公开(公告)号:US20240336726A1
公开(公告)日:2024-10-10
申请号:US18620458
申请日:2024-03-28
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Che-Tseng LIN , Kai-Chuan KUO , Jen-Chun CHIU
IPC: C08G63/183 , C08J9/00
CPC classification number: C08G63/183 , C08J9/00 , C08J2367/02
Abstract: A copolyester is formed by reacting 100 parts by weight of a polyester elastomer and 0.01 to 0.29 parts by weight of a compound having multi-functional groups. The polyester elastomer is formed by reacting polyethylene terephthalate, diol, and poly(alkylene ether)glycol. The polyethylene terephthalate and the diol have a weight ratio of 1:0.6 to 1:3, and the polyethylene terephthalate and the poly(alkylene ether) glycol have a weight ratio of 1:0.05 to 1:3.
-
公开(公告)号:US20240239986A1
公开(公告)日:2024-07-18
申请号:US18414890
申请日:2024-01-17
Applicant: INDUSTRIAL TECHNOLOGY RESEARCH INSTITUTE
Inventor: Che-Tseng LIN , Meng-Hsin CHEN , Jen-Chun CHIU , Kai-Chuan KUO , Yu-Lin CHU , Po-Hsien HO , Ke-Hsuan LUO , Chih-Hsiang LIN , Hui-Ching HSU
IPC: C08J11/24 , C08G63/183 , C09J167/02
CPC classification number: C08J11/24 , C08G63/183 , C09J167/02 , C08J2367/02
Abstract: A copolyester is formed by copolymerizing a depolymerized polyester and succinic acid. The depolymerized polyester includes depolymerized polyethylene terephthalate (PET), and the depolymerized PET is formed by depolymerizing PET with ethylene glycol. The repeating unit of PET and the succinic acid have a molar ratio of 40:60 to 50:50. The repeating unit of PET and the ethylene glycol have a molar ratio of 100:100 to 100:500. The copolyester has a storage modulus of 1*104 Pa to 1*106 Pa at 80° C. The copolyester can be used in a hot melt adhesive.
-