Abstract:
The present invention addresses the problem of providing a laminate having sufficient delamination prevention performance and simultaneously having an inorganic layer surface imparted with brightness. The laminate of the present invention is a laminate having a polyolefin-based resin layer, a layer for deposition and an inorganic layer in this order, wherein the layer for deposition includes a composition (P) for a layer for deposition and polypropylene (D), the composition (P) for a layer for deposition is obtained by melt-kneading 30 to 85% by weight of isotactic polypropylene (A) and 70 to 15% by weight of a propylene-based copolymer (B), a part or all of the isotactic polypropylene (A) and/or the propylene-based copolymer (B) has been graft-modified with a graft monomer (C), and the propylene-based copolymer (B) contains 45 to 89% by mol of constituent units derived from propylene and 11 to 55% by mol of constituent units derived from at least one α-olefin selected from ethylene and α-olefins of 4 to 20 carbon atoms.
Abstract:
An adhesive resin composition including a propylene polymer (A), an ethylene polymer (B), and a thermoplastic resin (C) including a copolymer containing not less than 60 mol % and not more than 99 mol % of structural units derived from 4-methyl-1-pentene, and not less than 1 mol % and not more than 40 mol % of structural units derived from a C2-C20 α-olefin other than 4-methyl-1-pentene, these structural units representing total 100 mol % of the copolymer, the thermoplastic resin (C) showing a melting point Tm of not more than 199° C. or showing substantially no melting point as analyzed with a differential scanning calorimeter (DSC). The total of the components (A), (B) and (C) includes 45 to 75 parts by mass of the component (A), 5 to 20 parts by mass of the component (B), and 15 to 45 parts by mass of the component (C).