Abstract:
The invention concerns a process for the preparation of a catalyst based on tungsten intended for hydrotreatment or hydrocracking processes.The invention concerns a process for the preparation of a catalyst for carrying out hydrogenation reactions in hydrotreatment and hydrocracking processes. Said catalyst is prepared from at least one mononuclear precursor compound based on tungsten (W), in its monomeric or dimeric form, having at least one W═O or W—OR bond or at least one W═S or W—SR bond where [R═CxHy where x≧1 and (x−1)≦y≦(2x+1) or R═Si(OR′)3 or R═Si(R′)3 where R′═Cx′Hy′ where x′≧1 and (x′−1)≦y′≦(2×t+1)], optionally at least one Mo precursor and optionally at least one promoter element from group VIII. Said precursors are deposited onto an oxide support which is suitable for the process in which it is used, said catalyst advantageously being sulphurized before being deployed in said process.
Abstract:
The invention relates to a method for selective hydrogenation of a hydrocarbon feedstock that contains at least 2 carbon atoms per molecule and that has a final boiling point that is less than or equal to 250° C. and that comprises at least one polyunsaturated compound, in which in the presence of hydrogen, said feedstock is brought into contact with at least one catalyst that comprises a substrate and an active metal phase deposited on said substrate; said active metal phase comprises copper and at least one metal that is selected from between nickel and cobalt in a molar ratio of Cu:(Ni and/or Co) of greater than 1.
Abstract:
The invention concerns a process for the preparation of a catalyst for carrying out hydrogenation reactions in hydrotreatment and hydrocracking processes. Said catalyst is prepared from at least one mononuclear precursor based on molybdenum (Mo), in its monomeric or dimeric form, having at least one Mo═O or Mo—OR bond or at least one Mo═S or Mo—SR bond where [R═CxHy where x≧1 and (x−1)≦y≦(2x+1) or R═Si(OR′)3 or R═Si(R′)3 where R′═Cx′Hy′ where x′≧1 and (x′−1)≦y′≦(2x′+1)], and optionally from at least one promoter element from group VIII. Said precursors are deposited onto an oxide support which is suitable for the process in which it is used, said catalyst being dried at a temperature of less than 200° C. then advantageously being sulphurized before being deployed in said process.
Abstract:
The invention concerns a method for selectively hydrogenating a hydrocarbon charge containing at least two carbon atoms per molecule, having a final boiling point which is less than or equal to 250° C., and comprising at least one polyunsaturated compound, wherein the charge, in the presence of hydrogen, is brought into contact with at least one catalyst comprising a carrier and an active metal phase deposited on the carrier, the active metal phase comprising iron and at least one metal selected from zinc and copper in a molar ratio of Fe:(Zn and/or Cu) of between 0.35 and 0.99.