METHOD FOR PRODUCING CROSSLINKED POLYMER, CROSSLINKED POLYMER, AND COATING COMPOSITION CONTAINING THE SAME
    7.
    发明申请
    METHOD FOR PRODUCING CROSSLINKED POLYMER, CROSSLINKED POLYMER, AND COATING COMPOSITION CONTAINING THE SAME 有权
    生产交联聚合物,交联聚合物和含有它的涂料组合物的方法

    公开(公告)号:US20140187710A1

    公开(公告)日:2014-07-03

    申请号:US14141933

    申请日:2013-12-27

    IPC分类号: C09D143/02

    摘要: The object of the present disclosure is to provide a method for producing a crosslinked polymer by radical polymerization of a monomer composition, by which method a desired crosslinked polymer can be produced in a high solid content with good productivity (also at a low production cost), and a crosslinked polymer obtained by the production method and a coating composition containing the same. A method for producing a crosslinked polymer having a weight average molecular weight of 15000 to 200000, the method comprising step [I] of obtaining a crosslinked polymer (A) by conducting polymerization of a monomer composition comprising 2 to 30% by weight of a polyfunctional methacrylate having 2 to 4 functional groups (a) and 98 to 70% by weight of one or more polymerizable monomers selected from the group consisting of monofunctional (meth)acrylates, (meth)acrylic acid, and monofunctional vinyl aromatic compounds (b) in an organic solvent in the presence of a radical polymerization initiator in a temperature region where the radical polymerization initiator comes to have a half-life of 4 to 18 minutes.

    摘要翻译: 本公开的目的是提供一种通过单体组合物的自由基聚合制备交联聚合物的方法,通过该方法,可以以高生产率(也以低生产成本)生产高固含量的所需交联聚合物, ,以及通过该制造方法得到的交联聚合物和含有该交联聚合物的涂料组合物。 一种重均分子量为15000〜200000的交联聚合物的制造方法,其特征在于,包括通过聚合含有2〜30重量%的多官能团的单体组合物来获得交联聚合物(A)的步骤[I] 具有2〜4个官能团(a)的甲基丙烯酸酯和98〜70重量%的选自单官能(甲基)丙烯酸酯,(甲基)丙烯酸和单官能乙烯基芳族化合物(b))中的一种或多种可聚合单体 在自由基聚合引发剂存在下,在自由基聚合引发剂的半衰期为4〜18分钟的温度范围内的有机溶剂。

    BELT ASSEMBLY, IMAGE-FORMING APPARATUS, AND METHOD FOR MANUFACTURING THE BELT ASSEMBLY
    8.
    发明申请
    BELT ASSEMBLY, IMAGE-FORMING APPARATUS, AND METHOD FOR MANUFACTURING THE BELT ASSEMBLY 审中-公开
    皮带组装,成像装置和制造带组件的方法

    公开(公告)号:US20150004416A1

    公开(公告)日:2015-01-01

    申请号:US14313071

    申请日:2014-06-24

    IPC分类号: B32B9/04 G03G15/01 B29C47/00

    摘要: A belt assembly is disclosed. The belt assembly comprises an incompatible-polymer alloy including at least one crystalline resin which is selected from polyphenylene sulfide, polyetheretherketone, and polyvinylidene difluoride and at least one amorphous resin which is selected from polyethersulfone and polycarbonate, polyphenyleneether, polysulfone, and polyarylate. Wherein the weight ratio between the crystalline resin and the amorphous resin is from 70:30 to 95:5, carbon as a first conductive agent is distributed unevenly only in a successive layer, at least a second conductive agent which is selected from ZnO particles, SnO2 particles. Sb-doped SnO2 particles, In-doped SnO2 particles, P-doped SnO2 particles and metal-oxide particles covered by one of these particles is distributed unevenly only in the successive layer, and a flame-resistance value of the belt is VTM-0 under a condition that a thickness thereof is from 50 [μm] to 150 [μm] at a UL 94 standard.

    摘要翻译: 公开了一种皮带组件。 带组件包括不对称聚合物合金,其包括选自聚苯硫醚,聚醚醚酮和聚偏二氟乙烯中的至少一种结晶树脂和选自聚醚砜和聚碳酸酯,聚苯醚,聚砜和聚芳酯中的至少一种无定形树脂。 其中,所述结晶性树脂与所述无定形树脂的重量比为70:30〜95:5,作为第一导电剂的碳仅在连续层中分布不均匀,至少第二导电剂选自ZnO颗粒, SnO2颗粒。 Sb掺杂的SnO 2颗粒,In掺杂的SnO 2颗粒,P掺杂的SnO 2颗粒和由这些颗粒之一覆盖的金属氧化物颗粒仅在连续层中分布不均匀,并且带的阻燃值为VTM-0 在UL94标准下,其厚度为50μm至150μm的条件。