Resin composition for capstock
    2.
    发明授权
    Resin composition for capstock 有权
    盖料的树脂组合物

    公开(公告)号:US06773821B2

    公开(公告)日:2004-08-10

    申请号:US10028368

    申请日:2001-12-28

    IPC分类号: C08L3312

    摘要: An acrylic resin composition suitable for the preparation of capstock for siding panels and having excellent impact resistance, weatherability and processability and a low gloss, which comprises 30 to 100% by weight of an impact modifier having a multilayer structure and 0 to 70% by weight of a methyl methacrylate homopolymer or copolymer and whose MFI (melt flow index measured according to ASTM D-1238 at 230° C. and a load of 3.8 kg) is not more than 0.35 g/10 minutes.

    摘要翻译: 一种丙烯酸树脂组合物,其适用于制备用于侧板的覆盖材料并且具有优异的耐冲击性,耐候性和加工性以及低光泽度,其包含30至100重量%的具有多层结构和0至70重量%的抗冲改性剂 的甲基丙烯酸甲酯均聚物或共聚物,其MFI(根据ASTM D-1238在230℃测量的熔体流动指数和3.8kg的负荷)不超过0.35g / 10分钟。

    Acrylic resin composition
    3.
    发明授权
    Acrylic resin composition 有权
    丙烯酸树脂组合物

    公开(公告)号:US06844396B2

    公开(公告)日:2005-01-18

    申请号:US10229277

    申请日:2002-08-28

    摘要: An acrylic resin composition with excellent impact resistance, weatherability, processability and low gloss is provided. The acrylic resin composition comprises, (A) 10 to 40 parts by weight of a high molecular weight acrylic (co)polymer which is a one-step or multi-step polymer containing 72 to 100% by weight of methyl methacrylate and 0 to 28% by weight of a copolymerizable monomer, the (co)polymer having a specific viscosity of at least 0.5 (solvent: toluene, concentration: 0.4%, temperature: 30° C.), wherein a polymer layer obtained in one of the steps contains at least 72% by weight of methyl methacrylate, has a specific viscosity of at least 0.5 and makes up at least 55% by weight of the total weight of the high molecular weight acrylic (co)polymer (A); (B) 0 to 80 parts by weight of an acrylic (co)polymer containing 50 to 100% by weight of methyl methacrylate and 0 to 50% by weight of a copolymerizable monomer, the acrylic (co)polymer having a specific viscosity of less than 0.5; (C) 10 to 90 parts by weight of an impact modifier with a multilayer structure, wherein the total of (A), (B) and (C) is 100 parts by weight and the composition has a melt flow index of 0.35 g/10 minutes to 1.4 g/10 minutes (230° C., 3.8 kg load).

    摘要翻译: 提供了耐冲击性,耐候性,加工性和低光泽性的丙烯酸树脂组合物。 丙烯酸树脂组合物包含:(A)10至40重量份的高分子量丙烯酸(共)聚合物,其为含有72至100重量%的甲基丙烯酸甲酯和0至28的一步或多步聚合物 重量比的可共聚单体,比重粘度至少为0.5的(共)聚合物(溶剂:甲苯,浓度:0.4%,温度:30℃)),其中在一个步骤中获得的聚合物层含有 至少72重量%的甲基丙烯酸甲酯具有至少0.5的比粘度和至少55重量%的高分子量丙烯酸(共)聚合物(A)的总重量; (B)0至80重量份的含有50至100重量%的甲基丙烯酸甲酯和0至50重量%的可共聚单体的丙烯酸(共)聚合物,所述丙烯酸(共)聚合物的比粘度较低 比0.5; (C)10〜90重量份具有多层结构的抗冲改性剂,其中(A),(B)和(C)的总计为100重量份,组合物的熔体流动指数为0.35g / 10分钟至1.4g / 10分钟(230℃,3.8kg负荷)。

    Resin composition for capstock
    4.
    发明授权
    Resin composition for capstock 有权
    盖料的树脂组合物

    公开(公告)号:US07338706B2

    公开(公告)日:2008-03-04

    申请号:US10311316

    申请日:2002-04-23

    IPC分类号: B32B5/16

    摘要: A resin composition for capstock, comprising 100 to 30 parts by weight of an impact resistance modifier having a multilayer structure, and 0 to 70 parts by weight of a methyl methacrylate (co)polymer containing 50 to 100% by weight of methyl methacrylate and 50 to 0% by weight of a monomer which is copolymerizable therewith, wherein the total amount of the impact resistance modifier and the methyl methacrylate (co)polymer is 100 parts by weight, wherein the outer layer of said impact resistance modifier and/or said methyl methacrylate copolymer is copolymerized with 0.5 to 40% by weight of a reactive monomer based on the total amount of the impact resistance modifier and the methyl methacrylate (co)polymer as a polymer component, and wherein the homopolymer of said reactive monomer has an SP value of 9.8 (cal/cm3)/1/2 or more.

