摘要:
Disclosed are a phosphor in which prevention of aging deterioration of luminance and prevention of deterioration of discharging characteristics are compatible, a method of manufacturing the phosphor, and a plasma display panel manufactured by using the phosphor. A phosphor of the invention containing Mn as an activator is one with Mn serving as a major emission, wherein a ratio of an activator concentration in a superficial portion of a phosphor particle to an activator concentration inside the phosphor particle is 0.3-0.7.
摘要:
Disclosed is a method of preparing a phosphor which exhibits superior optical characteristics and improved resistance to deterioration, comprising the steps of subjecting a phosphor precursor obtained by a liquid phase process to a first calcination under an oxygen-containing atmosphere at a prescribed temperature and then subjecting the calcined phosphor precursor to a second calcination at a temperature lower than the temperature of the first calcination.
摘要:
An objective is to provide a core/shell type particle phosphor exhibiting an optimal excitation wavelength for fluorescence observation and excellent emission luminance of PL, together with excellent durability, to which particles are produced so as to be suitable for the field of bio-nanotechnology. Disclosed is a core/shell type particle phosphor comprising a core particle phosphor and coated thereon, a shell made of a metal compound having a different composition from a composition constituting the core particle phosphor, wherein the core particle phosphor is a particle phosphor prepared by baking a precursor synthesized via a reactive crystallization method, satisfying a PL (photoluminescence) intensity ratio A of the core particle phosphor to the core/shell type particle phosphor, {PL intensity(core)/PL intensity(core/shell)}; 0.001≦A≦0.1, and a core/shell type particle diameter of at most 0.1 μm.
摘要翻译:目的是提供一种显示用于荧光观察的最佳激发波长的核/壳型粒子荧光体,并且PL的出色亮度优异,同时具有出色的耐久性,可以生产出适合于生物纳米技术领域的粒子。 公开了一种包含芯颗粒磷光体并涂覆在其上的核/壳型颗粒磷光体,由与构成芯颗粒磷光体的组成不同的组成的金属化合物制成的壳,其中核心颗粒磷光体是通过烘焙制备的颗粒磷光体 通过反应结晶法合成的前体,满足核心粒子荧光体的PL(光致发光)强度比A与核/壳型粒子荧光体{PL强度(核心)/ PL强度(核/壳))}。 0.001 <= A <= 0.1,核/壳型粒径为0.1μm以下。
摘要:
Disclosed is a fluorescent semiconductor microparticle assembly comprising at least three kinds of fluorescent semiconductor microparticles with an average particle size of from 1 to 10 nm, having the same chemical composition, a different average particle size and a different emission maximum wavelength in the emission spectra, wherein a standard deviation of emission intensity in each of the at least three kinds of fluorescent semiconductor microparticles is not more than 15%.
摘要:
A process for the production of semiconductor nanoparticles which realizes both uniform crystallite size and high crystallinity with the agglomeration thereof inhibited. This process is characterized by comprising the step (a) of generating nano-size particles from a semiconductor raw material and dispersing the particles in a gas phase, the step (b) of heat-treating the particles while keeping the particles in a state dispersed in the gas phase, and the step (c) of collecting the heat-treated particles immediately after the heat treatment with a solution of a surface modifier for modifying the surfaces of the particles.
摘要:
Disclosed is a fluorescent semiconductor microparticle assembly comprising at least three kinds of fluorescent semiconductor microparticles with an average particle size of from 1 to 10 nm, having the same chemical composition, a different average particle size and a different emission maximum wavelength in the emission spectra, wherein a standard deviation of emission intensity in each of the at least three kinds of fluorescent semiconductor microparticles is not more than 15%.
摘要:
Disclosed are a phosphor in which prevention of aging deterioration of luminance and prevention of deterioration of discharging characteristics are compatible, a method of manufacturing the phosphor, and a plasma display panel manufactured by using the phosphor. A phosphor of the invention containing Mn as an activator is one with Mn serving as a major emission, wherein a ratio of an activator concentration in a superficial portion of a phosphor particle to an activator concentration inside the phosphor particle is 0.3-0.7.
摘要:
A phosphor includes particles having an average particle size of from 10 nm to 2 μm, wherein 90% by mass or more of all of the particles have particle sizes within ±30% of the average particle size and a ratio of particles having no corners to all of the particles is 80% or more in number.
摘要:
A green light emitting silicate-containing phosphor having both enhanced luminescence intensity and a shortened persistence time and a method for manufacturing the foregoing phosphor can be provided, and a phosphor precursor can also be manufactured by releasing a mixed solution from an exit of the outlet flow passage, after a suspension containing a silicon compound is supplied into the first inlet flow passage, a solution containing a metallic compound for forming a silicate-containing phosphor precursor is supplied into the second inlet flow passage, and the foregoing suspension and solution are introduced into the contact section so as to mix with each other with controlling a flow of the mixed solution so as to keep a Reynolds number of the mixed solution to be 3×103 to 1×106.
摘要:
A biomolecule detection reagent comprising semiconductor nanoparticles and magnetic nanoparticles, incorporated in a bead comprising an inorganic compound or an organic polymer, and a surface of the beads is modified with a biomolecule detection molecule.