摘要:
A superconductive material is in composition expressed as Y.sub.0.33 Ba.sub.0.67).sub.a Cu.sub.b (OF).sub.c. The usual a, b and c are so selected as to satisfy a relation expression ax (mix valence of A)+bx (mix valence of B)=cx (mix valence of C).
摘要:
A method of manufacturing an oxide superconducting wire which can manufacture the longest possible wire by connecting relatively short wires with each other and is capable of suppressing reduction of a critical current resulting from influence by strain when the wires connected with each other are bent, an oxide superconducting wire, a superconducting coil and a superconducting apparatus are provided. According to the method of manufacturing an oxide superconducting wire by superposing end portions of two oxide superconducting wires with each other thereby bonding the end portions and connecting the oxide superconducting wires with each other, a junction formed by superposing the end portions with each other is so worked as to reduce the quantity of strain on an end of the junction when the two oxide superconducting wires and connected with each other are bent. Each of the oxide superconducting wire, the superconducting coil and the superconducting apparatus has the aforementioned junction, and the quantity of strain on the end of the junction is reduced in the aforementioned manner.
摘要:
A method of manufacturing an oxide superconducting wire which can manufacture the longest possible wire by connecting relatively short wires with each other and is capable of suppressing reduction of a critical current resulting from influence by strain when the wires connected with each other are bent, an oxide superconducting wire, a superconducting coil and a superconducting apparatus are provided. According to the method of manufacturing an oxide superconducting wire by superposing end portions of two oxide superconducting wires with each other thereby bonding the end portions and connecting the oxide superconducting wires with each other, a junction formed by superposing the end portions with each other is so worked as to reduce the quantity of strain on an end of the junction when the two oxide superconducting wires and connected with each other are bent. Each of the oxide superconducting wire, the superconducting coil and the superconducting apparatus has the aforementioned junction, and the quantity of strain on the end of the junction is reduced in the aforementioned manner.
摘要:
A method of manufacturing an oxide superconducting wire which can manufacture the longest possible wire by connecting relatively short wires with each other and is capable of suppressing reduction of a critical current resulting from influence by strain when the wires connected with each other are bent, an oxide superconducting wire, a superconducting coil and a superconducting apparatus are provided. According to the method of manufacturing an oxide superconducting wire by superposing end portions of two oxide superconducting wires with each other thereby bonding the end portions and connecting the oxide superconducting wires with each other, a junction formed by superposing the end portions with each other is so worked as to reduce the quantity of strain on an end of the junction when the two oxide superconducting wires and connected with each other are bent. Each of the oxide superconducting wire, the superconducting coil and the superconducting apparatus has the aforementioned junction, and the quantity of strain on the end of the junction is reduced in the aforementioned manner.
摘要:
A method of manufacturing an oxide superconducting wire which can manufacture the longest possible wire by connecting relatively short wires with each other and is capable of suppressing reduction of a critical current resulting from influence by strain when the wires connected with each other are bent, an oxide superconducting wire, a superconducting coil and a superconducting apparatus are provided. According to the method of manufacturing an oxide superconducting wire by superposing end portions of two oxide superconducting wires (1, 2) with each other thereby bonding the end portions and connecting the oxide superconducting wires with each other, a junction (L) formed by superposing the end portions with each other is so worked as to reduce the quantity of strain on an end of the junction (L) when the two oxide superconducting wires (1) and (2) connected with each other are bent. Each of the oxide superconducting wire, the superconducting coil and the superconducting apparatus has the aforementioned junction (L), and the quantity of strain on the end of the junction (L) is reduced in the aforementioned manner.
摘要:
Provided herein is a method of efficiently preparing a thin film having a higher critical temperature as to an oxide superconducting material containing Tl. A thin film of an oxide containing Tl is formed and then heat treated at a temperature of about 850.degree. to 950.degree. C. for a short time, and thereafter further heat treated at a temperature, which is lower than the preceding heat treatment temperature, of at least about 750.degree. C. for a long time. The thin film is heat treated in an atmosphere having an oxygen partial pressure of not more than about 0.1 atm. In formation of a Tl superconducting thin film, on the other hand, a 1212 phase layer is reacted with an amorphous Ca--Cu--O layer to form a 1223 phase layer, or a layer containing volatile metal elements (Tl, Bi and Pb, for example) and oxygen is reacted with another layer containing other elements than the volatile metal elements to form a superconducting film having a high critical temperature.
摘要:
A combination lamp body 10, which are attached with a combination lamp, is arranged in a position adjacent to headlamp bodies 50, and includes a shaft provided on the outer end in the vehicle width direction. A support provided to each of the headlamp bodies 50 regulates inward and forward movements of the shaft in the vehicle width direction. An engagement part is fixed to the vehicle body. An attachment member 20 is provided removable from the rear face of the combination lamp body 10, and includes a locking part 21 engaging with the engagement part. While the outer ends of the combination lamp body 10 are rotated and moved toward the rear centered around the shaft 14, which is regulated in movement by the support 53, and the combination lamp body 10 reaches a predetermined position, the support regulates inward and forward movements of the combination lamp body 10 in the vehicle width direction, and the engagement part engages with the locking part 21 to regulate outward and backward movements of the combination lamp body 10 in the vehicle width direction.
摘要:
A method of manufacturing an oxide superconducting wire which can manufacture the longest possible wire by connecting relatively short wires with each other and is capable of suppressing reduction of a critical current resulting from influence by strain when the wires connected with each other are bent, an oxide superconducting wire, a superconducting coil and a superconducting apparatus are provided. According to the method of manufacturing an oxide superconducting wire by superposing end portions of two oxide superconducting wires with each other thereby bonding the end portions and connecting the oxide superconducting wires with each other, a junction formed by superposing the end portions with each other is so worked as to reduce the quantity of strain on an end of the junction when the two oxide superconducting wires and connected with each other are bent. Each of the oxide superconducting wire, the superconducting coil and the superconducting apparatus has the aforementioned junction, and the quantity of strain on the end of the junction is reduced in the aforementioned manner.