    摘要翻译: 一种用于覆盖材料的树脂组合物,其包含100至30重量份的具有多层结构的抗冲击性改性剂和0至70重量份含有50至100重量%的甲基丙烯酸甲酯和50重量%的甲基丙烯酸甲酯(共)聚合物 至0重量%的与其可共聚的单体,其中耐冲击性改性剂和甲基丙烯酸甲酯(共)聚合物的总量为100重量份,其中所述耐冲击性改性剂的外层和/或所述甲基 甲基丙烯酸酯共聚物与作为聚合物成分的耐冲击性改性剂和甲基丙烯酸甲酯(共)聚合物的总量相当的反应性单体为0.5〜40重量%,其中所述反应性单体的均聚物具有SP值 为9.8(cal / cm 3)/ 1/2以上。

    Vinyl chloride resin composition
    6.
    发明授权
    Vinyl chloride resin composition 有权
    氯乙烯树脂组合物

    公开(公告)号:US06204327B1

    公开(公告)日:2001-03-20

    申请号:US09147076

    申请日:1999-04-27

    IPC分类号: C08L5104

    摘要: A vinyl chloride resin composition containing a graft copolymer A having an average particle diameter of at least 0.15 &mgr;m, prepared by polymerizing 50 to 90% of a solid matter of a rubber latex having a glass transition temperature of at most O° C., the rubber latex being prepared by polymerizing 50 to 100% of butadiene and/or alkyl acrylate, 0 to 40% of an aromatic vinyl monomer, 0 to 10% of a vinyl monomer and 0 to 5% of a polyfunctional monomer, with 10 to 50% of a mixture comprising 10 to 100% of an alkyl methacrylate, 0 to 90% of an aromatic vinyl monomer, 0 to 25% of a vinyl cyamide monomer and 0 to 20% of a vinyl monomer; a graft copolymer B having an average particle diameter of 0.05 to 0.13 &mgr;m, prepared by polymerizing 50 to 90% of the solid matter of the rubber latex with 10 to 50% of the mixture; and a vinyl chloride resin C; wherein the weight ratio of (copolymer A)/(copolymer B) is 50/50 to 90/15, and the weight ratio of (the total amount of copolymer A and copolymer B)/(vinyl chloride resin composition C) is 1/99 to 30/70; the composition being excellent in impact resistance and usable for the production of a pipe, a window frame and the like.

    摘要翻译: 一种氯乙烯树脂组合物,其含有平均粒径为0.15μm以上的接枝共聚物A,其通过聚合50〜90%的玻璃化转变温度为0℃以下的橡胶胶乳的固体成分, 橡胶胶乳通过将50至100%的丁二烯和/或丙烯酸烷基酯,0至40%的芳族乙烯基单体,0至10%的乙烯基单体和0至5%的多官能单体聚合而制备,其中10至50 %的包含10至100%的甲基丙烯酸烷基酯,0至90%的芳族乙烯基单体,0至25%的乙烯基酰胺单体和0至20%的乙烯基单体的混合物; 通过使10〜50%的混合物聚合50〜90%的橡胶胶乳固体成分而得到的平均粒径为0.05〜0.13μm的接枝共聚物B; 和氯乙烯树脂C; (共聚物A)/(共聚物B)的重量比为50/50〜90/15,(共聚物A和共聚物B的总量)/(氯乙烯树脂组合物C)的重量比为1 / 99至30/70; 该组合物的耐冲击性优异并且可用于制造管,窗框等。

    Process for preparing nano-sized metal oxide particles
    7.
    发明授权
    Process for preparing nano-sized metal oxide particles 有权
    制备纳米尺寸金属氧化物颗粒的方法

    公开(公告)号:US07482382B2

    公开(公告)日:2009-01-27

    申请号:US10848882

    申请日:2004-05-19

    摘要: The present invention is directed to novel sol-gel methods in which metal oxide precursor and an alcohol-based solution are mixed to form a reaction mixture that is then allowed to react to produce nanosized metal oxide particles. The methods of the present invention are more suitable for preparing nanosized metal oxide than are previously-described sol-gel methods. The present invention can provide for nanosized metal oxide particles more efficiently than the previously-described sol-gel methods by permitting higher concentrations of metal oxide precursor to be employed in the reaction mixture. The foregoing is provided by careful control of the pH conditions during synthesis and by ensuring that the pH is maintained at a value of about 7 or higher.

