摘要:
The invention relates to a method of preparing wholly aromatic polyester including: mixing monomers, introducing the mixed monomers into a reactor having a rectangular or trapezoidal plate type stirring impeller, and polymerizing the introduced monomers through esterification with a power per unit volume of 10˜60 kW/m3, a length (L) to diameter (D) ratio of the stirring impeller is 1˜3:1, and a distance between the bottom of the reactor and a lower portion of the stirring impeller is 1/100˜ 1/15 times of the diameter (D); b) pulverizing the obtained polymer; and c) solid state polymerizing the pulverized polymer. The present invention also relates to a method of preparing wholly aromatic polyester having excellent heat resistant properties in which byproduct is effectively discharged by controlling a heating rate and reaction holding time between the weight loss initiating temperature and the melting point of a low molecular weight polymer generated in a melt polymerization in a solid state polymerization, adhesion does not occur, and discoloration due to heating does not occur.
摘要:
Provided is a method of preparing a wholly aromatic liquid crystalline polyester resin and a wholly aromatic liquid crystalline polyester resin prepared by the method, and a compound of the wholly aromatic liquid crystalline polyester resin. The disclosed method of preparing the wholly aromatic liquid crystalline polyester resin includes a step (a first temperature increasing step) of increasing the temperature of a reaction mixture including at least one monomer at a first temperature increasing rate up to a first temperature; a step (an isothermal maintaining step) of maintaining the reaction mixture that passed through the first temperature increasing step at the first temperature for a first time; and a step (a second temperature increasing step) of increasing the temperature of the reaction mixture that passed through the isothermal maintaining step at a second temperature increasing rate.
摘要:
Disclosed are a production method for a wholly aromatic liquid crystalline polyester resin, a wholly aromatic liquid crystalline polyester resin produced using the method, and a compound of the wholly aromatic liquid crystalline polyester resin. The disclosed production method for a wholly aromatic liquid crystalline polyester resin comprises the steps of synthesizing a wholly aromatic liquid crystalline polyester resin by synthesizing a wholly aromatic liquid crystalline polyester prepolymer by a condensation polymerization of a monomer and then reducing the pressure inside a reaction vessel containing the synthesized prepolymer at a predetermined internal pressure reduction rate of the reaction vessel.
摘要:
Disclosed are a production method for a wholly aromatic liquid crystalline polyester resin, a wholly aromatic liquid crystalline polyester resin produced using the method, and a compound of the wholly aromatic liquid crystalline polyester resin. The disclosed production method for a wholly aromatic liquid crystalline polyester resin comprises the steps of synthesizing a wholly aromatic liquid crystalline polyester resin by synthesizing a wholly aromatic liquid crystalline polyester prepolymer by a condensation polymerization of a monomer and then reducing the pressure inside a reaction vessel containing the synthesized prepolymer at a predetermined internal pressure reduction rate of the reaction vessel.
摘要:
Disclosed are a wholly aromatic liquid crystal polyester resin compound, a preparation method thereof, parts for optical pickup, and a preparation method thereof. The disclosed wholly aromatic liquid crystal polyester resin compound comprises two kinds of wholly aromatic liquid crystal polyester resins having different melting points and an additive, and most of the terminal groups in the resins having lower melting points among the resins comprise a carboxyl group.