than 30 inches, wherein a steam temperature at first stage blades is 530° C., a ratio (L/D) of a length (L) defined between bearings of the rotor shaft to a diameter (D) measured between the terminal ends of final stage blades is 1.4 to 2.3. This rotor shaft is composed of heat resisting steel containing by weight 0.15 to 0.4% C, not more than 0.1% Si, 0.05 to 0.25% Mn, 1.5 to 2.5% Ni, 0.8 to 2.5% Cr, 0.8 to 2.5% Mo and 0.15 to 0.35% V and, further, the heat resisting steel may contain at least one of Nb, Ta, W, Ti, Al, Zr, B, Ca, and rare earth elements.
摘要翻译:一种蒸汽轮机,包括集成高压部分和低压部分的转子轴,所述转子轴在其最后阶段具有不小于30英寸的长度,其中第一级叶片处的蒸汽温度为530℃,比率(L / D 限定在转子轴的轴承之间的长度(L)与在最终级叶片的末端之间测量的直径(D)为1.4至2.3。 该转子轴由含有0.15〜0.4%C,0.1%以下的Si,0.05〜0.25%的Mn,1.5〜2.5%的Ni,0.8〜2.5%的Cr,0.8〜2.5%的Mo和0.15重量的耐热钢构成。 至0.35%V,此外,耐热钢可以含有Nb,Ta,W,Ti,Al,Zr,B,Ca和稀土元素中的至少一种。
摘要:
The present invention relates to a steam turbine comprising a rotor shaft integrating high and low pressure portions provided with blades at the final stage thereof having a length not less than 30 inches, wherein a steam temperature at first stage blades is 530.degree. C., a ratio (L/D) of a length (L) defined between bearings of the rotor shaft to a diameter (D) measured between the terminal ends of final stage blades is 1.4 to 2.3. This rotor shaft is composed of heat resisting steel containing by weight 0.15 to 0.4% C, not more than 0.1% Si, 0.05 to 0.25% Mn, 1.5 to 2.5% Ni, 0.8 to 2.5% Cr, 0.8 to 2.5% Mo and 0.15 to 0.35% V and, further, the heat resisting steel may contain at least one of Nb, Ta, W, Ti, Al, Zr, B, Ca, and rare earth elements.
摘要:
The present invention relates to a steam turbine comprising a rotor shaft integrating high and low pressure portions provided with blades at the final stage thereof having a length not less than 30 inches, wherein a steam temperature at first stage blades is 530.degree. C., a ratio (L/D) of a length (L) defined between bearings of the rotor shaft to a diameter (D) measured between the terminal ends of final stage blades is 1.4 to 2.3. This rotor shaft is composed of heat resisting steel containing by weight 0.15 to 0.4% C, not more than 0.1% Si, 0.05 to 0.25% Mn, 1.5 to 2.5% Ni, 0.8 to 2.5% Cr, 0.8 to 2.5% Mo and 0.15 to 0.35% V and, further, the heat resisting steel may contain at least one of Nb, Ta, W, Ti, Al, Zr, B, Ca, and rare earth elements.
摘要:
The present invention relates to a steam turbine comprising a rotor shaft integrating high and low pressure portions provided with blades at the final stage thereof having a length not less than 30 inches, wherein a steam temperature at first stage blades is 530.degree. C., a ratio (L/D) of a length (L) defined between bearings of the rotor shaft to a diameter (D) measured between the terminal ends of final stage blades is 1.4 to 2.3. This rotor shaft is composed of heat resisting steel containing by weight 0.15 to 0.4% C, not more than 0.1% Si, 0.05 to 0.25% Mn, 1.5 to 2.5% Ni, 0.8 to 2.5% Cr, 0.8 to 2.5% Mo and 0.15 to 0.35% V and, further, the heat resisting steel may contain at least one of Nb, Ta, W, Ti, Al, Zr, B, Ca, and rare earth elements.