    摘要翻译: 本发明涉及新型溶胶 - 凝胶法,其中将金属氧化物前体和醇基溶液混合以形成反应混合物,然后使其反应生成纳米尺寸的金属氧化物颗粒。 本发明的方法比上述溶胶 - 凝胶法更适用于制备纳米尺寸金属氧化物。 本发明通过允许在反应混合物中使用更高浓度的金属氧化物前体,可以比上述溶胶 - 凝胶方法更有效地提供纳米尺寸的金属氧化物颗粒。 通过在合成期间仔细控制pH条件并通过确保pH保持在约7或更高的值来提供上述内容。

    Process for preparing nano-sized metal oxide particles
    8.
    发明申请
    Process for preparing nano-sized metal oxide particles 有权
    制备纳米尺寸金属氧化物颗粒的方法

    公开(公告)号:US20050260122A1

    公开(公告)日:2005-11-24

    申请号:US10848882

    申请日:2004-05-19

    IPC分类号: C01B13/32 C01G9/02

    摘要: The present invention is directed to novel sol-gel methods in which metal oxide precursor and an alcohol-based solution are mixed to form a reaction mixture that is then allowed to react to produce nanosized metal oxide particles. The methods of the present invention are more suitable for preparing nanosized metal oxide than are previously-described sol-gel methods. The present invention can provide for nanosized metal oxide particles more efficiently than the previously-described sol-gel methods by permitting higher concentrations of metal oxide precursor to be employed in the reaction mixture. The foregoing is provided by careful control of the pH conditions during synthesis and by ensuring that the pH is maintained at a value of about 7 or higher.

    摘要翻译: 本发明涉及新型溶胶 - 凝胶法,其中将金属氧化物前体和醇基溶液混合以形成反应混合物,然后使其反应生成纳米尺寸的金属氧化物颗粒。 本发明的方法比上述溶胶 - 凝胶法更适用于制备纳米尺寸金属氧化物。 本发明通过允许在反应混合物中使用更高浓度的金属氧化物前体,可以比上述溶胶 - 凝胶方法更有效地提供纳米尺寸的金属氧化物颗粒。 通过在合成期间仔细控制pH条件并通过确保pH保持在约7或更高的值来提供上述内容。

    Dispersion and retrieval of de-bundled nanotubes
    9.
    发明授权
    Dispersion and retrieval of de-bundled nanotubes 有权
    脱束纳米管的分散和回收

    公开(公告)号:US08894963B2

    公开(公告)日:2014-11-25

    申请号:US12979945

    申请日:2010-12-28

    IPC分类号: D01F9/12 C01B31/02

    摘要: A method for dispersing nanotubes, comprising forming a nanocomposite solution with associated nanotubes and nanoplatelets, mixing a surfactant to the nanocomposite solution, separating the nanocomposite in solution, wherein the nanotubes remain suspended in the surfactant solution, and isolating the nanotubes in solution. In certain instances, the method further comprises functionalizing the nanotubes in solution.

    摘要翻译: 一种用于分散纳米管的方法,包括用相关联的纳米管和纳米片形成纳米复合溶液,将表面活性剂混合到纳米复合物溶液中,在溶液中分离纳米复合物,其中纳米管保持悬浮在表面活性剂溶液中,并在溶液中分离纳米管。 在某些情况下,该方法还包括在溶液中使纳米管功能化。

    Processing aid for thermoplastic resin and thermoplastic resin composition containing the same
    10.
    发明授权
    Processing aid for thermoplastic resin and thermoplastic resin composition containing the same 有权
    含有该热塑性树脂和热塑性树脂组合物的加工助剂

    公开(公告)号:US07105602B1

    公开(公告)日:2006-09-12

    申请号:US09926085

    申请日:2000-04-14

    IPC分类号: C08G85/00

    CPC分类号: C08F20/12 C08F2/38

    摘要: The present invention provides a processing aid for thermoplastic resin having a weight average molecular weight of 10,000 to 300,000, which is obtained by polymerizing an alkyl (meth)acrylate, or an alkyl (meth)acrylate and another vinyl monomer copolymerizable therewith, in the presence of a mercaptan having an alkyl ester group with C4-20 alkyl group as a chain transfer agent, and/or an organic peroxide having a tertiary-butyl peroxy group as a polymerization initiator.

    摘要翻译: 本发明提供一种重均分子量为10,000〜300,000的热塑性树脂加工助剂,其通过使(甲基)丙烯酸烷基酯或(甲基)丙烯酸烷基酯和可与其共聚的其它乙烯基单体在 的具有C 4-14-20烷基的烷基酯基的硫醇作为链转移剂,和/或具有叔丁基过氧基的有机过氧化物作为聚合引发剂。