公开(公告)号:US11643519B2
公开(公告)日:2023-05-09
申请号:US16348410
申请日:2017-11-08
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
IPC分类号: C08J9/22 , A43B13/04 , B29C44/34 , C08J9/18 , B29C44/00 , C08J9/12 , B29K23/00 , B29K105/00 , B29K105/04 , B29L31/50
CPC分类号: C08J9/22 , A43B13/04 , B29C44/00 , B29C44/3461 , C08J9/12 , C08J9/18 , B29K2023/08 , B29K2105/0085 , B29K2105/046 , B29L2031/504 , C08J2205/052 , C08J2353/00
摘要: The present invention relates to an expanded beads molded article containing a block copolymer of a polyethylene block and an ethylene-α-olefin copolymer block and having a density of 30 kg/m3 or more and less than 150 kg/m3 and a modulus of repulsion elasticity of 60% or more. The sole member of the present invention includes the expanded beads molded article of the present invention.
-
公开(公告)号:US11466137B2
公开(公告)日:2022-10-11
申请号:US16348108
申请日:2017-11-07
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
IPC分类号: C08J9/228 , C08J9/18 , C08K3/04 , C08K5/3417 , C08J9/16
摘要: The present invention is concerned with expanded beads that are olefin-based thermoplastic elastomer expanded beads containing a coloring agent, wherein an apparent density of the expanded beads is 40 to 300 g/L, and an average surface layer membrane thickness (a) is 3 to 25 μm, and a molded article thereof, and is able to provide expanded beads capable of producing an expanded beads molded article which is excellent in in-mold moldability and excellent in tensile characteristics and an expanded beads molded article using the expanded beads.
-
公开(公告)号:US11225562B2
公开(公告)日:2022-01-18
申请号:US16333479
申请日:2017-09-15
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
摘要: The present invention provides expanded beads comprising a crosslinked multi-block copolymer containing an ethylene block and an ethylene-α-olefin copolymer block, having an apparent density of 40 to 300 g/L, a gel fraction of 30 to 70% by weight by a hot xylene extraction method, an average cell diameter (a) of 50 to 180 μm, and an average surface layer thickness (b) of 3 to 27 μm, and the expanded beads are excellent in in-mold moldability, and can produce an expanded beads molded article being excellent in tensile characteristics in a well balanced manner.
-
公开(公告)号:US11174365B2
公开(公告)日:2021-11-16
申请号:US16344891
申请日:2017-11-02
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
IPC分类号: C08J9/232 , C08J3/20 , C08J9/18 , C08J9/16 , B29B9/12 , B29B7/00 , B29B9/06 , B29C44/34 , B29K23/00 , B29K96/04 , B29K105/00 , B29K105/04 , B29K105/24 , B29B7/38 , B29C44/00
摘要: The present invention is concerned with expanded beads of a block copolymer of a polyethylene block and an ethylene/α-olefin copolymer block, wherein a xylene insoluble fraction (A) of the expanded beads by a hot xylene extraction method is 10 to 70% by weight, and a ratio (A/B) of the xylene insoluble fraction (A) to a xylene insoluble fraction (B) of the expanded beads by a hot xylene extraction method when divided into two equal parts and measured is 1.0 to 1.1, and is able to provide expanded beads with excellent in-mold moldability and an expanded beads molded article with excellent fusion bondability and restorability.
-
公开(公告)号:US11597127B2
公开(公告)日:2023-03-07
申请号:US16348355
申请日:2017-11-08
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
摘要: An expanded beads molded article containing a block copolymer of a polyethylene block and an ethylene-α-olefin copolymer block and having a density of 150 kg/m3 or more and 500 kg/m3 or less and a tensile strength of 0.5 MPa or more.
