Abstract:
Provided is a polycarbonate-based resin composition containing a polycarbonate-based resin containing a polycarbonate-polyorganosiloxane copolymer, and 0.01 to 1.0 part by mass of a UV absorber with respect to 100 parts by mass of the polycarbonate-based resin, in which the molecular weight distribution of a polyorganosiloxane block in the polycarbonate-polyorganosiloxane copolymer is controlled within a specific region.
Abstract:
A polycarbonate-polyorganosiloxane copolymer comprises a polycarbonate block (A-1) formed of a repeating unit with a specific structure and a polyorganosiloxane block (A-2) containing a repeating unit with a specific structure. A difference between the haze value (haze A) after retention for 3 minutes and the haze value (haze B) after retention for 20 minutes, of the polycarbonate-polyorganosiloxane copolymer or a resin composition thereof at 300° C. or 340° C., Δhaze, is less than 0.4.
Abstract:
Provided is a polycarbonate resin for a liquid crystal member, which is produced by using an end terminator containing 3-pentadecylphenol obtained from a natural product, and which has a YI value of 1.1 or less or a light transmittance at a wavelength of 400 nm of 85% or more.
Abstract:
Provided are a polycarbonate-based resin composition, including: 99 mass % to 1 mass % of a polycarbonate-polyorganosiloxane copolymer (A) having a predetermined repeating unit (A-1) and predetermined constituent units (A-2) and (A-3); and 1 mass % to 99 mass % of a polycarbonate-based resin (B) except the polycarbonate-polyorganosiloxane copolymer (A), and a molded body thereof.
Abstract:
Provided is a polycarbonate-based resin composition containing: a polycarbonate-polyorganosiloxane copolymer (A-1) which contains a specific repeating unit and in which a polyorganosiloxane block has an average chain length of 20 or more and less than 60; a polycarbonate-polyorganosiloxane copolymer (A-2) which contains a specific repeating unit and in which a polyorganosiloxane block has an average chain length of 60 or more and less than 500; and a polycarbonate-based resin (A-3) except the polycarbonate-polyorganosiloxane copolymer (A-1) and the polycarbonate-polyorganosiloxane copolymer (A-2), wherein the ratio of the polycarbonate-based resin (A-3) to the total weight of the polycarbonate-polyorganosiloxane copolymer (A-1), the polycarbonate-polyorganosiloxane copolymer (A-2), and the polycarbonate-based resin (A-3) is 10 mass % or more.
Abstract:
Provided is a polycarbonate-based resin composition containing a polycarbonate-based resin containing a predetermined polycarbonate-polyorganosiloxane copolymer, and 0.5 to 5 parts by mass of a white pigment with respect to 100 parts by mass of the polycarbonate-based resin, in which the molecular weight distribution of a polyorganosiloxane block in the polycarbonate-polyorganosiloxane copolymer is controlled within a specific region.
Abstract:
Provided is a carbonate-olefin-based copolymer including a polycarbonate block, an olefin-based polymer block, and a specific constituent unit.
Abstract:
Provided is a polycarbonate-based resin composition, including: 10 to 90 mass % of a polycarbonate-polyorganosiloxane copolymer (E-1); and 10 to 90 mass % of an aromatic polycarbonate resin (E-2) except the polycarbonate-polyorganosiloxane copolymer (E-1), in which the molecular weight distribution of the polyorganosiloxane block of the polycarbonate-polyorganosiloxane copolymer is controlled within a specific region.
Abstract:
Provided is a polycarbonate-polyorganosiloxane copolymer, including a specific polycarbonate block unit (A) and a specific polyorganosiloxane block unit (B), in which in a differential molecular weight distribution curve obtained from measurement of the polyorganosiloxane block unit (B) by gel permeation chromatography using the polystyrene calibration curve, the curve having an axis of abscissa indicating a logarithmic value log(M) of a molecular weight M and an axis of ordinate indicating dw/d log(M) obtained by differentiating a concentration fraction w with respect to the logarithmic value log(M) of the molecular weight, (1) a dw/d log(M) value becomes maximum in a range of 3.4≦log(M)≦4.0, and (2) in the differential molecular weight distribution curve, a ratio of a value obtained by integrating the dw/d log(M) value over a range of 4.0≦Log(M)≦4.5 to a value obtained by integrating the dw/d log(M) value over the entire range of the log(M) is 6% or more and 40% or less.
Abstract translation:提供了聚碳酸酯 - 聚有机硅氧烷共聚物,其包括特定的聚碳酸酯嵌段单元(A)和特定的聚有机硅氧烷嵌段单元(B),其中通过凝胶渗透法测定聚有机硅氧烷嵌段单元(B)得到的微分分子量分布曲线 使用聚苯乙烯校准曲线的色谱法,具有表示分子量M的对数值log(M)和表示dw / d log(M)的纵坐标轴的横坐标轴的曲线表示通过将浓度分数w相对于 分子量的对数值log(M),(1)dw / d log(M)值在3.4≦̸ log(M)≦̸ 4.0和(2)的范围内变为最大,差示分子量 分布曲线,通过将dw / d log(M)值在4.0≦̸ Log(M)≦̸ 4.5的范围内积分得到的值的比率与通过将dw / d log(M)值相乘得到的值 对数(M)的整个范围为6%以上且40%以上 ss。