Method of welding with aluminum metal-core weld wire
    1.
    发明授权
    Method of welding with aluminum metal-core weld wire 有权
    铝金属芯焊丝焊接方法

    公开(公告)号:US08975559B1

    公开(公告)日:2015-03-10

    申请号:US10939904

    申请日:2004-09-13

    IPC分类号: B23K35/22

    摘要: Methods for forming an aluminum weld on an aluminum work surface are disclosed. The methods include providing an aluminum metal-core wire having a sheath with an outer surface and a core composition within the sheath, applying a voltage to the aluminum metal-core wire in the vicinity of the aluminum work surface to generate an arc, and melting the wire and the work surface to form the weld. The sheath is formed with an inorganic lubricant on its outer surface and the core composition includes metal powders, metal alloy powders, or combinations thereof and less than about 5% of non-metallic components or non-metallic agents based on the weight of the wire.

    摘要翻译: 公开了在铝工作表面上形成铝焊接的方法。 所述方法包括:提供具有护套的铝金属芯线,其外表面和芯组合物在护套内,向铝工作表面附近的铝金属芯线施加电压以产生电弧,并熔化 电线和工作面形成焊缝。 护套在其外表面上由无机润滑剂形成,并且核心组合物包括金属粉末,金属合金粉末或其组合,并且基于电线重量小于约5%的非金属组分或非金属制剂 。

    Aluminum metal-core weld wire and method for forming the same
    2.
    发明授权
    Aluminum metal-core weld wire and method for forming the same 有权
    铝金属芯焊丝及其形成方法

    公开(公告)号:US06933468B2

    公开(公告)日:2005-08-23

    申请号:US09965142

    申请日:2001-09-27

    IPC分类号: B23K35/02 B23K35/28 B23K35/40

    摘要: An aluminum metal-core weld wire, the sheath being aluminum, the metal-core having a composition that contains primarily metallic alloying powders e.g. Manganese nitride and/or barium. A method for manufacturing aluminum metal-core wire, the method including depositing a core composition onto strip of aluminum, forming strip of aluminum into a tube containing core composition, and applying an inorganic lube to surface of tube, and drawing tube through reducing dies.

    摘要翻译: 铝金属芯焊丝,护套为铝,金属芯具有主要包含金属合金粉末的组成。 氮化锰和/或钡。 一种制造铝金属芯线的方法,该方法包括将芯组合物沉积在铝条上,将铝条形成为含芯组合物的管,并将无机润滑剂涂覆在管表面上,并通过还原模拉伸管。

    Metal-core weld wire for welding galvanized steels
    3.
    发明授权
    Metal-core weld wire for welding galvanized steels 失效
    用于焊接镀锌钢的金属芯焊丝

    公开(公告)号:US5857141A

    公开(公告)日:1999-01-05

    申请号:US661390

    申请日:1996-06-11

    摘要: A metal-core weld wire usable for gas shielded arc welding gapless joints on low carbon and low alloy galvanized and galvanealed steels. The metal-core weld wire includes a low carbon steel sheath surrounding a core composition. In one embodiment, the low carbon steel sheath includes, by total weight of the metal-core weld wire, between approximately 0.01-0.03% C, and the core composition includes, by total weight of the metal-core weld wire, between approximately 0.05-0.20% Ti, between approximately 0.05-1.00% Nb, Fe powder, and Mn to the extent that the metal-core weld wire includes between approximately 0.1-1.0% Mn wherein the metal-core weld wire includes between approximately 0.1-1.0% Si. The core composition is, by total weight of the metal-core weld wire, between approximately 0.001-12.0%. The metal-core weld wire provides, at weld rates up to 150 cm/min, reduced arc ionization potential and spatter, and improved arc stability and shielding. The metal-core weld wire produces, at weld rates up to 150 cm/min, weld deposits having reduced blow holes and porosity, no liquid metal embrittlement, and reduced weld pool surface tension resulting in an improved wetting characteristic.

    摘要翻译: 一种金属芯焊丝,可用于低碳和低合金镀锌和镀锌钢的气体保护电弧焊缝隙接头。 金属芯焊丝包括围绕芯组合物的低碳钢护套。 在一个实施方案中,低碳钢护套包括金属芯焊丝的总重量在约0.01-0.03%C之间,并且芯组合物包括金属芯焊丝的总重量在约0.05 -0.20%的Ti,在约0.05-1.00%的Nb,Fe粉末和Mn之间,金属芯焊丝包括约0.1-1.0%的Mn,其中金属芯焊丝包括在约0.1-1.0% Si。 核心组成是金属芯焊丝的总重量在约0.001-12.0%之间。 金属芯焊丝以高达150厘米/分钟的焊接速率提供减少的电弧电离电位和飞溅,并提高电弧稳定性和屏蔽性。 金属芯焊丝以高达150厘米/分钟的焊接速率生产具有减少的吹气孔和孔隙率的焊接沉积物,没有液体金属脆化,并且减少焊池表面张力,导致改善的润湿特性。

    ADDITION OF RARE EARTH ELEMENTS TO IMPROVE THE PERFORMANCE OF SELF SHIELDED ELECTRODES
    6.
    发明申请
    ADDITION OF RARE EARTH ELEMENTS TO IMPROVE THE PERFORMANCE OF SELF SHIELDED ELECTRODES 有权
    添加稀土元素以提高自屏蔽电极的性能

    公开(公告)号:US20090321404A1

    公开(公告)日:2009-12-31

    申请号:US12147607

    申请日:2008-06-27

    申请人: James M. Keegan

    发明人: James M. Keegan

    IPC分类号: B23K35/24 B23K35/36

    摘要: A self-shielding welding electrode and a method of making the same are provided. The self-shielding welding electrode contains rare earth aluminide in either the flux or the electrode portion of the electrode. The self-shielding welding electrode contains at least about 0.5% by weight of the flux of rare earth aluminide.

    摘要翻译: 提供自屏蔽焊接电极及其制造方法。 自屏蔽焊接电极在电极的焊剂或电极部分中含有稀土铝化物。 自屏蔽焊接电极含有至少约0.5重量%的稀土铝化物焊剂。