公开(公告)号:US3793274A
公开(公告)日:1974-02-19
申请号:US17328571
申请日:1971-08-19
Applicant: KAO CORP
Inventor: HIYAMA O , TORIMAE Y , ITO K , KAWAHARA Y
IPC: C08L27/00 , C08K5/05 , C08K5/09 , C08K5/092 , C08L1/00 , C08L7/00 , C08L21/00 , C08L33/00 , C08L33/02 , C08L51/00 , C08L51/02 , C08F19/14 , C08F21/04
CPC classification number: C08K5/09 , C08K5/05 , C08K5/092 , C08L27/06 , C08L23/283
Abstract: THE RELEASE PROPERTIES OF POLYVINYL CHLORIDE RESIN ARE IMPROVED BY INCORPORATING THEREIN A TOTAL OF FROM 0.05 TO 2.0 PERCENT BY WEIGHT OF ONE OR MORE MATERIALS SELECTED FROM THE GROUP CONSISTING OF POLYMERIZED FATTY ACID, HYDROGENATED POLYMERIZED ACID AND POLYMERIZED FATTY ALCOHOLS.