Abstract:
It is an object to provide a method of producing a polyester resin composition with improved crystallization, the polyester resin composition making it possible to produce a molded article with reduced appearance defects, such as fish eyes. With the method, a polyester resin composition containing a polyester resin and pentaerythritol is produced, and the method of producing the polyester resin composition includes a step of mixing the polyester resin and the pentaerythritol together in the presence of water.
Abstract:
An object of the present invention is to provide a production method in which melting and kneading is performed to obtain a resin composition containing at least an aliphatic polyester, silica and a dispersion aid, the method being capable of stably ensuring favorable dispersibility of silica and improving the tear strength of the resin composition. Provided is a method for producing an aliphatic polyester resin composition containing 100 parts by weight of an aliphatic polyester (A), 5 to 23 parts by weight of silica (B) and 8 to 23 parts by weight of a dispersion aid (C), the method including: a first step of mixing the aliphatic polyester (A) in an amount of 20 to 50% by weight based on the total amount of the aliphatic polyester (A) constituting the composition, and the silica (B); a second step of mixing the dispersion aid (C) with the mixture obtained in the first step; a third step of mixing the mixture obtained in the second step with the aliphatic polyester (A) remaining in an amount of 80 to 50% by weight based on the total amount of the aliphatic polyester (A) constituting the composition; and a step of melting and kneading the mixture obtained in the third step.
Abstract:
Provided is a resin composition excellent in processability and productivity, which improves low crystallization rate and improves processability in forming such as injection molding or sheet forming. Provided is a polyester resin composition including a polyester resin (A), a crystallization promoter (B), and pentaerythritol (C).
Abstract:
Provided are a resin composition containing poly(3-hydroxyalkanoate), the resin composition enabling a film or a sheet to be stably produced under practical processing conditions by inflation molding; and a method for producing the resin composition. The resin composition includes 100 parts by weight of poly(3-hydroxyalkanoate) and 5 to 15 parts by weight of an ester compound, and having a ratio of 3.5×10−2 to 4.8×10−2 (sec/[Pa·s]) between a melt viscosity (Pa·s) and a drawdown time (sec).
Abstract:
Provided is a method with which a biodegradable polyester film containing polyhydroxyalkanoate can be stably produced by film blowing under practical processing conditions. A method for producing a biodegradable polyester film containing a biodegradable aliphatic polyester (A) and a fatty acid amide (B) by film blowing, the biodegradable aliphatic polyester (A) containing polyhydroxyalkanoate, the method including: a step (I) of dry-blending the biodegradable aliphatic polyester (A) with a masterbatch containing the fatty acid amide (B) and a base material resin; and a step (II) of subjecting the mixture obtained in the step (I) to film blowing.
Abstract:
An object of the present invention is to: improve slowness of crystallization that is a drawback of polyhydroxyalkanoate; suppress bloom of a nucleating agent or the like; and improve surface smoothness and mold transferability of an obtained molded body.The present invention provides an aliphatic polyester resin composition including polyhydroxyalkanoate (A), pentaerythritol (B), and a filler (C).