ENAMEL COMPOSITION, METHOD FOR PREPARATION THEREOF AND COOKING APPLIANCE USING SAME

    公开(公告)号:US20210214271A1

    公开(公告)日:2021-07-15

    申请号:US17147823

    申请日:2021-01-13

    Abstract: The present disclosure relates to an enamel composition, a method for preparation thereof, and a cooking appliance using the same, which provide excellent cleaning performance, reduce a defect caused by carbon gases when an enamel coating is implemented on a base material made of cast iron, and provides excellent thermal shock resistance and durability. In the enamel composition according to the disclosure, components implementing glass and components having catalytic performance have an optimal component system, thereby ensuring excellent thermal shock resistance and durability. The enamel composition of the present disclosure has a component system that helps enamel cast iron as well as low carbon steel, thereby ensuring excellent cleaning performance, thermal shock resistance and durability. The enamel composition of the present disclosure is appropriate for a cooktop grate, a hob burner, and the like which directly contact a fire and are exposed to repetitive thermal shock.

    ENAMEL COMPOSITION, METHOD FOR PREPARING ENAMEL COMPOSITION, AND COOKING APPLIANCE

    公开(公告)号:US20210009814A1

    公开(公告)日:2021-01-14

    申请号:US16925733

    申请日:2020-07-10

    Abstract: A cooking appliance includes a chamber surface that defines a cavity including a cooking chamber, a door that is configured to open and close the cavity and has a door surface configured to face the cavity, a heat source configured to supply heat to the cavity, and a coating layer disposed on the chamber surface or the door surface. The coating layer includes an enamel composition of materials including 30 to 45 wt % of phosphorus pentoxide (P2O5), 5 to 20 wt % of silicon dioxide (SiO2), 15 to 30 wt % of aluminum oxide (Al2O3), 10 to 20 wt % of zirconium dioxide (ZrO2), 5 to 20 wt % of at least one of lithium oxide (Li2O), sodium oxide (N2O), or potassium oxide (K2O), 5 to 15 wt % of boron trioxide (B2O3), and10 to 25 wt % of vanadium pentoxide (V2O5).

Patent Agency Ranking