-
公开(公告)号:US11168194B2
公开(公告)日:2021-11-09
申请号:US16625176
申请日:2018-06-21
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
IPC分类号: C08J9/16
摘要: The present invention relates to thermoplastic olefin elastomer expanded beads, having an average aspect ratio of 1.10 or less and an average circularity of 0.985 or more. The thermoplastic olefin elastomer expanded beads preferably have a crystal structure such that a melting peak inherent in the thermoplastic olefin elastomer (inherent peak) and one or more melting peaks on a higher temperature side than the inherent peak (high temperature peaks) appear on a DSC curve obtained when heating the expanded beads from 23° C. to 200° C. at a heating rate of 10° C./min.
-
公开(公告)号:US10435530B2
公开(公告)日:2019-10-08
申请号:US15572873
申请日:2016-03-28
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
IPC分类号: C08F297/08 , C08J9/18 , C08J9/224 , C08J9/228 , C08J9/12 , C08J9/232 , C08F210/16 , C08L53/00
摘要: An object of the present invention is to provide expanded beads capable of producing an expanded beads molded article that is excellent in in-mold moldability and is excellent with good balance in lightweight property, flexibility, repulsion, restorability, and tensile characteristics, and an expanded beads molded article using the expanded beads. The expanded beads molded article of the present invention is produced by subjecting the crosslinked expanded beads of the present invention, to in-mold molding. The expanded beads molded article of the present invention may have an apparent density of from 40 to 150 g/L.
-
公开(公告)号:US11952474B2
公开(公告)日:2024-04-09
申请号:US17289169
申请日:2019-10-02
申请人: JSP Corporation
发明人: Shota Takagi , Akinobu Hira
CPC分类号: C08J9/18 , C08J9/0061 , C08J9/228 , C08L53/00 , C08J2203/22 , C08J2353/00 , C08J2423/06 , C08L2203/14
摘要: Expanded beads are those including a mixture of an olefin-based thermoplastic elastomer and a polyethylene-based resin, wherein a melt flow rate MFR(I) of the olefin-based thermoplastic elastomer is 2-10 g/10 min; a difference ((MFR(II))−(MFR(I))) between a melt flow rate MFR(II) of the polyethylene-based resin and the melt flow rate MFR(I) of the olefin-based thermoplastic elastomer is 1-35 g/10 min; and a content of the polyethylene-based resin in the mixture is 3-40% by weight.
-
公开(公告)号:US11795286B2
公开(公告)日:2023-10-24
申请号:US16349236
申请日:2017-11-13
申请人: JSP Corporation
发明人: Shota Takagi , Masaharu Oikawa
CPC分类号: C08J9/232 , C08J9/18 , C08J9/228 , C08L53/00 , A43B13/04 , C08J2201/026 , C08J2203/22 , C08J2353/00
摘要: The present invention relates to an in-mold expanded beads molded article of expanded beads of an olefin thermoplastic elastomer, a cushion for shoe sole, and a method of producing expanded beads provided with through-holes and composed of a block copolymer of a polyethylene block and an ethylene/α-olefin copolymer block, and with respect to the in-mold expanded beads molded article of expanded beads of an olefin thermoplastic elastomer, a voidage of the expanded beads molded article is 5 to 40%; a density of the expanded beads molded article is 30 to 150 g/L; and a flexural modulus of the olefin thermoplastic elastomer that constitutes the expanded beads molded article is 10 to 100 MPa.
-
公开(公告)号:US11458710B2
公开(公告)日:2022-10-04
申请号:US17264725
申请日:2019-07-12
申请人: JSP CORPORATION
发明人: Shota Takagi , Akinobu Hira
摘要: A laminated article includes a thermoplastic resin expanded beads molded layer A having a volume Va and a tensile modulus TMa which is 2 to 100 MPa, and a thermoplastic elastomer expanded beads molded layer B having a volume Vb and a tensile modulus TMb which is 0.05 MPa or more and less than 2 MPa, the layers A and B being laminated and bonded to each other. Va:Vb is 90:10 to 50:50 and TMb/TMa is 0.025 or less.
-
-
-
-
-
-
-
-
-